Final Magnetic Moment3.112 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.648 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.71 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP6 [174] |
HallP 6 |
Point Group6 |
Crystal Systemhexagonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 280.8 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 156.0 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 343.2 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 156.0 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 187.2 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 312.0 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 343.2 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 280.8 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 203.1 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 218.4 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 249.6 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 149.1 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 218.4 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 156.0 |
KCl (mp-23193) | <1 1 0> | <1 1 1> | 173.2 |
GaAs (mp-2534) | <1 0 0> | <1 1 1> | 259.9 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 218.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 67.7 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 280.8 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 343.2 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 280.8 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 156.0 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 218.4 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 67.7 |
ZnSe (mp-1190) | <1 0 0> | <1 1 1> | 259.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 203.1 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 67.7 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 218.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 203.1 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 298.2 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 324.2 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 203.1 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 54.0 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 298.2 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 249.6 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 312.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 1> | 259.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 270.2 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 280.8 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 249.6 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 216.1 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 218.4 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 298.2 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 203.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 67.7 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 156.0 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 108.1 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 156.0 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 54.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 203.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sc2Ni12P7 (mp-3084) | 0.2737 | 0.000 | 3 |
Sr7(H6Cl)2 (mp-23827) | 0.2899 | 0.000 | 3 |
Li2Ni12P7 (mp-541010) | 0.2669 | 0.000 | 3 |
Zr2Ni12P7 (mp-18648) | 0.2648 | 0.000 | 3 |
Zr2Fe12P7 (mp-540809) | 0.2897 | 0.000 | 3 |
Yb3In3Ge2Au (mp-981207) | 0.6718 | 0.000 | 4 |
LiYb2InGe2 (mp-977355) | 0.7126 | 0.000 | 4 |
Sr2LiInGe2 (mp-571617) | 0.7106 | 0.000 | 4 |
LiCa2InGe2 (mp-570850) | 0.7007 | 0.000 | 4 |
Ba6Eu(ClF6)2 (mp-556702) | 0.4784 | 0.024 | 4 |
Mg6Si5 (mp-1073911) | 0.6794 | 0.168 | 2 |
Mg6Si5 (mp-1073935) | 0.6537 | 0.153 | 2 |
Mg6Si5 (mp-1073921) | 0.6494 | 0.131 | 2 |
Mg3Si4 (mp-1075277) | 0.6033 | 0.188 | 2 |
Mg6Si5 (mp-1073910) | 0.6310 | 0.136 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nb_pv Co P |
Final Energy/Atom-7.4759 eV |
Corrected Energy-156.9932 eV
Uncorrected energy = -156.9932 eV
Corrected energy = -156.9932 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)