material

GaAs

ID:

mp-15619

DOI:

10.17188/1191274


Tags: Gallium arsenide - HP

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.208 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.144 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.48 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
GaAs
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pa3 [205]
Hall
-P 2ac 2ab 3
Point Group
m3
Crystal System
cubic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
MoSe2 (mp-1634) <0 0 1> <1 1 1> 0.001 86.2
WSe2 (mp-1821) <0 0 1> <1 1 1> 0.001 86.2
Ge (mp-32) <1 1 0> <1 1 0> 0.001 140.7
SiC (mp-8062) <1 0 0> <1 0 0> 0.003 248.7
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.004 248.7
GaAs (mp-2534) <1 1 0> <1 1 0> 0.004 140.7
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.006 199.0
SrTiO3 (mp-4651) <1 1 0> <1 0 0> 0.006 248.7
SiC (mp-7631) <0 0 1> <1 1 1> 0.013 258.5
DyScO3 (mp-31120) <0 0 1> <1 1 0> 0.015 281.4
LiF (mp-1138) <1 1 0> <1 1 0> 0.015 70.4
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.015 248.7
LiF (mp-1138) <1 1 1> <1 1 1> 0.015 86.2
Al2O3 (mp-1143) <0 0 1> <1 1 1> 0.015 258.5
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.016 140.7
SiC (mp-11714) <0 0 1> <1 1 1> 0.016 258.5
MgAl2O4 (mp-3536) <1 1 0> <1 1 0> 0.020 281.4
CsI (mp-614603) <1 0 0> <1 0 0> 0.021 248.7
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.031 199.0
BN (mp-984) <0 0 1> <1 0 0> 0.041 348.2
AlN (mp-661) <1 0 0> <1 0 0> 0.046 248.7
TiO2 (mp-390) <0 0 1> <1 0 0> 0.046 248.7
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.050 248.7
Ni (mp-23) <1 0 0> <1 0 0> 0.052 49.7
Ni (mp-23) <1 1 0> <1 1 0> 0.052 70.4
Ni (mp-23) <1 1 1> <1 1 1> 0.052 86.2
TbScO3 (mp-31119) <0 0 1> <1 1 0> 0.053 281.4
Te2Mo (mp-602) <0 0 1> <1 0 0> 0.059 348.2
Mg (mp-153) <0 0 1> <1 0 0> 0.064 348.2
SiO2 (mp-6930) <1 1 1> <1 1 0> 0.070 211.1
SiO2 (mp-6930) <0 0 1> <1 1 1> 0.081 86.2
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.108 348.2
WS2 (mp-224) <0 0 1> <1 0 0> 0.109 348.2
KP(HO2)2 (mp-23959) <0 0 1> <1 0 0> 0.116 149.2
C (mp-48) <0 0 1> <1 1 0> 0.118 211.1
NaCl (mp-22862) <1 1 1> <1 1 0> 0.118 281.4
Al (mp-134) <1 1 0> <1 1 0> 0.126 70.4
Al (mp-134) <1 1 1> <1 1 1> 0.126 86.2
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.133 248.7
CaCO3 (mp-3953) <0 0 1> <1 0 0> 0.150 348.2
C (mp-66) <1 1 1> <1 0 0> 0.167 348.2
C (mp-66) <1 1 0> <1 0 0> 0.168 248.7
DyScO3 (mp-31120) <1 1 0> <1 0 0> 0.171 248.7
KP(HO2)2 (mp-23959) <0 1 1> <1 1 0> 0.187 211.1
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.194 70.4
KTaO3 (mp-3614) <1 1 1> <1 1 1> 0.194 86.2
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.215 199.0
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.217 248.7
ZnSe (mp-1190) <1 1 1> <1 1 0> 0.227 281.4
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.235 348.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
109 29 29 0 0 0
29 109 29 0 0 0
29 29 109 0 0 0
0 0 0 41 0 0
0 0 0 0 41 0
0 0 0 0 0 41
Compliance Tensor Sij (10-12Pa-1)
10.3 -2.2 -2.2 0 0 0
-2.2 10.3 -2.2 0 0 0
-2.2 -2.2 10.3 0 0 0
0 0 0 24.1 0 0
0 0 0 0 24.1 0
0 0 0 0 0 24.1
Shear Modulus GV
41 GPa
Bulk Modulus KV
56 GPa
Shear Modulus GR
41 GPa
Bulk Modulus KR
56 GPa
Shear Modulus GVRH
41 GPa
Bulk Modulus KVRH
56 GPa
Elastic Anisotropy
0.00
Poisson's Ratio
0.21

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Li2CrO3 (mp-770149) 0.6968 0.072 3
CaSnN2 (mp-1029633) 0.7044 0.000 3
Mg2CrN3 (mp-1029520) 0.6394 0.000 3
Mg2VN3 (mp-1029368) 0.7454 0.000 3
Mg2MnN3 (mp-1029288) 0.6211 0.019 3
Li5MnOF5 (mp-764320) 0.7132 0.061 4
GaP (mp-971632) 0.0153 0.170 2
AlAs (mp-988945) 0.0132 0.150 2
InAs (mp-20412) 0.0602 0.113 2
LaN (mp-567290) 0.5779 0.000 2
AlSb (mp-15621) 0.0524 0.117 2
Si (mp-571520) 0.4629 0.161 1
Ge (mp-128) 0.5208 0.148 1
C (mp-24) 0.5103 0.833 1
Si (mp-168) 0.3567 0.160 1
Ge (mp-1080106) 0.3498 0.146 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Synthesis Descriptions

All samples were grown by solid-source molecular beam epitaxy (MBE). GaAs (001) substrates were degreased and etched by using NH4OH solution. Then they were mounted on Mo-holder using indium. The su [...]
To grow QDs, first, a 70-nm-thick GaAs buffer layer was deposited by MBE on a (001) semi-insulating GaAs substrate, sequentially followed by a 50-nm-thick Al0.3Ga0.7As layer, 20 periods of 2-nm-thic [...]
chef hat mixing beaker

Explore more synthesis descriptions for materials of composition GaAs.

Text computed by synthesisproject.org.

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ga_d As
Final Energy/Atom
-4.0521 eV
Corrected Energy
-64.8336 eV
Uncorrected energy = -64.8336 eV Corrected energy = -64.8336 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 41992
Submitted by
User remarks:
  • Gallium arsenide - HP

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)