Final Magnetic Moment4.601 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.037 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.046 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.31 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnTe |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 173.0 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 230.7 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 230.7 |
AlN (mp-661) | <1 0 0> | <1 1 1> | 288.3 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 199.8 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 299.6 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 199.8 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 266.3 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 33.3 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 47.1 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 57.7 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 166.5 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 332.9 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 329.6 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 199.8 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 266.3 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 141.2 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 166.5 |
BN (mp-984) | <1 0 0> | <1 0 0> | 99.9 |
BN (mp-984) | <1 1 1> | <1 1 0> | 235.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 94.2 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 133.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 47.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 166.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 66.6 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 299.6 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 33.3 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 47.1 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 57.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 299.6 |
Al (mp-134) | <1 0 0> | <1 0 0> | 33.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 33.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 47.1 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 166.5 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 329.6 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 230.7 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 266.3 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 33.3 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 299.6 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 166.5 |
CdTe (mp-406) | <1 1 1> | <1 1 1> | 230.7 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 33.3 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 47.1 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 233.0 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 282.5 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 282.5 |
MgO (mp-1265) | <1 1 1> | <1 1 1> | 230.7 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 266.3 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 166.5 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 188.3 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
115 | 64 | 64 | 0 | 0 | 0 |
64 | 115 | 64 | 0 | 0 | 0 |
64 | 64 | 115 | 0 | 0 | 0 |
0 | 0 | 0 | 25 | 0 | 0 |
0 | 0 | 0 | 0 | 25 | 0 |
0 | 0 | 0 | 0 | 0 | 25 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
14.5 | -5.2 | -5.2 | 0 | 0 | 0 |
-5.2 | 14.5 | -5.2 | 0 | 0 | 0 |
-5.2 | -5.2 | 14.5 | 0 | 0 | 0 |
0 | 0 | 0 | 39.7 | 0 | 0 |
0 | 0 | 0 | 0 | 39.7 | 0 |
0 | 0 | 0 | 0 | 0 | 39.7 |
Shear Modulus GV25 GPa |
Bulk Modulus KV81 GPa |
Shear Modulus GR25 GPa |
Bulk Modulus KR81 GPa |
Shear Modulus GVRH25 GPa |
Bulk Modulus KVRH81 GPa |
Elastic Anisotropy0.00 |
Poisson's Ratio0.36 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sr4SO3 (mp-1079788) | 0.0000 | 0.200 | 3 |
BaSr3O4 (mp-984729) | 0.0000 | 0.044 | 3 |
ScH4Pd3 (mp-981386) | 0.0000 | 0.037 | 3 |
Sr3CdO4 (mp-981103) | 0.0000 | 0.019 | 3 |
SrCa3O4 (mp-978844) | 0.0000 | 0.040 | 3 |
HoP (mp-744) | 0.0000 | 0.000 | 2 |
GeSe (mp-10759) | 0.0000 | 0.008 | 2 |
ThGe (mp-1093) | 0.0000 | 0.000 | 2 |
CeAs (mp-2748) | 0.0000 | 0.000 | 2 |
UBi (mp-22886) | 0.0000 | 0.191 | 2 |
Sc (mp-1008681) | 0.0000 | 0.719 | 1 |
Ca (mp-10683) | 0.0000 | 0.400 | 1 |
C (mp-998866) | 0.0000 | 2.755 | 1 |
Sb (mp-133) | 0.0000 | 0.051 | 1 |
Na (mp-1093989) | 0.0000 | 1.076 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mn_pv Te |
Final Energy/Atom-6.1893 eV |
Corrected Energy-12.3785 eV
-12.3785 eV = -12.3785 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)