material

AlAgSe2

ID:

mp-14091

DOI:

10.17188/1189924


Tags: Silver aluminium selenide

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.855 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.79 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
1.717 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I42d [122]
Hall
I 4 2bw
Point Group
42m
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 28745 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.001 146.1
NaCl (mp-22862) <1 0 0> <0 0 1> 0.002 292.1
Fe3O4 (mp-19306) <1 0 0> <0 0 1> 0.004 73.0
KCl (mp-23193) <1 0 0> <0 0 1> 0.009 328.6
Cu (mp-30) <1 0 0> <0 0 1> 0.012 328.6
Al (mp-134) <1 0 0> <0 0 1> 0.012 146.1
ZnO (mp-2133) <1 0 1> <0 0 1> 0.013 219.1
CdWO4 (mp-19387) <0 0 1> <1 0 1> 0.015 152.9
GaN (mp-804) <0 0 1> <1 1 0> 0.017 285.0
PbS (mp-21276) <1 1 0> <1 0 1> 0.019 152.9
Ag (mp-124) <1 0 0> <0 0 1> 0.025 292.1
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.027 134.3
MgO (mp-1265) <1 0 0> <0 0 1> 0.027 36.5
TiO2 (mp-390) <0 0 1> <0 0 1> 0.030 73.0
TiO2 (mp-2657) <1 1 0> <0 0 1> 0.032 255.6
MgO (mp-1265) <1 1 0> <1 0 1> 0.033 76.5
SiC (mp-7631) <0 0 1> <0 0 1> 0.034 292.1
SiC (mp-11714) <0 0 1> <0 0 1> 0.037 292.1
KCl (mp-23193) <1 1 0> <1 0 1> 0.055 229.4
C (mp-48) <0 0 1> <0 0 1> 0.066 255.6
Au (mp-81) <1 0 0> <0 0 1> 0.072 292.1
PbS (mp-21276) <1 0 0> <0 0 1> 0.077 36.5
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.078 146.1
BaTiO3 (mp-5986) <1 0 0> <1 1 1> 0.080 101.8
LiGaO2 (mp-5854) <1 0 0> <1 1 0> 0.083 285.0
ZrO2 (mp-2858) <1 0 -1> <1 1 0> 0.097 285.0
ZnO (mp-2133) <1 1 0> <1 0 0> 0.101 268.7
ZnO (mp-2133) <1 0 0> <1 1 0> 0.104 190.0
Mg (mp-153) <1 0 0> <0 0 1> 0.104 182.6
BaTiO3 (mp-5986) <1 1 0> <1 1 0> 0.114 95.0
ZnSe (mp-1190) <1 0 0> <0 0 1> 0.116 292.1
TeO2 (mp-2125) <1 1 0> <0 0 1> 0.116 292.1
InP (mp-20351) <1 1 0> <1 0 1> 0.125 152.9
LiGaO2 (mp-5854) <0 1 1> <0 0 1> 0.125 219.1
AlN (mp-661) <0 0 1> <0 0 1> 0.130 292.1
SiO2 (mp-6930) <1 1 0> <1 1 0> 0.133 95.0
C (mp-48) <1 1 0> <0 0 1> 0.142 328.6
CdWO4 (mp-19387) <0 1 1> <1 1 1> 0.144 203.5
GaN (mp-804) <1 0 0> <0 0 1> 0.152 182.6
Ga2O3 (mp-886) <1 0 1> <0 0 1> 0.153 182.6
Ga2O3 (mp-886) <1 0 -1> <1 0 1> 0.154 76.5
MgO (mp-1265) <1 1 1> <0 0 1> 0.154 255.6
C (mp-48) <1 0 1> <0 0 1> 0.156 219.1
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.156 109.5
GaAs (mp-2534) <1 0 0> <0 0 1> 0.159 292.1
Mg (mp-153) <1 0 1> <1 0 0> 0.164 134.3
TeO2 (mp-2125) <0 0 1> <0 0 1> 0.166 292.1
InAs (mp-20305) <1 1 0> <1 0 0> 0.170 268.7
AlN (mp-661) <1 1 1> <1 0 0> 0.170 201.5
GaN (mp-804) <1 0 1> <1 0 0> 0.171 134.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
71 44 44 0 0 0
44 71 44 0 0 0
44 44 62 0 0 0
0 0 0 23 0 0
0 0 0 0 23 0
0 0 0 0 0 25
Compliance Tensor Sij (10-12Pa-1)
28.4 -9.6 -13.2 0 0 0
-9.6 28.4 -13.2 0 0 0
-13.2 -13.2 34.6 0 0 0
0 0 0 43.7 0 0
0 0 0 0 43.7 0
0 0 0 0 0 39.3
Shear Modulus GV
19 GPa
Bulk Modulus KV
52 GPa
Shear Modulus GR
17 GPa
Bulk Modulus KR
52 GPa
Shear Modulus GVRH
18 GPa
Bulk Modulus KVRH
52 GPa
Elastic Anisotropy
0.65
Poisson's Ratio
0.35

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 -0.23683 0.00000 0.00000
0.00000 0.00000 0.00000 0.00000 -0.23683 0.00000
0.00000 0.00000 0.00000 0.00000 0.00000 -0.02283
Piezoelectric Modulus ‖eijmax
0.23683 C/m2
Crystallographic Direction vmax
0.00000
1.00000
0.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
7.07 0.00 0.00
0.00 7.07 -0.00
0.00 -0.00 6.79
Dielectric Tensor εij (total)
9.70 0.00 0.00
0.00 9.70 -0.00
0.00 -0.00 9.29
Polycrystalline dielectric constant εpoly
(electronic contribution)
6.97
Polycrystalline dielectric constant εpoly
(total)
9.57
Refractive Index n
2.64
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CdSiAs2 (mp-3078) 0.0401 0.000 3
CdGeP2 (mp-3668) 0.0855 0.000 3
GaAgS2 (mp-5342) 0.0220 0.000 3
MgSiSb2 (mp-1078680) 0.0873 0.048 3
MgSiAs2 (mp-1016197) 0.0133 0.000 3
Cu2SnHgS4 (mp-1025467) 0.1807 0.000 4
CdCu2SnSe4 (mp-16565) 0.1736 0.006 4
CdCu2SnS4 (mp-1078292) 0.1811 0.000 4
ZnAg2SnS4 (mp-1079889) 0.1798 0.000 4
Cu2SnHgSe4 (mp-16566) 0.1738 0.000 4
BC5 (mp-1077743) 0.2143 0.272 2
BC7 (mp-1078935) 0.2085 0.214 2
BC5 (mp-1018649) 0.2256 0.278 2
BC5 (mp-1077125) 0.2056 0.249 2
BC7 (mp-1079046) 0.1825 0.246 2
Sn (mp-949028) 0.2400 0.030 1
Si (mp-971662) 0.2405 0.064 1
C (mp-569517) 0.3803 0.145 1
C (mp-1078845) 0.3527 0.266 1
Ge (mp-1091415) 0.3778 0.014 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Al Ag Se
Final Energy/Atom
-4.0118 eV
Corrected Energy
-33.9821 eV
Uncorrected energy = -32.0941 eV Composition-based energy adjustment (-0.472 eV/atom x 4.0 atoms) = -1.8880 eV Corrected energy = -33.9821 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 604704
  • 28745
  • 604706
Submitted by
User remarks:
  • Silver aluminium selenide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)