AlTlO2

ID:

mp-14105

DOI:

10.17188/1189933


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.440 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.028 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.62 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Al11TlO17 + Tl2O
Band Gap
2.254 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fd3m [227]
Hall
F 4d 2 3 1d
Point Group
m3m
Crystal System
cubic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Cu (mp-30) <1 0 0> <1 0 0> 0.000 65.4
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.000 261.4
KCl (mp-23193) <1 0 0> <1 0 0> 0.001 326.8
Al (mp-134) <1 0 0> <1 0 0> 0.001 65.4
Al (mp-134) <1 1 0> <1 1 0> 0.002 92.4
Al (mp-134) <1 1 1> <1 1 1> 0.002 113.2
MgO (mp-1265) <1 0 0> <1 0 0> 0.002 326.8
SiC (mp-8062) <1 0 0> <1 0 0> 0.003 326.8
TiO2 (mp-390) <0 0 1> <1 0 0> 0.004 130.7
GaSe (mp-1943) <0 0 1> <1 1 1> 0.007 113.2
Ni (mp-23) <1 1 0> <1 1 0> 0.011 277.3
AlN (mp-661) <1 0 1> <1 0 0> 0.012 196.1
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.017 65.4
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.019 92.4
KTaO3 (mp-3614) <1 1 1> <1 1 1> 0.020 113.2
BN (mp-984) <1 0 1> <1 0 0> 0.027 261.4
ZnO (mp-2133) <0 0 1> <1 1 1> 0.029 113.2
PbS (mp-21276) <1 0 0> <1 0 0> 0.030 326.8
C (mp-48) <1 0 1> <1 0 0> 0.035 261.4
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.037 184.9
DyScO3 (mp-31120) <0 1 0> <1 0 0> 0.040 130.7
NaCl (mp-22862) <1 0 0> <1 0 0> 0.041 65.4
CdTe (mp-406) <1 1 0> <1 1 0> 0.044 184.9
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.044 65.4
TbScO3 (mp-31119) <1 0 0> <1 1 0> 0.044 92.4
NaCl (mp-22862) <1 1 0> <1 1 0> 0.045 92.4
TeO2 (mp-2125) <1 1 0> <1 0 0> 0.047 196.1
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.049 92.4
DyScO3 (mp-31120) <1 0 0> <1 1 0> 0.050 92.4
InSb (mp-20012) <1 1 0> <1 1 0> 0.057 184.9
TbScO3 (mp-31119) <0 1 0> <1 0 0> 0.062 130.7
TePb (mp-19717) <1 1 0> <1 1 0> 0.066 184.9
CdS (mp-672) <1 1 1> <1 0 0> 0.073 261.4
GaAs (mp-2534) <1 0 0> <1 0 0> 0.075 65.4
GdScO3 (mp-5690) <1 0 0> <1 1 0> 0.076 92.4
ZnO (mp-2133) <1 0 0> <1 0 0> 0.076 261.4
GaAs (mp-2534) <1 1 0> <1 1 0> 0.083 92.4
Ge (mp-32) <1 0 0> <1 0 0> 0.142 65.4
C (mp-66) <1 0 0> <1 0 0> 0.148 326.8
BaTiO3 (mp-5986) <1 0 1> <1 1 0> 0.148 92.4
ZrO2 (mp-2858) <1 0 1> <1 0 0> 0.154 130.7
BN (mp-984) <1 0 0> <1 0 0> 0.157 196.1
Ge (mp-32) <1 1 0> <1 1 0> 0.158 92.4
MgO (mp-1265) <1 1 0> <1 1 0> 0.161 277.3
Mg (mp-153) <1 1 0> <1 0 0> 0.172 261.4
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.177 65.4
GaTe (mp-542812) <1 0 1> <1 0 0> 0.185 196.1
SiO2 (mp-6930) <1 0 1> <1 1 0> 0.193 277.3
TeO2 (mp-2125) <1 0 0> <1 1 0> 0.197 277.3
SiC (mp-7631) <0 0 1> <1 0 0> 0.202 326.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
118 90 90 0 0 0
90 118 90 0 0 0
90 90 118 0 0 0
0 0 0 62 0 0
0 0 0 0 62 0
0 0 0 0 0 62
Compliance Tensor Sij (10-12Pa-1)
25.5 -11.1 -11.1 0 0 0
-11.1 25.5 -11.1 0 0 0
-11.1 -11.1 25.5 0 0 0
0 0 0 16.2 0 0
0 0 0 0 16.2 0
0 0 0 0 0 16.2
Shear Modulus GV
42 GPa
Bulk Modulus KV
100 GPa
Shear Modulus GR
26 GPa
Bulk Modulus KR
100 GPa
Shear Modulus GVRH
34 GPa
Bulk Modulus KVRH
100 GPa
Elastic Anisotropy
3.29
Poisson's Ratio
0.35

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CsNbN2 (mp-8978) 0.0141 0.008 3
CsScO2 (mp-754826) 0.0141 0.000 3
CsAlO2 (mp-14069) 0.0141 0.000 3
RbAlO2 (mp-14070) 0.0141 0.000 3
RbFeO2 (mp-772592) 0.0141 0.072 3
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Al Tl_d O
Final Energy/Atom
-6.0892 eV
Corrected Energy
-51.5226 eV
-51.5226 eV = -48.7134 eV (uncorrected energy) - 2.8092 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)