Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.771 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.009 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.91 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCu5Si2S7 + SiS2 + Cu |
Band Gap1.605 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCc [9] |
HallC 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <1 0 0> | 70.8 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 267.3 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 190.9 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 267.3 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 305.5 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 283.2 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 -1> | 248.8 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 152.7 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 267.3 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 141.6 |
Te2Mo (mp-602) | <1 1 1> | <0 1 0> | 190.9 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 76.4 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 267.3 |
GaSe (mp-1943) | <1 0 0> | <0 1 0> | 267.3 |
GaSe (mp-1943) | <1 0 1> | <0 1 0> | 267.3 |
BN (mp-984) | <1 0 1> | <0 1 0> | 305.5 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 190.9 |
MoS2 (mp-1434) | <1 0 0> | <1 1 -1> | 273.9 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 267.3 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 267.3 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 70.8 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 141.6 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 -1> | 165.9 |
SiC (mp-7631) | <0 0 1> | <1 1 0> | 241.3 |
MgO (mp-1265) | <1 0 0> | <1 1 0> | 160.9 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 76.4 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 212.4 |
C (mp-66) | <1 1 0> | <0 1 0> | 305.5 |
C (mp-66) | <1 1 1> | <1 0 -1> | 248.8 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 -1> | 248.8 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 267.3 |
Mg (mp-153) | <1 1 0> | <1 0 1> | 114.9 |
Mg (mp-153) | <1 1 1> | <1 0 -1> | 248.8 |
LaF3 (mp-905) | <0 0 1> | <1 0 0> | 141.6 |
LaF3 (mp-905) | <1 0 0> | <1 0 -1> | 165.9 |
PbS (mp-21276) | <1 1 0> | <0 1 0> | 152.7 |
PbS (mp-21276) | <1 1 1> | <0 1 0> | 305.5 |
InP (mp-20351) | <1 1 0> | <0 1 0> | 152.7 |
InP (mp-20351) | <1 1 1> | <0 1 0> | 305.5 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 -1> | 248.8 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 343.7 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 190.9 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 114.6 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 114.9 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 283.2 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 283.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 70.9 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 114.6 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 114.6 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 152.7 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
143 | 45 | 45 | 0 | -2 | 0 |
45 | 146 | 57 | 0 | -12 | 0 |
45 | 57 | 133 | 0 | 10 | 0 |
0 | 0 | 0 | 39 | 0 | -11 |
-2 | -12 | 10 | 0 | 30 | 0 |
0 | 0 | 0 | -11 | 0 | 31 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
8.2 | -1.6 | -2.1 | 0 | 0.7 | 0 |
-1.6 | 9.2 | -3.8 | 0 | 5 | 0 |
-2.1 | -3.8 | 10.2 | 0 | -5.3 | 0 |
0 | 0 | 0 | 28.2 | 0 | 10 |
0.7 | 5 | -5.3 | 0 | 37.7 | 0 |
0 | 0 | 0 | 10 | 0 | 35.8 |
Shear Modulus GV38 GPa |
Bulk Modulus KV80 GPa |
Shear Modulus GR34 GPa |
Bulk Modulus KR79 GPa |
Shear Modulus GVRH36 GPa |
Bulk Modulus KVRH79 GPa |
Elastic Anisotropy0.71 |
Poisson's Ratio0.30 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cu2GeTe3 (mp-674953) | 0.1238 | 0.007 | 3 |
Cu2GeTe3 (mp-12806) | 0.1428 | 0.000 | 3 |
Cu2GeS3 (mp-15252) | 0.1393 | 0.001 | 3 |
Cu2SiSe3 (mp-15896) | 0.0785 | 0.000 | 3 |
Ag2SnSe3 (mp-1096812) | 0.1395 | 0.000 | 3 |
MnCu2SnSe4 (mp-22400) | 0.1576 | 0.000 | 4 |
Cu4Si2NiS7 (mp-557274) | 0.1280 | 0.024 | 4 |
CdCu2SnSe4 (mp-16565) | 0.1672 | 0.005 | 4 |
ZnCu2SnSe4 (mvc-16089) | 0.1606 | 0.009 | 4 |
ZnCu2SnS4 (mp-1025500) | 0.1672 | 0.003 | 4 |
AuS (mp-984598) | 0.2047 | 0.105 | 2 |
BeP2 (mp-27148) | 0.1743 | 0.000 | 2 |
CuI (mp-673245) | 0.1517 | 0.008 | 2 |
BC5 (mp-1018649) | 0.1964 | 0.271 | 2 |
BC5 (mp-1095514) | 0.1580 | 0.295 | 2 |
Sn (mp-949028) | 0.1841 | 0.030 | 1 |
Si (mp-971662) | 0.1843 | 0.064 | 1 |
C (mp-569517) | 0.2965 | 0.145 | 1 |
C (mp-611426) | 0.2899 | 0.146 | 1 |
Ge (mp-1091415) | 0.2944 | 0.014 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cu_pv Si S |
Final Energy/Atom-4.7783 eV |
Corrected Energy-61.3203 eV
-61.3203 eV = -57.3396 eV (uncorrected energy) - 3.9808 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)