Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.133 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.41 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbca [61] |
Hall-P 2ac 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological ClassificationTI*
|
SubclassificationNLC†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 151.5 |
MgF2 (mp-1249) | <0 0 1> | <0 1 1> | 198.3 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 170.7 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 170.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 244.1 |
Al (mp-134) | <1 0 0> | <1 1 0> | 244.1 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 198.3 |
GaAs (mp-2534) | <1 1 1> | <0 1 0> | 170.7 |
TiO2 (mp-2657) | <1 0 0> | <1 1 1> | 264.2 |
Ni (mp-23) | <1 0 0> | <0 1 1> | 99.2 |
ZnO (mp-2133) | <1 1 1> | <0 0 1> | 252.5 |
Cu (mp-30) | <1 0 0> | <1 0 0> | 261.8 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 256.0 |
Ge (mp-32) | <1 1 1> | <0 1 0> | 170.7 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 1> | 297.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 151.5 |
CdWO4 (mp-19387) | <0 0 1> | <1 1 0> | 122.1 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 151.5 |
NaCl (mp-22862) | <1 1 1> | <0 1 0> | 170.7 |
CdWO4 (mp-19387) | <0 1 0> | <1 0 0> | 261.8 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 87.3 |
Fe3O4 (mp-19306) | <1 1 1> | <0 1 0> | 256.0 |
MgF2 (mp-1249) | <1 1 0> | <1 1 1> | 264.2 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 151.5 |
SiC (mp-11714) | <1 0 1> | <0 1 0> | 256.0 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 174.5 |
TiO2 (mp-2657) | <0 0 1> | <0 1 1> | 198.3 |
ZnO (mp-2133) | <1 0 0> | <1 1 1> | 264.2 |
Al2O3 (mp-1143) | <1 0 1> | <1 0 1> | 201.6 |
SiC (mp-8062) | <1 1 1> | <1 0 0> | 261.8 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 303.0 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 303.0 |
BN (mp-984) | <1 0 1> | <1 1 1> | 264.2 |
MgO (mp-1265) | <1 1 1> | <0 1 0> | 256.0 |
C (mp-66) | <1 0 0> | <0 0 1> | 50.5 |
Ag (mp-124) | <1 1 1> | <0 1 1> | 297.5 |
C (mp-66) | <1 1 0> | <0 0 1> | 252.5 |
LaF3 (mp-905) | <1 0 0> | <1 0 0> | 261.8 |
PbSe (mp-2201) | <1 0 0> | <0 1 1> | 198.3 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 252.5 |
CdWO4 (mp-19387) | <1 0 0> | <0 1 0> | 256.0 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 1> | 297.5 |
GaSb (mp-1156) | <1 0 0> | <0 1 1> | 198.3 |
Au (mp-81) | <1 1 1> | <1 1 0> | 122.1 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 0> | 256.0 |
C (mp-48) | <1 0 1> | <1 0 0> | 261.8 |
SiC (mp-11714) | <1 1 0> | <1 1 1> | 264.2 |
CdSe (mp-2691) | <1 0 0> | <0 1 1> | 198.3 |
ZnO (mp-2133) | <1 0 1> | <0 1 0> | 256.0 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 256.0 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
105 | 38 | 50 | 0 | 0 | 0 |
38 | 68 | 44 | 0 | 0 | 0 |
50 | 44 | 107 | 0 | 0 | 0 |
0 | 0 | 0 | 15 | 0 | 0 |
0 | 0 | 0 | 0 | 14 | 0 |
0 | 0 | 0 | 0 | 0 | 15 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
13.2 | -4.4 | -4.4 | 0 | 0 | 0 |
-4.4 | 21.7 | -6.9 | 0 | 0 | 0 |
-4.4 | -6.9 | 14.3 | 0 | 0 | 0 |
0 | 0 | 0 | 64.8 | 0 | 0 |
0 | 0 | 0 | 0 | 71.8 | 0 |
0 | 0 | 0 | 0 | 0 | 67.3 |
Shear Modulus GV19 GPa |
Bulk Modulus KV60 GPa |
Shear Modulus GR17 GPa |
Bulk Modulus KR56 GPa |
Shear Modulus GVRH18 GPa |
Bulk Modulus KVRH58 GPa |
Elastic Anisotropy0.50 |
Poisson's Ratio0.36 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CoGeTe (mp-3715) | 0.5668 | 0.000 | 3 |
Na3(FeSe2)2 (mp-505443) | 0.6341 | 0.121 | 3 |
Li3(FeS2)2 (mp-753818) | 0.6303 | 0.276 | 3 |
SiSbPt (mp-11152) | 0.6344 | 0.000 | 3 |
Ca3(AlAs2)2 (mp-28304) | 0.5935 | 0.118 | 3 |
Sr2Li2NiO4 (mp-769674) | 0.7185 | 0.091 | 4 |
CoSb2 (mp-755) | 0.6194 | 0.002 | 2 |
Yb2S3 (mp-632532) | 0.6019 | 0.143 | 2 |
Bi2Rh (mp-23217) | 0.6066 | 0.000 | 2 |
Sb2Rh (mp-2682) | 0.5772 | 0.000 | 2 |
Sb2Ir (mp-1247) | 0.5883 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sn_d Au |
Final Energy/Atom-3.8973 eV |
Corrected Energy-93.5349 eV
-93.5349 eV = -93.5349 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)