material

As2Ir

ID:

mp-15649

DOI:

10.17188/1191293


Tags: Iridarsenite Iridium arsenide (1/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.483 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
10.45 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
1.153 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P21/c [14]
Hall
-P 2ybc
Point Group
2/m
Crystal System
monoclinic

Electronic Structure

Topological data for ICSD ID 42573 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
BN (mp-984) <1 0 0> <0 1 1> 0.007 155.2
GaP (mp-2490) <1 0 0> <0 0 1> 0.009 151.2
Mg (mp-153) <1 1 1> <0 0 1> 0.013 151.2
Te2Mo (mp-602) <1 1 0> <0 0 1> 0.020 189.0
CaF2 (mp-2741) <1 0 0> <0 0 1> 0.044 151.2
SiO2 (mp-6930) <1 1 1> <0 0 1> 0.050 264.6
LiF (mp-1138) <1 0 0> <0 0 1> 0.063 151.2
Te2W (mp-22693) <0 1 1> <1 1 1> 0.063 291.0
GdScO3 (mp-5690) <0 0 1> <0 1 0> 0.064 318.0
Te2Mo (mp-602) <1 1 1> <0 0 1> 0.072 189.0
NaCl (mp-22862) <1 1 0> <1 1 -1> 0.074 274.7
LiGaO2 (mp-5854) <1 0 1> <0 0 1> 0.086 226.8
LiGaO2 (mp-5854) <0 1 0> <1 1 0> 0.100 261.1
SiC (mp-8062) <1 1 0> <0 0 1> 0.103 189.0
CaCO3 (mp-3953) <1 1 0> <0 0 1> 0.117 151.2
YAlO3 (mp-3792) <1 1 1> <1 0 -1> 0.118 126.2
SiC (mp-7631) <1 0 1> <0 0 1> 0.120 189.0
NdGaO3 (mp-3196) <0 0 1> <0 1 0> 0.125 247.3
YAlO3 (mp-3792) <1 0 0> <0 1 0> 0.130 282.6
InAs (mp-20305) <1 0 0> <0 0 1> 0.133 37.8
Si (mp-149) <1 0 0> <0 0 1> 0.135 151.2
CeO2 (mp-20194) <1 0 0> <0 0 1> 0.146 151.2
GdScO3 (mp-5690) <1 0 1> <0 1 0> 0.149 282.6
Ge (mp-32) <1 0 0> <0 0 1> 0.149 302.4
ZnTe (mp-2176) <1 0 0> <0 0 1> 0.160 37.8
NdGaO3 (mp-3196) <1 1 0> <0 0 1> 0.164 302.4
TiO2 (mp-2657) <1 0 0> <1 1 1> 0.167 291.0
SrTiO3 (mp-4651) <1 0 0> <0 1 1> 0.184 310.4
DyScO3 (mp-31120) <1 0 0> <1 1 -1> 0.195 274.7
ZnO (mp-2133) <1 1 0> <1 1 0> 0.196 208.8
CdWO4 (mp-19387) <0 1 0> <0 1 0> 0.196 106.0
TePb (mp-19717) <1 0 0> <0 0 1> 0.215 340.1
YVO4 (mp-19133) <0 0 1> <1 0 1> 0.228 317.9
SiC (mp-8062) <1 0 0> <0 0 1> 0.246 37.8
TbScO3 (mp-31119) <1 0 0> <1 1 -1> 0.246 274.7
TiO2 (mp-390) <1 0 1> <1 0 1> 0.252 317.9
AlN (mp-661) <1 1 1> <1 0 1> 0.256 254.3
Mg (mp-153) <0 0 1> <1 0 0> 0.262 269.1
ZnO (mp-2133) <1 0 1> <1 1 0> 0.263 156.6
BN (mp-984) <1 0 1> <0 0 1> 0.264 302.4
ZrO2 (mp-2858) <0 0 1> <1 1 1> 0.273 218.2
GaN (mp-804) <1 1 1> <0 0 1> 0.277 151.2
TbScO3 (mp-31119) <1 0 1> <0 1 0> 0.288 282.6
Ni (mp-23) <1 1 0> <1 0 -1> 0.297 210.3
C (mp-48) <1 0 1> <0 1 0> 0.298 141.3
SiC (mp-7631) <1 0 0> <0 0 1> 0.323 189.0
CdS (mp-672) <1 1 0> <1 0 -1> 0.329 252.4
Te2W (mp-22693) <0 0 1> <1 0 0> 0.344 153.8
YAlO3 (mp-3792) <0 1 0> <0 1 0> 0.353 353.3
TiO2 (mp-390) <1 1 1> <1 1 1> 0.369 218.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
295 71 79 0 26 0
71 352 77 0 19 0
79 77 277 0 -13 0
0 0 0 103 0 26
26 19 -13 0 81 0
0 0 0 26 0 86
Compliance Tensor Sij (10-12Pa-1)
3.9 -0.5 -1 0 -1.3 0
-0.5 3.1 -0.8 0 -0.7 0
-1 -0.8 4.2 0 1.2 0
0 0 0 10.5 0 -3.2
-1.3 -0.7 1.2 0 13 0
0 0 0 -3.2 0 12.7
Shear Modulus GV
100 GPa
Bulk Modulus KV
153 GPa
Shear Modulus GR
92 GPa
Bulk Modulus KR
151 GPa
Shear Modulus GVRH
96 GPa
Bulk Modulus KVRH
152 GPa
Elastic Anisotropy
0.46
Poisson's Ratio
0.24

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
20.16 0.00 0.26
0.00 23.60 0.00
0.26 0.00 20.32
Dielectric Tensor εij (total)
28.06 0.00 0.05
0.00 30.83 0.00
0.05 0.00 27.82
Polycrystalline dielectric constant εpoly
(electronic contribution)
21.36
Polycrystalline dielectric constant εpoly
(total)
28.91
Refractive Index n
4.62
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
GeTeRh (mp-607818) 0.3972 0.048 3
FeAsS (mp-561511) 0.2677 0.000 3
SiSbPt (mp-11152) 0.4309 0.000 3
PRuS (mp-1095584) 0.2287 0.005 3
TeAsRu (mp-1095634) 0.3162 0.000 3
Sr2Li2NiO4 (mp-769674) 0.6576 0.091 4
Na2Li3CoO4 (mp-540990) 0.7362 0.000 4
LiCaGaN2 (mp-570948) 0.7472 0.000 4
P2Ir (mp-10155) 0.1758 0.000 2
CoP2 (mp-14285) 0.1503 0.000 2
Sb2Ir (mp-1247) 0.1963 0.000 2
P2Rh (mp-15953) 0.1487 0.000 2
As2Rh (mp-15954) 0.1134 0.000 2
NaZr2SN2Cl (mp-679669) 0.6285 0.077 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: As Ir
Final Energy/Atom
-6.5349 eV
Corrected Energy
-78.4191 eV
Uncorrected energy = -78.4191 eV Corrected energy = -78.4191 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 610742
  • 610739
  • 42573
  • 610734
Submitted by
User remarks:
  • Iridarsenite
  • Iridium arsenide (1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)