Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.548 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.13 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.342 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPcca [54] |
Hall-P 2a 2ac |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 0 1> | 110.9 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 143.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 110.9 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 189.6 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 143.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 189.6 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 143.8 |
Ag (mp-124) | <1 1 1> | <0 1 1> | 181.6 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 221.8 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 143.8 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 110.9 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 0> | 143.8 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 153.8 |
C (mp-66) | <1 0 0> | <1 0 0> | 153.8 |
C (mp-66) | <1 1 0> | <0 1 0> | 143.8 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 1> | 189.6 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 110.9 |
GdScO3 (mp-5690) | <1 1 1> | <0 0 1> | 221.8 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 153.8 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 153.8 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 1> | 189.6 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 221.8 |
SiC (mp-11714) | <1 1 0> | <0 0 1> | 110.9 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 221.8 |
Au (mp-81) | <1 1 0> | <0 0 1> | 221.8 |
Au (mp-81) | <1 1 1> | <0 1 1> | 181.6 |
WS2 (mp-224) | <1 1 0> | <1 0 0> | 153.8 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 221.8 |
YAlO3 (mp-3792) | <0 0 1> | <0 0 1> | 110.9 |
CdWO4 (mp-19387) | <0 0 1> | <0 1 1> | 181.6 |
ZnO (mp-2133) | <1 1 1> | <1 0 1> | 189.6 |
GaTe (mp-542812) | <1 0 0> | <0 0 1> | 221.8 |
Ge (mp-32) | <1 1 0> | <0 1 0> | 143.8 |
Cu (mp-30) | <1 1 0> | <0 0 1> | 110.9 |
Cu (mp-30) | <1 1 1> | <0 1 1> | 181.6 |
Fe2O3 (mp-24972) | <0 0 1> | <0 1 1> | 181.6 |
Fe2O3 (mp-24972) | <1 0 0> | <0 1 0> | 143.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
NiP4O11 (mp-764190) | 0.4902 | 0.010 | 3 |
Fe(PO3)4 (mp-31874) | 0.4532 | 0.047 | 3 |
Co(PO3)4 (mp-687059) | 0.4835 | 0.083 | 3 |
Co(PO3)4 (mp-31550) | 0.4683 | 0.068 | 3 |
Fe(PO3)4 (mp-697781) | 0.4740 | 0.047 | 3 |
LiP4WO12 (mp-762190) | 0.3406 | 0.032 | 4 |
LiMn(PO3)3 (mp-763643) | 0.3844 | 0.080 | 4 |
ZnAg(PO3)3 (mp-14260) | 0.0945 | 0.000 | 4 |
NaCd(PO3)3 (mp-15250) | 0.4033 | 0.000 | 4 |
NaNi(PO3)3 (mp-579459) | 0.2075 | 0.030 | 4 |
LiVCr(P2O7)2 (mp-767629) | 0.5559 | 0.007 | 5 |
LiMnV(P2O7)2 (mp-764454) | 0.5277 | 0.003 | 5 |
LiVFe(P2O7)2 (mp-767272) | 0.5658 | 0.006 | 5 |
LiVFe(P2O7)2 (mp-765110) | 0.5407 | 0.006 | 5 |
LiVFe(P2O7)2 (mp-765188) | 0.5680 | 0.009 | 5 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.6286 | 0.255 | 6 |
K3Na3TeP6(HO4)6 (mp-720804) | 0.6518 | 0.030 | 6 |
CsAlBP2HO9 (mp-542129) | 0.6546 | 0.000 | 6 |
RbAlBP2HO9 (mp-542130) | 0.6974 | 0.000 | 6 |
CsFeBP2HO9 (mp-761395) | 0.7194 | 0.000 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.6982 | 0.002 | 7 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Mg_pv Ag P O |
Final Energy/Atom-6.7542 eV |
Corrected Energy-807.0307 eV
-807.0307 eV = -756.4658 eV (uncorrected energy) - 50.5649 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)