material

Hf3(SiCu2)2

ID:

mp-15987

DOI:

10.17188/1191499


Tags: Copper hafnium silicide (4/3/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Unknown
Formation Energy / Atom
-0.501 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
10.25 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P62m [189]
Hall
P 6 2
Point Group
6m2
Crystal System
hexagonal

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
BN (mp-984) <0 0 1> <0 0 1> 0.016 103.4
LiGaO2 (mp-5854) <0 0 1> <1 1 1> 0.023 55.4
Te2W (mp-22693) <1 0 1> <1 0 0> 0.025 100.3
GaSe (mp-1943) <0 0 1> <0 0 1> 0.027 241.2
BN (mp-984) <1 0 1> <1 0 0> 0.042 100.3
Au (mp-81) <1 0 0> <1 0 0> 0.046 225.7
Ag (mp-124) <1 0 0> <1 0 0> 0.049 225.7
TbScO3 (mp-31119) <0 1 1> <1 1 0> 0.054 217.2
TiO2 (mp-2657) <1 1 0> <1 0 0> 0.061 275.9
PbS (mp-21276) <1 0 0> <1 0 0> 0.063 326.0
ZrO2 (mp-2858) <1 0 0> <0 0 1> 0.065 172.3
BaTiO3 (mp-5986) <1 0 0> <1 0 0> 0.072 50.2
Mg (mp-153) <1 0 1> <1 0 0> 0.073 75.2
LaAlO3 (mp-2920) <1 0 1> <1 1 0> 0.074 304.1
Au (mp-81) <1 1 0> <1 1 1> 0.080 221.8
LaF3 (mp-905) <0 0 1> <0 0 1> 0.081 137.8
AlN (mp-661) <1 0 0> <1 0 0> 0.084 125.4
GdScO3 (mp-5690) <0 1 1> <1 1 0> 0.088 217.2
Mg (mp-153) <1 1 0> <0 0 1> 0.091 172.3
Mg (mp-153) <1 1 1> <0 0 1> 0.095 241.2
Cu (mp-30) <1 1 1> <1 0 0> 0.101 225.7
YVO4 (mp-19133) <1 0 0> <0 0 1> 0.102 137.8
Ag (mp-124) <1 1 0> <1 1 1> 0.105 221.8
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.111 175.5
WS2 (mp-224) <0 0 1> <1 0 0> 0.111 175.5
C (mp-48) <0 0 1> <1 1 1> 0.116 110.9
DyScO3 (mp-31120) <0 1 1> <1 1 0> 0.123 217.2
ZrO2 (mp-2858) <1 1 1> <1 1 0> 0.146 304.1
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.151 100.3
DyScO3 (mp-31120) <0 0 1> <0 0 1> 0.160 310.2
TiO2 (mp-2657) <1 0 1> <1 1 0> 0.162 304.1
DyScO3 (mp-31120) <0 1 0> <0 0 1> 0.178 172.3
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.179 137.8
AlN (mp-661) <1 0 1> <1 0 1> 0.193 213.1
AlN (mp-661) <0 0 1> <0 0 1> 0.198 34.5
LaF3 (mp-905) <1 1 0> <0 0 1> 0.206 275.7
CdS (mp-672) <1 1 1> <1 1 0> 0.209 260.6
CdS (mp-672) <1 1 0> <1 0 1> 0.211 298.3
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.227 200.6
Fe2O3 (mp-24972) <0 0 1> <1 0 0> 0.228 225.7
MoS2 (mp-1434) <1 0 1> <1 0 0> 0.229 275.9
TiO2 (mp-390) <1 1 1> <1 1 0> 0.239 217.2
WS2 (mp-224) <1 1 1> <0 0 1> 0.247 241.2
CsI (mp-614603) <1 1 0> <1 1 0> 0.255 86.9
ZrO2 (mp-2858) <1 0 -1> <1 0 1> 0.263 213.1
TbScO3 (mp-31119) <0 1 0> <0 0 1> 0.264 172.3
CdWO4 (mp-19387) <0 1 0> <1 0 1> 0.269 213.1
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.270 103.4
Mg (mp-153) <0 0 1> <0 0 1> 0.272 34.5
InP (mp-20351) <1 1 1> <0 0 1> 0.276 241.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
233 87 117 -0 -0 0
87 233 117 0 -0 0
117 117 224 0 0 0
0 0 0 112 0 0
0 0 0 0 112 0
0 0 0 0 -0 73
Compliance Tensor Sij (10-12Pa-1)
6 -0.9 -2.7 0 0 0
-0.9 6 -2.7 0 0 0
-2.7 -2.7 7.3 0 0 0
0 0 0 9 0 0
0 0 0 0 9 0
0 0 0 0 0 13.7
Shear Modulus GV
84 GPa
Bulk Modulus KV
148 GPa
Shear Modulus GR
76 GPa
Bulk Modulus KR
148 GPa
Shear Modulus GVRH
80 GPa
Bulk Modulus KVRH
148 GPa
Elastic Anisotropy
0.49
Poisson's Ratio
0.27

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
28
U Values
--
Pseudopotentials
VASP PAW: Si Cu_pv Hf_pv
Final Energy/Atom
-6.8460 eV
Corrected Energy
-61.6141 eV
-61.6141 eV = -61.6141 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 53288

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)