material

ZrSi2

ID:

mp-1515

DOI:

10.17188/1191039


Tags: Zirconium silicide (1/2) Zirconium silicide(-II)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.649 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.85 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Cmcm [63]
Hall
-C 2c 2
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 16772 from Topological Materials Database
Topological Classification
TI*
Subclassification
NLC
* Topological insulator
No Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
KCl (mp-23193) <1 1 0> <1 0 1> 0.009 232.1
TiO2 (mp-2657) <1 0 1> <0 1 0> 0.014 205.0
LiAlO2 (mp-3427) <0 0 1> <0 1 0> 0.017 27.3
GaN (mp-804) <1 1 0> <1 0 1> 0.027 232.1
CsI (mp-614603) <1 0 0> <0 1 0> 0.036 123.0
LiTaO3 (mp-3666) <1 0 0> <0 1 0> 0.037 218.7
Mg (mp-153) <1 1 0> <1 0 1> 0.045 232.1
YAlO3 (mp-3792) <0 1 0> <1 0 1> 0.049 77.4
NdGaO3 (mp-3196) <1 1 0> <0 1 0> 0.055 123.0
InAs (mp-20305) <1 0 0> <0 1 0> 0.058 341.7
Te2Mo (mp-602) <1 1 0> <1 1 0> 0.066 281.2
ZnTe (mp-2176) <1 0 0> <0 1 0> 0.072 341.7
MgF2 (mp-1249) <0 0 1> <0 1 0> 0.073 109.3
SrTiO3 (mp-4651) <0 0 1> <0 1 0> 0.080 123.0
C (mp-48) <1 1 1> <1 1 1> 0.080 235.7
InSb (mp-20012) <1 0 0> <0 1 0> 0.090 177.7
GaN (mp-804) <1 1 1> <0 1 0> 0.098 123.0
TiO2 (mp-2657) <0 0 1> <0 1 0> 0.108 109.3
CaF2 (mp-2741) <1 0 0> <0 1 0> 0.110 123.0
CdTe (mp-406) <1 0 0> <0 1 0> 0.112 177.7
PbS (mp-21276) <1 1 0> <1 0 1> 0.114 154.8
ZrO2 (mp-2858) <0 0 1> <0 1 0> 0.119 27.3
Ni (mp-23) <1 1 0> <1 0 1> 0.121 154.8
MoSe2 (mp-1634) <1 0 0> <0 1 0> 0.122 205.0
LiAlO2 (mp-3427) <1 0 0> <0 1 0> 0.133 164.0
C (mp-48) <0 0 1> <0 1 0> 0.141 109.3
LiAlO2 (mp-3427) <1 1 1> <0 1 0> 0.152 54.7
Al (mp-134) <1 1 0> <0 1 0> 0.159 300.7
LiGaO2 (mp-5854) <1 0 1> <0 1 0> 0.161 136.7
BN (mp-984) <1 1 1> <1 1 1> 0.168 235.7
SrTiO3 (mp-4651) <1 1 0> <0 1 0> 0.171 123.0
LiNbO3 (mp-3731) <1 0 1> <1 1 1> 0.174 78.6
Ni (mp-23) <1 0 0> <0 1 0> 0.175 109.3
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.179 224.9
NdGaO3 (mp-3196) <0 0 1> <0 1 0> 0.179 123.0
Ag (mp-124) <1 0 0> <0 1 0> 0.181 68.3
KTaO3 (mp-3614) <1 1 0> <0 1 0> 0.183 300.7
GaP (mp-2490) <1 0 0> <0 1 0> 0.184 123.0
ZrO2 (mp-2858) <1 1 -1> <1 1 0> 0.195 224.9
CdWO4 (mp-19387) <1 0 0> <1 0 1> 0.210 154.8
Mg (mp-153) <1 0 1> <0 1 0> 0.216 205.0
SiC (mp-8062) <1 1 1> <0 1 0> 0.222 300.7
LiTaO3 (mp-3666) <0 0 1> <1 0 1> 0.224 232.1
SiC (mp-7631) <0 0 1> <0 1 0> 0.235 150.4
Mg (mp-153) <1 1 1> <0 1 0> 0.239 123.0
SiC (mp-11714) <0 0 1> <0 1 0> 0.241 150.4
GaTe (mp-542812) <1 0 0> <0 1 0> 0.246 314.4
MgO (mp-1265) <1 1 1> <1 0 1> 0.254 154.8
CdS (mp-672) <0 0 1> <1 0 0> 0.262 109.1
Si (mp-149) <1 1 0> <1 1 0> 0.262 168.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
232 74 85 0 0 0
74 183 66 0 0 0
85 66 276 0 0 0
0 0 0 105 0 0
0 0 0 0 121 0
0 0 0 0 0 107
Compliance Tensor Sij (10-12Pa-1)
5.3 -1.7 -1.2 0 0 0
-1.7 6.5 -1 0 0 0
-1.2 -1 4.2 0 0 0
0 0 0 9.5 0 0
0 0 0 0 8.3 0
0 0 0 0 0 9.4
Shear Modulus GV
98 GPa
Bulk Modulus KV
127 GPa
Shear Modulus GR
93 GPa
Bulk Modulus KR
123 GPa
Shear Modulus GVRH
95 GPa
Bulk Modulus KVRH
125 GPa
Elastic Anisotropy
0.29
Poisson's Ratio
0.20

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TmSnGe (mp-1025129) 0.4777 0.000 3
ScCoSi (mp-1024998) 0.4447 0.751 3
ErSnGe (mp-1071492) 0.5152 0.000 3
TbSnGe (mp-1077556) 0.4509 0.000 3
DySnGe (mp-1080405) 0.4059 0.000 3
LuGe2 (mp-973906) 0.2262 0.000 2
ThGe2 (mp-16372) 0.3064 0.033 2
ZrGe2 (mp-2430) 0.2728 0.007 2
TmGe2 (mp-13037) 0.2260 0.000 2
HfSi2 (mp-1069) 0.0548 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Zr_sv Si
Final Energy/Atom
-7.1139 eV
Corrected Energy
-42.6834 eV
-42.6834 eV = -42.6834 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 652610
  • 652606
  • 26758
  • 16772
  • 44871
  • 95179
Submitted by
User remarks:
  • Zirconium silicide (1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)