Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.012 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.022 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.51 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToAg2GeO3 + Ag2O |
Band Gap0.011 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 213.2 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 169.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 169.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 339.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 56.5 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 56.5 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 90.4 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 169.5 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 271.2 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 189.7 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 189.7 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 56.5 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 213.2 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 176.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 56.5 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 282.5 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 282.5 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 189.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 90.4 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 106.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 180.8 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 271.2 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 189.7 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 282.5 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 271.2 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 189.7 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 271.2 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 166.8 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 180.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 339.0 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 226.0 |
GaSe (mp-1943) | <0 0 1> | <1 0 1> | 176.3 |
BN (mp-984) | <0 0 1> | <0 1 0> | 180.8 |
BN (mp-984) | <1 0 0> | <0 1 0> | 271.2 |
BN (mp-984) | <1 0 1> | <0 0 1> | 339.0 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 282.5 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 282.5 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 282.5 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 56.5 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 169.5 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 106.6 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 90.4 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 339.0 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 189.7 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 226.0 |
TeO2 (mp-2125) | <0 1 0> | <0 1 0> | 271.2 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 226.0 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 339.0 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 282.5 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 282.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2Cr2O7 (mp-772666) | 0.5423 | 0.079 | 3 |
Si2Ag6O7 (mp-541728) | 0.3607 | 0.047 | 3 |
Ag4GeO4 (mp-560342) | 0.4484 | 0.012 | 3 |
Hg3AsO4 (mp-556339) | 0.5511 | 0.000 | 3 |
Ag8Ge3O10 (mp-679950) | 0.4081 | 0.022 | 3 |
LiSiBiO4 (mp-766196) | 0.5704 | 0.060 | 4 |
SiAg5ClO4 (mp-647305) | 0.5029 | 0.027 | 4 |
RbNa11(WN3)4 (mp-569098) | 0.5871 | 0.006 | 4 |
LiSnPO4 (mp-757885) | 0.5960 | 0.078 | 4 |
LiSnPO4 (mp-757106) | 0.5021 | 0.069 | 4 |
K2LiVPO6 (mp-764301) | 0.5701 | 0.080 | 5 |
LiFe2P2HO8 (mp-763773) | 0.5787 | 0.024 | 5 |
NaZnSiHO4 (mp-699219) | 0.6508 | 0.000 | 5 |
MnZn2Si(HO3)2 (mp-745154) | 0.6326 | 0.132 | 5 |
Li2SbSO4F3 (mp-769153) | 0.6481 | 0.069 | 5 |
Na2TeHSO5F3 (mp-696485) | 0.6569 | 0.016 | 6 |
Na3CaAl3Si3CO15 (mp-705635) | 0.7494 | 0.327 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ag Ge_d O |
Final Energy/Atom-4.7428 eV |
Corrected Energy-304.2313 eV
-304.2313 eV = -284.5672 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)