Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingUnknown |
Formation Energy / Atom-0.950 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.482 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFdd2 [43] |
HallF 2 2d |
Point Groupmm2 |
Crystal Systemorthorhombic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 93.7 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 281.2 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 115.0 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 281.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 187.4 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 281.2 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 115.0 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 115.0 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 281.2 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 229.9 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 93.7 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 229.9 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 187.4 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 93.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 229.9 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 281.2 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 93.7 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 229.9 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 281.2 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 281.2 |
LaF3 (mp-905) | <0 0 1> | <0 1 0> | 229.9 |
PbSe (mp-2201) | <1 0 0> | <0 1 0> | 115.0 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 281.2 |
Ga2O3 (mp-886) | <1 0 -1> | <0 0 1> | 187.4 |
Ga2O3 (mp-886) | <1 0 1> | <0 0 1> | 93.7 |
Ga2O3 (mp-886) | <1 1 -1> | <0 1 0> | 229.9 |
CdSe (mp-2691) | <1 0 0> | <0 1 0> | 115.0 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 281.2 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 281.2 |
SiC (mp-8062) | <1 0 0> | <0 1 0> | 115.0 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 187.4 |
MgF2 (mp-1249) | <1 0 0> | <0 1 0> | 115.0 |
MgF2 (mp-1249) | <1 0 1> | <0 0 1> | 187.4 |
ZnO (mp-2133) | <1 0 1> | <0 0 1> | 281.2 |
GaSb (mp-1156) | <1 0 0> | <0 1 0> | 115.0 |
GaSb (mp-1156) | <1 1 0> | <0 0 1> | 281.2 |
GaTe (mp-542812) | <0 0 1> | <0 1 0> | 229.9 |
GaTe (mp-542812) | <1 0 -1> | <0 1 0> | 229.9 |
LiAlO2 (mp-3427) | <1 0 0> | <0 1 0> | 229.9 |
LiAlO2 (mp-3427) | <1 1 0> | <0 0 1> | 93.7 |
ZnTe (mp-2176) | <1 0 0> | <0 1 0> | 115.0 |
ZnTe (mp-2176) | <1 1 0> | <0 0 1> | 281.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
8.58 | 0.00 | -0.45 |
-0.00 | 10.90 | 0.00 |
-0.47 | -0.00 | 9.79 |
Dielectric Tensor εij (total) |
||
---|---|---|
15.77 | 0.00 | -2.22 |
-0.00 | 20.87 | 0.00 |
-2.23 | 0.00 | 21.66 |
Polycrystalline dielectric constant
εpoly∞
9.75
|
Polycrystalline dielectric constant
εpoly
19.43
|
Refractive Index n3.12 |
Potentially ferroelectric?False |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points66 |
U Values-- |
PseudopotentialsVASP PAW: P Ba_sv |
Final Energy/Atom-4.8644 eV |
Corrected Energy-68.1012 eV
-68.1012 eV = -68.1012 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)