Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.793 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.028 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.01 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Ti3Zn2O8 + ZnO
Band Gap
3.049 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3 [148]
Hall
-R 3
Point Group
3
Crystal System
trigonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
WS2 (mp-224) <0 0 1> <0 0 1> 0.000 273.4
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.000 68.4
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.000 273.4
C (mp-48) <0 0 1> <0 0 1> 0.006 68.4
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.008 22.8
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.009 68.4
Mg (mp-153) <0 0 1> <0 0 1> 0.017 273.4
TiO2 (mp-2657) <1 1 1> <0 0 1> 0.017 205.1
Cu (mp-30) <1 1 1> <0 0 1> 0.026 22.8
Te2W (mp-22693) <0 1 0> <1 0 0> 0.030 216.7
Au (mp-81) <1 0 0> <0 0 1> 0.032 364.5
BaTiO3 (mp-5986) <1 0 0> <1 0 0> 0.042 289.0
LiGaO2 (mp-5854) <0 1 1> <1 0 0> 0.044 216.7
Mg (mp-153) <1 0 1> <0 0 1> 0.045 319.0
Au (mp-81) <1 1 1> <0 0 1> 0.049 91.1
CdS (mp-672) <1 0 1> <1 0 1> 0.049 227.2
TePb (mp-19717) <1 1 1> <0 0 1> 0.056 296.2
TiO2 (mp-2657) <1 0 0> <1 1 0> 0.058 125.1
Cu (mp-30) <1 0 0> <0 0 1> 0.058 250.6
CaF2 (mp-2741) <1 1 1> <0 0 1> 0.058 159.5
AlN (mp-661) <1 1 1> <1 1 1> 0.062 254.4
SiC (mp-8062) <1 1 1> <0 0 1> 0.069 296.2
AlN (mp-661) <0 0 1> <0 0 1> 0.075 159.5
AlN (mp-661) <1 0 0> <0 0 1> 0.076 205.1
Te2Mo (mp-602) <1 0 0> <1 0 0> 0.082 216.7
BaTiO3 (mp-5986) <1 1 1> <1 0 0> 0.091 144.5
NdGaO3 (mp-3196) <0 1 0> <0 0 1> 0.096 341.8
SiC (mp-7631) <0 0 1> <0 0 1> 0.107 159.5
ZnO (mp-2133) <1 0 1> <0 0 1> 0.109 296.2
GaP (mp-2490) <1 1 1> <0 0 1> 0.115 159.5
SiC (mp-11714) <0 0 1> <0 0 1> 0.118 159.5
GaP (mp-2490) <1 1 0> <0 0 1> 0.120 341.8
SiC (mp-11714) <1 1 0> <0 0 1> 0.125 273.4
Ag (mp-124) <1 1 1> <0 0 1> 0.132 91.1
Ni (mp-23) <1 1 1> <0 0 1> 0.141 273.4
BN (mp-984) <0 0 1> <0 0 1> 0.143 205.1
AlN (mp-661) <1 0 1> <1 0 1> 0.146 303.0
Ag (mp-124) <1 1 0> <0 0 1> 0.152 364.5
CaF2 (mp-2741) <1 1 0> <0 0 1> 0.152 341.8
Fe2O3 (mp-24972) <1 0 1> <1 0 1> 0.168 75.7
CdWO4 (mp-19387) <0 0 1> <0 0 1> 0.171 91.1
Si (mp-149) <1 1 0> <0 0 1> 0.179 341.8
CeO2 (mp-20194) <1 1 0> <0 0 1> 0.186 341.8
GaN (mp-804) <0 0 1> <0 0 1> 0.192 273.4
LiTaO3 (mp-3666) <1 0 1> <1 0 1> 0.201 75.7
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.204 205.1
Fe2O3 (mp-24972) <1 1 1> <1 1 1> 0.206 127.2
LiTaO3 (mp-3666) <1 1 1> <1 1 1> 0.218 127.2
Fe2O3 (mp-24972) <1 0 0> <1 0 0> 0.227 72.2
Fe2O3 (mp-24972) <1 1 0> <1 1 0> 0.227 125.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
308 154 99 20 -7 0
154 308 99 -20 7 0
99 99 241 0 0 0
20 -20 0 31 0 7
-7 7 0 0 31 20
0 0 0 7 20 77
Compliance Tensor Sij (10-12Pa-1)
5.3 -2.7 -1.1 -5.3 1.8 0
-2.7 5.3 -1.1 5.3 -1.8 0
-1.1 -1.1 5 0 0 0
-5.3 5.3 0 40.2 0 -3.6
1.8 -1.8 0 0 40.2 -10.6
0 0 0 -3.6 -10.6 16.1
Shear Modulus GV
61 GPa
Bulk Modulus KV
174 GPa
Shear Modulus GR
40 GPa
Bulk Modulus KR
168 GPa
Shear Modulus GVRH
51 GPa
Bulk Modulus KVRH
171 GPa
Elastic Anisotropy
2.65
Poisson's Ratio
0.36

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TiMnO3 (mp-819025) 0.1418 0.000 3
TiCoO3 (mp-19424) 0.1763 0.003 3
LiNbO3 (mp-1078377) 0.1296 0.021 3
TiMnO3 (mp-19082) 0.1429 0.000 3
TiFeO3 (mp-19417) 0.1773 0.012 3
Li3Nb4NiO12 (mp-772009) 0.3210 0.080 4
Li3Nb4FeO12 (mp-771984) 0.3124 0.051 4
Li13Nb14ZnO42 (mp-768142) 0.3088 0.008 4
InNi2SbO6 (mp-1078367) 0.3369 0.000 4
LiCoOF2 (mp-849507) 0.3136 0.151 4
In2S3 (mp-22375) 0.3985 0.023 2
Sc2O3 (mp-755313) 0.3714 0.039 2
Y2O3 (mp-754759) 0.3884 0.051 2
Ga2O3 (mp-1243) 0.3545 0.030 2
In2O3 (mp-22323) 0.3728 0.029 2
Li4NbTe2WO12 (mp-763988) 0.6624 0.075 5
Li4Fe2TeWO12 (mp-768021) 0.5100 0.085 5
Li4Cr2TeWO12 (mp-775566) 0.6081 0.080 5
Li4Mn2TeWO12 (mp-768044) 0.5870 0.058 5
Li4V2CrTeO12 (mp-775632) 0.6560 0.104 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

The Zn(ZrxTi1x)O3 samples with x=00.1 were prepared by a conventional solid-state reaction method using ZnO, TiO2, and ZrO2 powders as the starting materials with a purity of 99.99% supplied from [...]
ZnTiO3 powders were prepared via a chemical route with A.R Zn5(CO3)2(OH)6 (zinc hydroxide carbonate) and TiO2 (anatase, >99.0%, 3080nm). Zinc hydroxide carbonate was heat-treated at 350C for 2h [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition TiZnO3.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ti_pv Zn O
Final Energy/Atom
-7.1802 eV
Corrected Energy
-75.9238 eV
Uncorrected energy = -71.8018 eV Composition-based energy adjustment (-0.687 eV/atom x 6.0 atoms) = -4.1220 eV Corrected energy = -75.9238 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 22382
  • 262709
Submitted by
User remarks:
  • Zinc titanate
  • Ecandrewsite

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)