material

Mo2C

ID:

mp-1552

DOI:

10.17188/1191211


Tags: Molybdenum carbide (2/1) - zeta Molybdenum carbide (2/1) - alpha Molybdenum carbide (2/1)

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.113 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.94 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pbcn [60]
Hall
-P 2n 2ab
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 43322 from Topological Materials Database
Topological Classification
TI*
Subclassification
NLC
* Topological insulator
No Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Te2W (mp-22693) <0 1 0> <1 0 1> 0.002 161.8
LiAlO2 (mp-3427) <1 0 0> <0 0 1> 0.023 99.7
TiO2 (mp-390) <1 0 1> <0 0 1> 0.024 199.3
BN (mp-984) <1 1 0> <1 0 1> 0.034 202.2
Mg (mp-153) <1 1 0> <0 0 1> 0.048 174.4
Mg (mp-153) <1 0 0> <0 0 1> 0.054 49.8
KP(HO2)2 (mp-23959) <0 1 1> <1 1 0> 0.056 215.0
DyScO3 (mp-31120) <1 0 0> <0 1 1> 0.080 228.9
CdS (mp-672) <1 0 1> <1 0 1> 0.090 161.8
GdScO3 (mp-5690) <0 1 0> <1 0 0> 0.091 222.9
TiO2 (mp-2657) <1 1 1> <0 0 1> 0.104 174.4
YAlO3 (mp-3792) <0 1 1> <1 0 0> 0.137 95.5
Fe3O4 (mp-19306) <1 1 1> <1 0 0> 0.139 127.4
TbScO3 (mp-31119) <1 0 0> <0 1 1> 0.151 228.9
BaTiO3 (mp-5986) <0 0 1> <0 1 1> 0.153 190.8
AlN (mp-661) <1 1 0> <0 0 1> 0.166 323.9
LiNbO3 (mp-3731) <0 0 1> <1 0 0> 0.166 95.5
GdScO3 (mp-5690) <1 1 1> <1 0 0> 0.171 286.6
TbScO3 (mp-31119) <1 1 0> <0 1 1> 0.173 190.8
KCl (mp-23193) <1 1 1> <1 0 0> 0.180 286.6
GaN (mp-804) <0 0 1> <1 1 0> 0.194 172.0
Mg (mp-153) <1 1 1> <1 1 0> 0.195 301.0
ZrO2 (mp-2858) <1 0 1> <1 0 0> 0.218 127.4
GaP (mp-2490) <1 0 0> <1 0 1> 0.221 121.3
Al2O3 (mp-1143) <1 0 0> <0 0 1> 0.227 124.6
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.228 222.9
NdGaO3 (mp-3196) <1 1 0> <1 0 1> 0.230 121.3
LiNbO3 (mp-3731) <1 0 0> <0 0 1> 0.236 74.8
GaSe (mp-1943) <0 0 1> <1 0 1> 0.241 202.2
CaF2 (mp-2741) <1 0 0> <1 0 1> 0.243 121.3
GdScO3 (mp-5690) <1 1 0> <0 1 1> 0.246 190.8
PbS (mp-21276) <1 0 0> <0 1 0> 0.255 144.4
ZnO (mp-2133) <1 0 0> <1 0 1> 0.260 121.3
MgO (mp-1265) <1 0 0> <0 1 0> 0.264 144.4
CdS (mp-672) <1 1 1> <1 1 0> 0.267 258.0
TbScO3 (mp-31119) <1 1 1> <1 0 0> 0.268 286.6
InSb (mp-20012) <1 1 1> <0 1 0> 0.269 231.1
KCl (mp-23193) <1 1 0> <1 0 0> 0.279 286.6
WS2 (mp-224) <1 0 1> <0 1 1> 0.294 228.9
CdTe (mp-406) <1 1 1> <0 1 0> 0.305 231.1
LiAlO2 (mp-3427) <1 0 1> <1 0 0> 0.309 127.4
ZnSe (mp-1190) <1 1 1> <0 1 1> 0.315 114.5
GaAs (mp-2534) <1 1 1> <0 1 1> 0.317 114.5
KP(HO2)2 (mp-23959) <0 1 0> <1 1 0> 0.323 301.0
WS2 (mp-224) <1 0 0> <0 0 1> 0.336 224.3
Ge (mp-32) <1 1 1> <0 1 1> 0.362 114.5
LiTaO3 (mp-3666) <0 0 1> <1 0 0> 0.364 95.5
Ga2O3 (mp-886) <1 0 0> <0 1 0> 0.364 144.4
SrTiO3 (mp-4651) <1 0 0> <1 0 0> 0.364 222.9
LiNbO3 (mp-3731) <1 1 0> <0 1 0> 0.379 260.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
488 169 226 0 0 0
169 489 216 0 0 0
226 216 453 0 0 0
0 0 0 179 0 0
0 0 0 0 167 0
0 0 0 0 0 139
Compliance Tensor Sij (10-12Pa-1)
2.7 -0.4 -1.2 0 0 0
-0.4 2.7 -1.1 0 0 0
-1.2 -1.1 3.3 0 0 0
0 0 0 5.6 0 0
0 0 0 0 6 0
0 0 0 0 0 7.2
Shear Modulus GV
152 GPa
Bulk Modulus KV
294 GPa
Shear Modulus GR
148 GPa
Bulk Modulus KR
294 GPa
Shear Modulus GVRH
150 GPa
Bulk Modulus KVRH
294 GPa
Elastic Anisotropy
0.14
Poisson's Ratio
0.28

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Sr2CaI6 (mp-754710) 0.1624 0.041 3
SrCa2I6 (mp-754517) 0.1849 0.033 3
BaSr2I6 (mp-754212) 0.2151 0.014 3
Ba2SrI6 (mp-754196) 0.2254 0.039 3
SrCaI4 (mp-754885) 0.2294 0.046 3
LiGaPdF6 (mp-9245) 0.4708 0.012 4
LiV2OF5 (mp-765048) 0.5088 0.058 4
Li2NbOF5 (mp-756639) 0.4950 0.010 4
LiMnFeF6 (mp-566418) 0.4864 0.000 4
LiTiMnF6 (mp-556715) 0.4618 0.025 4
V2N (mp-684903) 0.1332 0.000 2
Mn2N (mp-9981) 0.1321 0.000 2
V2C (mp-20648) 0.1396 0.000 2
W2C (mp-567397) 0.1416 0.083 2
W2C (mp-2034) 0.0598 0.065 2
Li4MnCr(WO6)2 (mp-761370) 0.7403 0.071 5
Li4ZrNb(TeO6)2 (mp-756177) 0.6350 0.058 5
Li4Cr2TeWO12 (mp-775566) 0.7106 0.080 5
Li4Mn2TeWO12 (mp-768044) 0.7193 0.058 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Mo_pv C
Final Energy/Atom
-10.4192 eV
Corrected Energy
-125.0305 eV
Uncorrected energy = -125.0305 eV Corrected energy = -125.0305 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 43322
  • 600624
  • 246147
  • 65701
  • 246148
  • 246146
Submitted by
User remarks:
  • Molybdenum carbide (2/1) - alpha