Final Magnetic Moment0.025 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.114 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.150 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.15 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTlTe |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mcm [140] |
Hall-I 4 2c |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 0 0> | <1 1 0> | 116.1 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 116.1 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 164.2 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 246.2 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 174.0 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 246.2 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 246.2 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 246.2 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 164.2 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 164.2 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 164.2 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 174.0 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 246.2 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 232.2 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 174.0 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 174.0 |
C (mp-66) | <1 1 0> | <1 0 0> | 164.2 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 246.2 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 1> | 192.4 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 246.2 |
LaF3 (mp-905) | <0 0 1> | <1 1 0> | 232.2 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 174.0 |
PbSe (mp-2201) | <1 1 0> | <1 0 0> | 164.2 |
SiC (mp-11714) | <1 0 0> | <1 0 0> | 246.2 |
InSb (mp-20012) | <1 1 0> | <1 0 0> | 246.2 |
PbSe (mp-2201) | <1 0 0> | <1 1 0> | 116.1 |
Au (mp-81) | <1 0 0> | <0 0 1> | 174.0 |
CdSe (mp-2691) | <1 0 0> | <1 1 0> | 116.1 |
CdSe (mp-2691) | <1 1 0> | <1 0 0> | 164.2 |
WS2 (mp-224) | <0 0 1> | <1 0 0> | 246.2 |
SiC (mp-8062) | <1 0 0> | <1 1 0> | 116.1 |
SiC (mp-8062) | <1 1 0> | <1 0 0> | 82.1 |
ZnTe (mp-2176) | <1 0 0> | <1 1 0> | 116.1 |
MgF2 (mp-1249) | <1 0 0> | <1 1 0> | 116.1 |
MgF2 (mp-1249) | <1 1 0> | <1 0 0> | 82.1 |
MgF2 (mp-1249) | <1 1 1> | <1 0 0> | 246.2 |
GaSb (mp-1156) | <1 0 0> | <1 1 0> | 116.1 |
GaSb (mp-1156) | <1 1 0> | <1 0 0> | 164.2 |
Cu (mp-30) | <1 1 0> | <1 0 0> | 164.2 |
GaTe (mp-542812) | <0 0 1> | <1 1 0> | 232.2 |
GaTe (mp-542812) | <1 0 -1> | <1 1 0> | 232.2 |
LiAlO2 (mp-3427) | <1 0 0> | <1 0 0> | 164.2 |
LiAlO2 (mp-3427) | <1 1 0> | <1 1 0> | 232.2 |
Al2O3 (mp-1143) | <1 0 0> | <1 0 1> | 192.4 |
ZnTe (mp-2176) | <1 1 0> | <1 0 0> | 164.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Nb5SiSn2 (mp-7557) | 0.6530 | 0.001 | 3 |
Ti5Sb2Rh (mp-16687) | 0.6137 | 0.030 | 3 |
Ni(TePd)2 (mp-12463) | 0.6541 | 0.000 | 3 |
Ti5CuSb2 (mp-13020) | 0.5024 | 0.001 | 3 |
Nb5GaSn2 (mp-17230) | 0.5350 | 0.000 | 3 |
Ce5Sn3 (mp-637308) | 0.2558 | 0.000 | 2 |
Cd5Au3 (mp-30371) | 0.3389 | 0.000 | 2 |
Dy5In3 (mp-568144) | 0.2724 | 0.000 | 2 |
Ce5Ga3 (mp-542328) | 0.0785 | 0.002 | 2 |
Zr5Al3 (mp-16724) | 0.3064 | 0.037 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tl_d Te |
Final Energy/Atom-2.8663 eV |
Corrected Energy-45.8616 eV
-45.8616 eV = -45.8616 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)