material

V3Sb

ID:

mp-1555

DOI:

10.17188/1191232


Tags: Vanadium antimonide (1/3) Vanadium antimonide (3/1)

Material Details

Final Magnetic Moment
0.004 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.216 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.59 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3n [223]
Hall
-P 4n 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 52330 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.000 194.8
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.000 121.8
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.000 68.9
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.003 219.2
NaCl (mp-22862) <1 1 1> <1 1 1> 0.005 168.7
NaCl (mp-22862) <1 1 0> <1 1 0> 0.005 137.8
CdTe (mp-406) <1 0 0> <1 0 0> 0.006 219.2
Cu (mp-30) <1 1 1> <1 1 1> 0.007 295.3
Fe3O4 (mp-19306) <1 1 1> <1 1 1> 0.011 126.5
Fe3O4 (mp-19306) <1 1 0> <1 1 0> 0.011 103.3
InSb (mp-20012) <1 0 0> <1 0 0> 0.014 219.2
AlN (mp-661) <1 0 1> <1 0 0> 0.016 267.9
GaP (mp-2490) <1 0 0> <1 0 0> 0.016 121.8
BN (mp-984) <0 0 1> <1 1 1> 0.018 168.7
Al (mp-134) <1 1 0> <1 1 0> 0.021 68.9
PbSe (mp-2201) <1 0 0> <1 0 0> 0.024 194.8
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.032 121.8
Fe2O3 (mp-24972) <0 0 1> <1 1 1> 0.038 295.3
WS2 (mp-224) <0 0 1> <1 1 1> 0.048 168.7
MoS2 (mp-1434) <0 0 1> <1 1 1> 0.049 168.7
Mg (mp-153) <1 1 1> <1 0 0> 0.050 121.8
Ni (mp-23) <1 1 1> <1 0 0> 0.051 170.5
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.052 310.0
C (mp-48) <1 0 1> <1 1 0> 0.054 241.1
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.055 219.2
GaSb (mp-1156) <1 0 0> <1 0 0> 0.055 194.8
C (mp-48) <1 0 0> <1 0 0> 0.057 267.9
MgO (mp-1265) <1 1 1> <1 1 1> 0.062 126.5
MgO (mp-1265) <1 1 0> <1 1 0> 0.063 103.3
GaN (mp-804) <0 0 1> <1 1 1> 0.073 168.7
CdSe (mp-2691) <1 0 0> <1 0 0> 0.089 194.8
YAlO3 (mp-3792) <0 1 1> <1 1 1> 0.099 337.5
ZnO (mp-2133) <1 0 1> <1 1 1> 0.105 295.3
Ni (mp-23) <1 1 0> <1 1 0> 0.107 34.4
GaN (mp-804) <1 1 1> <1 0 0> 0.109 121.8
Ni (mp-23) <1 0 0> <1 0 0> 0.112 24.4
LiF (mp-1138) <1 0 0> <1 0 0> 0.122 219.2
Mg (mp-153) <0 0 1> <1 1 1> 0.125 168.7
TePb (mp-19717) <1 1 1> <1 1 1> 0.127 295.3
CdWO4 (mp-19387) <1 0 0> <1 1 1> 0.130 126.5
LiGaO2 (mp-5854) <1 1 1> <1 1 0> 0.150 275.5
GdScO3 (mp-5690) <0 1 1> <1 1 0> 0.152 275.5
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 0.156 219.2
C (mp-48) <0 0 1> <1 0 0> 0.157 170.5
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.171 194.8
PbS (mp-21276) <1 1 0> <1 1 0> 0.173 103.3
ZnO (mp-2133) <1 1 0> <1 1 0> 0.198 275.5
CsI (mp-614603) <1 0 0> <1 0 0> 0.209 121.8
ZrO2 (mp-2858) <0 1 0> <1 0 0> 0.210 365.3
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.218 126.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
315 110 110 0 0 0
110 315 110 0 0 0
110 110 315 0 0 0
0 0 0 67 0 0
0 0 0 0 67 0
0 0 0 0 0 67
Compliance Tensor Sij (10-12Pa-1)
3.9 -1 -1 0 0 0
-1 3.9 -1 0 0 0
-1 -1 3.9 0 0 0
0 0 0 15 0 0
0 0 0 0 15 0
0 0 0 0 0 15
Shear Modulus GV
81 GPa
Bulk Modulus KV
178 GPa
Shear Modulus GR
78 GPa
Bulk Modulus KR
178 GPa
Shear Modulus GVRH
79 GPa
Bulk Modulus KVRH
178 GPa
Elastic Anisotropy
0.22
Poisson's Ratio
0.31

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Nb3In (mp-1078807) 0.0000 0.032 2
UH3 (mp-24659) 0.0000 0.000 2
V3Sn (mp-21342) 0.0000 0.000 2
Cr3Ge (mp-20685) 0.0000 0.000 2
Tl3Ir (mp-1080016) 0.0000 0.539 2
Cs (mp-949029) 0.0000 0.047 1
F2 (mp-21848) 0.0000 0.000 1
Rb (mp-974620) 0.0000 0.036 1
Cr (mp-17) 0.0000 0.085 1
W (mp-11334) 0.0000 0.087 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: V_pv Sb
Final Energy/Atom
-8.0604 eV
Corrected Energy
-64.4830 eV
-64.4830 eV = -64.4830 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 651731
  • 52330
  • 106037
  • 651717
Submitted by
User remarks:
  • Vanadium antimonide (3/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)