material

HfSiSe

ID:

mp-13962

DOI:

10.17188/1189843


Tags: Hafnium silicide selenide (1/1/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Unknown
Formation Energy / Atom
-1.001 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.57 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P4/nmm [129]
Hall
P 4ab 2ab 1ab
Point Group
4/mmm
Crystal System
tetragonal

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
TiO2 (mp-390) <0 0 1> <0 0 1> 0.000 115.9
GaSe (mp-1943) <1 0 0> <0 0 1> 0.014 270.4
GdScO3 (mp-5690) <1 1 0> <0 0 1> 0.017 64.4
CaCO3 (mp-3953) <1 0 0> <1 1 0> 0.019 87.2
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.020 64.4
LiGaO2 (mp-5854) <0 1 0> <1 1 0> 0.029 130.9
PbS (mp-21276) <1 1 0> <1 0 0> 0.032 154.2
CaCO3 (mp-3953) <1 0 1> <0 0 1> 0.034 90.1
DyScO3 (mp-31120) <1 0 0> <0 0 1> 0.034 321.9
NaCl (mp-22862) <1 0 0> <0 0 1> 0.035 64.4
MgO (mp-1265) <1 1 0> <1 0 0> 0.035 154.2
TePb (mp-19717) <1 1 1> <1 0 1> 0.037 300.8
WS2 (mp-224) <1 0 1> <0 0 1> 0.049 231.8
LaAlO3 (mp-2920) <1 0 1> <1 0 1> 0.049 300.8
C (mp-66) <1 0 0> <0 0 1> 0.049 12.9
CdWO4 (mp-19387) <0 0 1> <1 1 1> 0.055 91.0
C (mp-66) <1 1 0> <0 0 1> 0.056 90.1
LiGaO2 (mp-5854) <0 1 1> <1 1 0> 0.057 43.6
InAs (mp-20305) <1 1 1> <1 1 0> 0.068 130.9
ZnTe (mp-2176) <1 1 1> <1 1 0> 0.073 130.9
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.076 64.4
CaCO3 (mp-3953) <0 0 1> <1 1 0> 0.078 43.6
C (mp-66) <1 1 1> <1 1 0> 0.086 43.6
SiC (mp-7631) <1 0 1> <0 0 1> 0.088 334.8
TeO2 (mp-2125) <0 0 1> <1 1 0> 0.091 349.0
BN (mp-984) <0 0 1> <1 1 0> 0.093 43.6
LaAlO3 (mp-2920) <0 0 1> <1 0 1> 0.093 100.3
ZnO (mp-2133) <0 0 1> <1 1 0> 0.095 130.9
LiGaO2 (mp-5854) <1 1 1> <1 0 0> 0.099 339.3
YAlO3 (mp-3792) <1 0 0> <0 0 1> 0.100 321.9
CdTe (mp-406) <1 1 1> <1 0 1> 0.100 300.8
SiO2 (mp-6930) <0 0 1> <1 1 0> 0.113 43.6
LiAlO2 (mp-3427) <1 1 1> <0 0 1> 0.120 218.9
CdSe (mp-2691) <1 1 0> <1 0 0> 0.121 215.9
GaSb (mp-1156) <1 1 0> <1 0 0> 0.123 215.9
InSb (mp-20012) <1 1 1> <1 0 1> 0.123 300.8
KP(HO2)2 (mp-23959) <0 1 0> <0 0 1> 0.127 77.3
PbSe (mp-2201) <1 1 0> <1 0 0> 0.132 215.9
TbScO3 (mp-31119) <1 1 0> <0 0 1> 0.154 64.4
Al (mp-134) <1 0 0> <0 0 1> 0.156 64.4
SiC (mp-11714) <1 1 0> <1 0 1> 0.164 267.4
KP(HO2)2 (mp-23959) <1 0 0> <0 0 1> 0.164 115.9
YVO4 (mp-19133) <1 0 1> <0 0 1> 0.165 206.0
PbS (mp-21276) <1 0 0> <1 0 0> 0.168 215.9
SiO2 (mp-6930) <1 0 0> <1 1 0> 0.169 218.1
CdSe (mp-2691) <1 1 1> <1 1 0> 0.174 130.9
YVO4 (mp-19133) <0 0 1> <0 0 1> 0.177 51.5
ZnTe (mp-2176) <1 1 0> <1 0 0> 0.179 215.9
Ga2O3 (mp-886) <1 0 -1> <1 0 1> 0.187 234.0
SiO2 (mp-6930) <1 1 1> <1 0 1> 0.188 267.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
233 62 77 0 0 0
62 233 77 0 0 0
77 77 62 0 0 0
0 0 0 82 0 0
0 0 0 0 82 0
0 0 0 0 0 116
Compliance Tensor Sij (10-12Pa-1)
7.6 1.8 -11.5 0 0 0
1.8 7.6 -11.5 0 0 0
-11.5 -11.5 44.2 0 0 0
0 0 0 12.2 0 0
0 0 0 0 12.2 0
0 0 0 0 0 8.6
Shear Modulus GV
77 GPa
Bulk Modulus KV
106 GPa
Shear Modulus GR
36 GPa
Bulk Modulus KR
59 GPa
Shear Modulus GVRH
56 GPa
Bulk Modulus KVRH
83 GPa
Elastic Anisotropy
6.59
Poisson's Ratio
0.22

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
20
U Values
--
Pseudopotentials
VASP PAW: Si Se Hf_pv
Final Energy/Atom
-7.2910 eV
Corrected Energy
-43.7461 eV
-43.7461 eV = -43.7461 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 25736

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)