Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.250 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.06 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.220 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 281.2 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 208.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 312.5 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 199.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 187.5 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 234.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 31.2 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 211.1 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 156.2 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 31.2 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 312.5 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 281.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 78.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 203.1 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 281.2 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 140.6 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 265.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 171.9 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 171.9 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 149.3 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 144.2 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 216.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 125.0 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 288.3 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 140.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 250.0 |
SiO2 (mp-6930) | <1 1 0> | <1 1 1> | 144.2 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 78.1 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 296.8 |
BN (mp-984) | <0 0 1> | <0 0 1> | 125.0 |
BN (mp-984) | <1 0 0> | <0 0 1> | 93.7 |
BN (mp-984) | <1 0 1> | <0 0 1> | 203.1 |
BN (mp-984) | <1 1 0> | <1 0 1> | 104.3 |
BN (mp-984) | <1 1 1> | <0 0 1> | 312.5 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 31.2 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 218.7 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 281.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 218.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 211.1 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 62.5 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 296.8 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 78.1 |
LiNbO3 (mp-3731) | <1 1 1> | <1 0 1> | 260.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 31.2 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 312.5 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 281.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 15.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 156.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 140.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 312.5 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
184 | 48 | 42 | 0 | 0 | 0 |
48 | 184 | 42 | 0 | 0 | 0 |
42 | 42 | 122 | 0 | 0 | 0 |
0 | 0 | 0 | 20 | 0 | 0 |
0 | 0 | 0 | 0 | 20 | 0 |
0 | 0 | 0 | 0 | 0 | 60 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
6.2 | -1.2 | -1.7 | 0 | 0 | 0 |
-1.2 | 6.2 | -1.7 | 0 | 0 | 0 |
-1.7 | -1.7 | 9.4 | 0 | 0 | 0 |
0 | 0 | 0 | 50.5 | 0 | 0 |
0 | 0 | 0 | 0 | 50.5 | 0 |
0 | 0 | 0 | 0 | 0 | 16.6 |
Shear Modulus GV44 GPa |
Bulk Modulus KV84 GPa |
Shear Modulus GR33 GPa |
Bulk Modulus KR81 GPa |
Shear Modulus GVRH38 GPa |
Bulk Modulus KVRH82 GPa |
Elastic Anisotropy1.72 |
Poisson's Ratio0.30 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Th2TeN2 (mp-7523) | 0.0423 | 0.000 | 3 |
Y2TeO2 (mp-755756) | 0.0174 | 0.000 | 3 |
Sm2TeO2 (mp-16033) | 0.0432 | 0.000 | 3 |
Gd2TeO2 (mp-16035) | 0.0399 | 0.000 | 3 |
Dy2TeO2 (mp-16037) | 0.0126 | 0.000 | 3 |
KLiZnS2 (mp-774907) | 0.4209 | 0.000 | 4 |
SrBiClO2 (mp-547244) | 0.4261 | 0.000 | 4 |
SrBiBrO2 (mp-552234) | 0.4080 | 0.000 | 4 |
KLiMnS2 (mp-753940) | 0.3704 | 0.000 | 4 |
BiPbClO2 (mp-23084) | 0.3349 | 0.000 | 4 |
Bi3O2 (mp-1022722) | 0.7018 | 0.127 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tb_3 Te O |
Final Energy/Atom-7.4303 eV |
Corrected Energy-38.5559 eV
-38.5559 eV = -37.1514 eV (uncorrected energy) - 1.4046 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)