Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.852 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density12.91 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFd3m [227] |
HallF 4d 2 3 1d |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | elastic energy [meV] | MCIA† [Å2] |
---|---|---|---|---|
Ag (mp-124) | <1 0 0> | <1 0 0> | 0.000 | 311.5 |
SiC (mp-8062) | <1 0 0> | <1 0 0> | 0.000 | 249.2 |
SiC (mp-7631) | <0 0 1> | <1 1 1> | 0.000 | 107.9 |
SiC (mp-11714) | <0 0 1> | <1 1 1> | 0.001 | 107.9 |
SrTiO3 (mp-4651) | <1 1 0> | <1 0 0> | 0.005 | 62.3 |
SrTiO3 (mp-4651) | <1 0 0> | <1 1 0> | 0.006 | 88.1 |
SrTiO3 (mp-4651) | <1 0 1> | <1 1 1> | 0.006 | 107.9 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 0.012 | 107.9 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 0.015 | 311.5 |
SrTiO3 (mp-4651) | <0 0 1> | <1 0 0> | 0.020 | 62.3 |
Au (mp-81) | <1 0 0> | <1 0 0> | 0.025 | 311.5 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 0.026 | 249.2 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 0.031 | 107.9 |
GaSb (mp-1156) | <1 0 0> | <1 0 0> | 0.038 | 311.5 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 0.061 | 249.2 |
CsI (mp-614603) | <1 0 0> | <1 0 0> | 0.062 | 62.3 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 0.064 | 311.5 |
CsI (mp-614603) | <1 1 0> | <1 1 0> | 0.064 | 88.1 |
CsI (mp-614603) | <1 1 1> | <1 1 1> | 0.065 | 107.9 |
MgF2 (mp-1249) | <1 0 1> | <1 1 0> | 0.075 | 264.3 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 0.106 | 311.5 |
NdGaO3 (mp-3196) | <1 0 0> | <1 1 0> | 0.108 | 88.1 |
LiAlO2 (mp-3427) | <0 0 1> | <1 0 0> | 0.123 | 249.2 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 0.128 | 62.3 |
CdWO4 (mp-19387) | <0 1 0> | <1 1 0> | 0.130 | 264.3 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 0.147 | 311.5 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 0.161 | 311.5 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 0.197 | 311.5 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 0.203 | 176.2 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 0.232 | 62.3 |
GdScO3 (mp-5690) | <0 1 0> | <1 1 0> | 0.245 | 88.1 |
C (mp-48) | <1 0 0> | <1 1 0> | 0.246 | 176.2 |
ZnTe (mp-2176) | <1 0 0> | <1 0 0> | 0.261 | 311.5 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 0> | 0.274 | 186.9 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 0.283 | 62.3 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 0.293 | 311.5 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 0.302 | 264.3 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 0.306 | 264.3 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 0.317 | 249.2 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 0.329 | 311.5 |
TbScO3 (mp-31119) | <0 1 0> | <1 1 0> | 0.341 | 88.1 |
WS2 (mp-224) | <1 1 0> | <1 0 0> | 0.344 | 311.5 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 0.366 | 62.3 |
Si (mp-149) | <1 1 1> | <1 0 0> | 0.377 | 311.5 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 0.378 | 311.5 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 0.397 | 186.9 |
C (mp-48) | <1 1 0> | <1 1 0> | 0.401 | 264.3 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 0> | 0.420 | 186.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 0.431 | 311.5 |
BN (mp-984) | <1 0 0> | <1 1 0> | 0.442 | 176.2 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
171 | 91 | 91 | 0 | 0 | 0 |
91 | 171 | 91 | 0 | 0 | 0 |
91 | 91 | 171 | 0 | 0 | 0 |
0 | 0 | 0 | 58 | 0 | 0 |
0 | 0 | 0 | 0 | 58 | 0 |
0 | 0 | 0 | 0 | 0 | 58 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
9.3 | -3.2 | -3.2 | 0 | 0 | 0 |
-3.2 | 9.3 | -3.2 | 0 | 0 | 0 |
-3.2 | -3.2 | 9.3 | 0 | 0 | 0 |
0 | 0 | 0 | 17.2 | 0 | 0 |
0 | 0 | 0 | 0 | 17.2 | 0 |
0 | 0 | 0 | 0 | 0 | 17.2 |
Shear Modulus GV51 GPa |
Bulk Modulus KV118 GPa |
Shear Modulus GR49 GPa |
Bulk Modulus KR118 GPa |
Shear Modulus GVRH50 GPa |
Bulk Modulus KVRH118 GPa |
Elastic Anisotropy0.17 |
Poisson's Ratio0.31 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YbNi4Au (mp-1024977) | 0.0000 | 0.040 | 3 |
TmInCu4 (mp-1024957) | 0.0028 | 0.000 | 3 |
GdNi4Au (mp-1077131) | 0.0027 | 0.855 | 3 |
YbCu4Au (mp-1077165) | 0.0028 | 0.000 | 3 |
GdInCu4 (mp-1077293) | 0.0009 | 0.000 | 3 |
BaPt2 (mp-747) | 0.0000 | 0.000 | 2 |
CeRh2 (mp-951) | 0.0000 | 0.000 | 2 |
NpAl2 (mp-20660) | 0.0000 | 0.000 | 2 |
HfZn2 (mp-514) | 0.0000 | 0.000 | 2 |
DyIr2 (mp-1358) | 0.0000 | 0.000 | 2 |
Co (mp-1072089) | 0.0000 | 0.199 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sr_sv Pt |
Final Energy/Atom-5.4629 eV |
Corrected Energy-32.7773 eV
-32.7773 eV = -32.7773 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)