material

CuSiO3

ID:

mp-16053

DOI:

10.17188/1191542


Tags: Copper catena-silicate

Material Details

Final Magnetic Moment
1.006 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-2.250 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.088 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.68 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
CuO + SiO2
Band Gap
0.112 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pmma [51]
Hall
-P 2a 2a
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 89669 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Al (mp-134) <1 1 1> <0 0 1> 0.004 28.1
LiTaO3 (mp-3666) <1 1 1> <1 1 0> 0.004 254.8
CdTe (mp-406) <1 1 0> <1 0 1> 0.006 185.0
InSb (mp-20012) <1 1 0> <1 0 1> 0.006 185.0
Ni (mp-23) <1 1 1> <0 0 1> 0.008 42.2
TiO2 (mp-2657) <1 1 0> <1 0 0> 0.008 176.2
SiC (mp-11714) <1 0 1> <0 0 1> 0.009 225.1
GaSe (mp-1943) <1 0 0> <1 1 0> 0.009 203.9
CdS (mp-672) <1 1 1> <0 0 1> 0.009 211.0
ZnO (mp-2133) <1 1 0> <1 1 0> 0.012 152.9
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.012 305.8
LiGaO2 (mp-5854) <0 1 0> <0 1 1> 0.014 263.1
NaCl (mp-22862) <1 0 0> <0 0 1> 0.014 225.1
GaSe (mp-1943) <1 0 1> <1 1 0> 0.014 203.9
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.014 28.1
Ge3(BiO3)4 (mp-23560) <1 1 1> <0 0 1> 0.016 196.9
Al (mp-134) <1 0 0> <0 0 1> 0.016 112.5
C (mp-48) <0 0 1> <0 0 1> 0.018 42.2
KCl (mp-23193) <1 0 0> <0 0 1> 0.018 281.3
NdGaO3 (mp-3196) <0 1 0> <1 1 1> 0.019 211.5
ZnO (mp-2133) <0 0 1> <0 0 1> 0.020 28.1
ZnSe (mp-1190) <1 1 0> <0 0 1> 0.020 140.7
BaF2 (mp-1029) <1 1 0> <1 0 0> 0.020 220.3
MgF2 (mp-1249) <1 1 0> <1 0 1> 0.020 185.0
TeO2 (mp-2125) <1 0 1> <1 1 0> 0.020 152.9
TePb (mp-19717) <1 1 0> <1 0 1> 0.021 185.0
TiO2 (mp-2657) <0 0 1> <1 1 1> 0.021 264.4
AlN (mp-661) <1 0 0> <1 0 1> 0.021 46.2
Si (mp-149) <1 1 0> <1 1 1> 0.022 211.5
Mg (mp-153) <0 0 1> <0 0 1> 0.022 112.5
CeO2 (mp-20194) <1 1 0> <1 1 1> 0.022 211.5
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.023 112.5
GaP (mp-2490) <1 1 0> <1 1 1> 0.024 211.5
KCl (mp-23193) <1 1 0> <1 0 0> 0.024 176.2
Fe2O3 (mp-24972) <1 1 1> <1 1 0> 0.024 254.8
NdGaO3 (mp-3196) <0 1 1> <1 0 0> 0.025 264.3
ZrO2 (mp-2858) <1 1 1> <0 0 1> 0.027 154.7
KCl (mp-23193) <1 1 1> <0 1 0> 0.028 281.8
GaN (mp-804) <1 0 0> <0 1 1> 0.029 204.6
LiNbO3 (mp-3731) <1 1 1> <1 1 0> 0.030 254.8
CaF2 (mp-2741) <1 1 0> <1 1 1> 0.030 211.5
NdGaO3 (mp-3196) <1 0 1> <1 0 1> 0.030 323.7
TbScO3 (mp-31119) <0 1 1> <1 0 0> 0.031 264.3
Ga2O3 (mp-886) <1 0 -1> <1 0 1> 0.032 231.2
GaAs (mp-2534) <1 1 0> <0 0 1> 0.033 140.7
TeO2 (mp-2125) <0 1 1> <1 1 0> 0.035 152.9
Al2O3 (mp-1143) <1 0 1> <1 0 0> 0.035 132.2
CdWO4 (mp-19387) <0 1 1> <1 0 1> 0.036 277.5
NdGaO3 (mp-3196) <0 0 1> <1 1 0> 0.036 152.9
SiO2 (mp-6930) <1 1 1> <0 0 1> 0.037 211.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
15 10 8 0 0 0
10 20 2 0 0 0
8 2 301 0 0 0
0 0 0 50 0 0
0 0 0 0 10 0
0 0 0 0 0 5
Compliance Tensor Sij (10-12Pa-1)
100.4 -47.2 -2.3 0 0 0
-47.2 71.4 0.7 0 0 0
-2.3 0.7 3.4 0 0 0
0 0 0 19.9 0 0
0 0 0 0 104.9 0
0 0 0 0 0 200.1
Shear Modulus GV
34 GPa
Bulk Modulus KV
42 GPa
Shear Modulus GR
8 GPa
Bulk Modulus KR
13 GPa
Shear Modulus GVRH
21 GPa
Bulk Modulus KVRH
27 GPa
Elastic Anisotropy
18.48
Poisson's Ratio
0.19

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
AgGeO3 (mp-779664) 0.3417 0.086 3
CuGeO3 (mp-561216) 0.4697 0.021 3
CuGeO3 (mp-917381) 0.5030 0.032 3
CuGeO3 (mp-21344) 0.4887 0.032 3
AgGeO3 (mp-779706) 0.4019 0.091 3
Li2CuP2O7 (mp-6412) 0.4217 0.000 4
Li2CrP2O7 (mp-540481) 0.4728 0.000 4
Li2NiP2O7 (mp-585297) 0.4196 0.021 4
Li2FeP2O7 (mp-540098) 0.4822 0.011 4
Li2CoP2O7 (mp-540132) 0.4469 0.017 4
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Cu_pv Si O
Final Energy/Atom
-6.7111 eV
Corrected Energy
-71.2330 eV
Uncorrected energy = -67.1110 eV Composition-based energy adjustment (-0.687 eV/atom x 6.0 atoms) = -4.1220 eV Corrected energy = -71.2330 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 89669
Submitted by
User remarks:
  • Copper catena-silicate

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)