Final Magnetic Moment0.008 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.355 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.055 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.30 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToYbSi + Yb2Ag7 + Yb(SiAg)2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP62m [189] |
HallP 6 2 |
Point Group6m2 |
Crystal Systemhexagonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 168.8 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 153.4 |
AlN (mp-661) | <1 0 0> | <1 1 1> | 271.5 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 214.8 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 265.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 168.8 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 184.1 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 295.5 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 245.4 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 245.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 295.5 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 211.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 260.9 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 168.8 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 276.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 260.9 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 168.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 208.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 295.5 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 208.7 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 368.2 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 153.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 211.1 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 245.4 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 245.4 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 214.8 |
KCl (mp-23193) | <1 1 1> | <1 1 0> | 212.6 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 260.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 337.5 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 214.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 260.9 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 276.1 |
Te2Mo (mp-602) | <1 0 1> | <1 0 0> | 214.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 211.1 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 260.9 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 208.7 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 276.1 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 211.1 |
GaSe (mp-1943) | <0 0 1> | <1 0 1> | 313.1 |
GaSe (mp-1943) | <1 0 0> | <1 0 1> | 260.9 |
BN (mp-984) | <1 0 0> | <1 0 0> | 214.8 |
BN (mp-984) | <1 1 0> | <1 1 0> | 265.7 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 295.5 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 214.8 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 211.1 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 168.8 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 0> | 122.7 |
LiNbO3 (mp-3731) | <1 1 1> | <1 0 0> | 122.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 295.5 |
Al (mp-134) | <1 1 0> | <1 0 1> | 208.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YbAgGe (mp-9776) | 0.0785 | 0.000 | 3 |
SmMgIn (mp-21456) | 0.1231 | 0.000 | 3 |
ScCuSi (mp-15322) | 0.1334 | 0.000 | 3 |
YMgTl (mp-11984) | 0.1231 | 0.000 | 3 |
SmMgTl (mp-11987) | 0.1174 | 0.000 | 3 |
Yb3In3Ge2Au (mp-981207) | 0.3216 | 0.000 | 4 |
LiYb2InGe2 (mp-977355) | 0.4148 | 0.000 | 4 |
Sr2LiInGe2 (mp-571617) | 0.3866 | 0.000 | 4 |
LiCa2InGe2 (mp-570850) | 0.4183 | 0.000 | 4 |
U3Al3NiRu2 (mp-1080528) | 0.5294 | 0.088 | 4 |
Fe2P (mp-778) | 0.4925 | 0.000 | 2 |
CoSn3 (mp-985707) | 0.5704 | 0.000 | 2 |
BaCl2 (mp-567680) | 0.5959 | 0.030 | 2 |
Co2As (mp-1079254) | 0.5941 | 0.071 | 2 |
CeSe2 (mp-1080312) | 0.6027 | 0.012 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Yb_2 Si Ag |
Final Energy/Atom-3.6212 eV |
Corrected Energy-32.5908 eV
-32.5908 eV = -32.5908 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)