Final Magnetic Moment0.044 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.680 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.57 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.284 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP42/n [86] |
HallP 4n 1n |
Point Group4/m |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CdTe (mp-406) | <1 1 0> | <1 0 1> | 181.7 |
MgO (mp-1265) | <1 0 0> | <1 0 1> | 181.7 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 87.2 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 261.6 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 174.4 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 261.6 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 87.2 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 181.7 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 87.2 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 159.4 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 87.2 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 174.4 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 261.6 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 87.2 |
InSb (mp-20012) | <1 1 0> | <1 0 1> | 181.7 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 261.6 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 0> | 159.4 |
Si (mp-149) | <1 1 1> | <0 0 1> | 261.6 |
Au (mp-81) | <1 0 0> | <0 0 1> | 87.2 |
WS2 (mp-224) | <0 0 1> | <1 0 0> | 159.4 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 174.4 |
MgF2 (mp-1249) | <0 0 1> | <0 0 1> | 87.2 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 87.2 |
MgF2 (mp-1249) | <1 0 1> | <1 0 0> | 159.4 |
MgF2 (mp-1249) | <1 1 1> | <1 0 1> | 181.7 |
Al2O3 (mp-1143) | <0 0 1> | <1 0 0> | 159.4 |
Al2O3 (mp-1143) | <1 0 1> | <0 0 1> | 261.6 |
CaF2 (mp-2741) | <1 1 1> | <0 0 1> | 261.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZrVSi (mp-5541) | 0.6803 | 0.000 | 3 |
ThAsSe (mp-1019357) | 0.6958 | 0.000 | 3 |
HfVGe (mp-1018726) | 0.6776 | 0.000 | 3 |
HfVSi (mp-1018720) | 0.6776 | 0.000 | 3 |
ThPS (mp-12876) | 0.7055 | 0.000 | 3 |
La10Se19 (mp-8866) | 0.1298 | 0.000 | 2 |
Ce10Te19 (mp-645273) | 0.3905 | 0.166 | 2 |
Ce10Se19 (mp-652044) | 0.2785 | 0.000 | 2 |
Pr10Se19 (mp-14613) | 0.0366 | 0.000 | 2 |
Sm10Se19 (mp-29832) | 0.0425 | 0.002 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nd_3 Se |
Final Energy/Atom-5.6145 eV |
Corrected Energy-325.6435 eV
-325.6435 eV = -325.6435 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)