material

HfGe2

ID:

mp-13683

DOI:

10.17188/1189717


Tags: Hafnium germanium (1:2) Hafnium germanide (1/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.406 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.017 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
9.87 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Hf5Ge4 + Ge
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Cmcm [63]
Hall
-C 2c 2
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 16698 from Topological Materials Database
Topological Classification
TI*
Subclassification
NLC
* Topological insulator
No Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
YAlO3 (mp-3792) <1 0 0> <1 0 1> 0.022 80.7
Fe3O4 (mp-19306) <1 0 0> <0 1 0> 0.046 72.8
BN (mp-984) <1 0 0> <0 1 0> 0.047 58.3
SrTiO3 (mp-4651) <0 0 1> <0 1 0> 0.049 247.6
CsI (mp-614603) <1 0 0> <0 1 0> 0.049 247.6
SrTiO3 (mp-4651) <1 1 0> <0 1 0> 0.053 247.6
YVO4 (mp-19133) <0 0 1> <0 1 0> 0.055 262.2
YVO4 (mp-19133) <1 0 0> <0 1 0> 0.056 276.8
ZnO (mp-2133) <1 0 1> <0 1 0> 0.059 218.5
Ni (mp-23) <1 1 0> <0 1 0> 0.059 276.8
Al (mp-134) <1 0 0> <0 1 0> 0.061 131.1
MgO (mp-1265) <1 0 0> <0 1 0> 0.064 72.8
SiC (mp-7631) <1 1 1> <1 1 1> 0.064 82.0
TiO2 (mp-390) <0 0 1> <0 1 0> 0.068 14.6
AlN (mp-661) <0 0 1> <0 1 0> 0.076 160.2
AlN (mp-661) <1 1 0> <1 0 1> 0.079 80.7
ZnSe (mp-1190) <1 0 0> <0 1 0> 0.081 131.1
C (mp-48) <1 0 1> <0 1 0> 0.094 218.5
GaSe (mp-1943) <1 0 1> <0 1 0> 0.095 276.8
KTaO3 (mp-3614) <1 0 0> <0 1 0> 0.101 131.1
LaAlO3 (mp-2920) <0 0 1> <0 1 0> 0.108 276.8
SiC (mp-8062) <1 1 1> <0 1 0> 0.111 233.1
GaAs (mp-2534) <1 0 0> <0 1 0> 0.116 131.1
SiC (mp-11714) <1 1 1> <0 1 0> 0.117 276.8
PbS (mp-21276) <1 0 0> <0 1 0> 0.129 72.8
Cu (mp-30) <1 0 0> <0 1 0> 0.136 116.5
NaCl (mp-22862) <1 0 0> <0 1 0> 0.150 131.1
CdWO4 (mp-19387) <1 1 0> <0 1 0> 0.166 247.6
InAs (mp-20305) <1 1 0> <1 0 1> 0.168 161.5
ZnTe (mp-2176) <1 1 0> <1 0 1> 0.171 161.5
C (mp-66) <1 0 0> <0 1 0> 0.181 116.5
TePb (mp-19717) <1 1 0> <1 0 1> 0.182 242.2
C (mp-66) <1 1 0> <1 0 1> 0.184 161.5
TeO2 (mp-2125) <1 0 1> <0 1 0> 0.189 305.9
BaTiO3 (mp-5986) <1 1 0> <0 1 0> 0.189 262.2
AlN (mp-661) <1 0 1> <1 1 0> 0.192 175.8
MoSe2 (mp-1634) <1 1 0> <1 1 0> 0.194 175.8
Au (mp-81) <1 1 0> <0 1 0> 0.198 320.5
Ge3(BiO3)4 (mp-23560) <1 1 0> <1 0 1> 0.200 161.5
Ge (mp-32) <1 0 0> <0 1 0> 0.200 131.1
NdGaO3 (mp-3196) <1 0 0> <1 1 0> 0.212 175.8
Te2Mo (mp-602) <0 0 1> <0 1 0> 0.213 233.1
DyScO3 (mp-31120) <0 1 1> <1 0 1> 0.215 161.5
SiC (mp-7631) <1 1 0> <1 0 1> 0.216 80.7
Ag (mp-124) <1 1 0> <0 1 0> 0.227 320.5
GaSe (mp-1943) <0 0 1> <0 1 0> 0.228 102.0
CdS (mp-672) <1 0 1> <0 0 1> 0.229 229.7
SiC (mp-11714) <1 1 0> <1 0 1> 0.230 161.5
LiGaO2 (mp-5854) <1 1 0> <0 1 0> 0.241 145.7
GaN (mp-804) <0 0 1> <0 1 0> 0.246 160.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
198 66 85 0 0 0
66 172 68 0 0 0
85 68 213 0 0 0
0 0 0 71 0 0
0 0 0 0 104 0
0 0 0 0 0 65
Compliance Tensor Sij (10-12Pa-1)
6.5 -1.7 -2.1 0 0 0
-1.7 7.1 -1.6 0 0 0
-2.1 -1.6 6 0 0 0
0 0 0 14.2 0 0
0 0 0 0 9.6 0
0 0 0 0 0 15.5
Shear Modulus GV
72 GPa
Bulk Modulus KV
113 GPa
Shear Modulus GR
69 GPa
Bulk Modulus KR
112 GPa
Shear Modulus GVRH
71 GPa
Bulk Modulus KVRH
113 GPa
Elastic Anisotropy
0.24
Poisson's Ratio
0.24

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TmSnGe (mp-1025129) 0.4319 0.000 3
Hf2CuGe4 (mp-17801) 0.4564 0.040 3
Zr2CuGe4 (mp-18279) 0.4389 0.026 3
ErSnGe (mp-1071492) 0.4331 0.000 3
DySnGe (mp-1080405) 0.4187 0.000 3
UGe2 (mp-1071400) 0.2820 0.174 2
ZrGe2 (mp-2430) 0.0887 0.007 2
ScGe2 (mp-10212) 0.1898 0.000 2
TiSi2 (mp-1077503) 0.2182 0.000 2
ThSn2 (mp-30872) 0.2756 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Hf_pv Ge_d
Final Energy/Atom
-6.8038 eV
Corrected Energy
-40.8225 eV
-40.8225 eV = -40.8225 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 636542
  • 16698
  • 636552
Submitted by
User remarks:
  • Hafnium germanide (1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)