Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.001 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.001 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.23 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLa |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 195.4 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 118.4 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 83.7 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 78.9 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 276.3 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 251.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 139.5 |
BaF2 (mp-1029) | <1 0 0> | <1 1 1> | 241.7 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 118.4 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 193.4 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 145.0 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 83.7 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 118.4 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 193.4 |
SiO2 (mp-6930) | <1 0 0> | <1 1 1> | 338.4 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 315.8 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 334.9 |
KCl (mp-23193) | <1 0 0> | <1 1 1> | 241.7 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 118.4 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 139.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 251.2 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 362.8 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 157.9 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 193.4 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 139.5 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 251.2 |
AlN (mp-661) | <1 0 1> | <1 1 1> | 193.4 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 355.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 139.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 355.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 193.4 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 139.5 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 197.3 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 157.9 |
GaN (mp-804) | <1 0 1> | <1 1 1> | 241.7 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 355.2 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 157.9 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 223.3 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 145.0 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 157.9 |
Te2Mo (mp-602) | <1 0 1> | <1 1 0> | 276.3 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 139.5 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 355.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 307.0 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 195.4 |
GaSe (mp-1943) | <1 0 1> | <1 1 0> | 276.3 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 139.5 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 193.4 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 251.2 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 118.4 |
* indicates reconstructed surface.
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
36 | 17 | 17 | 0 | 0 | 0 |
17 | 36 | 17 | 0 | 0 | 0 |
17 | 17 | 36 | 0 | 0 | 0 |
0 | 0 | 0 | 20 | 0 | 0 |
0 | 0 | 0 | 0 | 20 | 0 |
0 | 0 | 0 | 0 | 0 | 20 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
39.3 | -12.5 | -12.5 | 0 | 0 | 0 |
-12.5 | 39.3 | -12.5 | 0 | 0 | 0 |
-12.5 | -12.5 | 39.3 | 0 | 0 | 0 |
0 | 0 | 0 | 50.3 | 0 | 0 |
0 | 0 | 0 | 0 | 50.3 | 0 |
0 | 0 | 0 | 0 | 0 | 50.3 |
Shear Modulus GV16 GPa |
Bulk Modulus KV23 GPa |
Shear Modulus GR14 GPa |
Bulk Modulus KR23 GPa |
Shear Modulus GVRH15 GPa |
Bulk Modulus KVRH23 GPa |
Elastic Anisotropy0.66 |
Poisson's Ratio0.24 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCu2Ni (mp-30593) | 0.0042 | 0.005 | 3 |
CrCoPt2 (mp-570863) | 0.0923 | 0.034 | 3 |
LiCa6Ge (mp-12609) | 0.1082 | 0.183 | 3 |
GaFeNi2 (mp-1065359) | 0.0932 | 0.065 | 3 |
GaCo2Ni (mp-1018060) | 0.1011 | 0.075 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.1775 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.3220 | 0.065 | 4 |
CrFeCoNi (mp-1096923) | 0.3683 | 0.193 | 4 |
Zn3Ge (mp-971928) | 0.0057 | 0.118 | 2 |
Ce3Zn (mp-984772) | 0.0062 | 0.058 | 2 |
NbPd3 (mp-1135) | 0.0021 | 0.003 | 2 |
VPt (mp-2678) | 0.0083 | 0.000 | 2 |
TaPd3 (mp-30836) | 0.0063 | 0.000 | 2 |
Pr (mp-97) | 0.0918 | 0.008 | 1 |
Sm (mp-21377) | 0.0941 | 0.011 | 1 |
Hg (mp-753304) | 0.1039 | 0.012 | 1 |
Th (mp-37) | 0.1019 | 0.000 | 1 |
Rb (mp-12628) | 0.0864 | 0.015 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: La |
Final Energy/Atom-4.9353 eV |
Corrected Energy-4.9353 eV
-4.9353 eV = -4.9353 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)