Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.528 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.626 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.53 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCdGeP2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <1 1 0> | 314.6 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 251.7 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 188.8 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 77.1 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 0> | 314.6 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 125.8 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 251.7 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 125.8 |
CeO2 (mp-20194) | <1 1 1> | <1 1 0> | 251.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 188.8 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 188.8 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 222.5 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 188.8 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 188.8 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 231.2 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 251.7 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 314.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 266.9 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 62.9 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 188.8 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 231.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 188.8 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 222.5 |
MoS2 (mp-1434) | <0 0 1> | <1 1 0> | 314.6 |
Al (mp-134) | <1 1 0> | <1 1 0> | 188.8 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 1> | 308.2 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 44.5 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 77.1 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 77.1 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 89.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 0> | 251.7 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 62.9 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 251.7 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 89.0 |
BN (mp-984) | <0 0 1> | <1 0 0> | 311.4 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 1> | 308.2 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 311.4 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 222.5 |
C (mp-66) | <1 0 0> | <1 0 0> | 222.5 |
GdScO3 (mp-5690) | <1 0 0> | <1 1 0> | 188.8 |
Mg (mp-153) | <1 0 0> | <1 1 0> | 251.7 |
Mg (mp-153) | <1 1 0> | <1 1 0> | 251.7 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 251.7 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 44.5 |
CdTe (mp-406) | <1 1 1> | <1 1 1> | 77.1 |
KP(HO2)2 (mp-23959) | <1 0 0> | <1 0 0> | 222.5 |
LaF3 (mp-905) | <0 0 1> | <1 1 1> | 308.2 |
LaF3 (mp-905) | <1 0 0> | <1 0 0> | 222.5 |
GaP (mp-2490) | <1 1 0> | <1 1 0> | 125.8 |
GaP (mp-2490) | <1 1 1> | <1 1 0> | 251.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnInPd2 (mp-31328) | 0.0000 | 0.000 | 3 |
Li2SbAu (mp-30404) | 0.0000 | 0.000 | 3 |
NbAlCo2 (mp-5149) | 0.0000 | 0.009 | 3 |
HfAlNi2 (mp-5748) | 0.0000 | 0.000 | 3 |
AlCrCo2 (mp-10883) | 0.0000 | 0.058 | 3 |
LiMgSnPd (mp-7555) | 0.0000 | 0.000 | 4 |
VFeCoGe (mp-1063914) | 0.0000 | 0.000 | 4 |
VGaFeCo (mp-1066581) | 0.0000 | 0.029 | 4 |
LiMgSbPd (mp-10179) | 0.0000 | 0.096 | 4 |
LiMgSnPt (mp-11806) | 0.0000 | 0.000 | 4 |
Rb3Bi (mp-23304) | 0.0000 | 0.028 | 2 |
Sr3In (mp-31349) | 0.0000 | 0.131 | 2 |
Fe3Ge (mp-20711) | 0.0000 | 0.000 | 2 |
LiGa (mp-1307) | 0.0000 | 0.000 | 2 |
NaTl (mp-1564) | 0.0000 | 0.000 | 2 |
Eu (mp-20071) | 0.0000 | 0.085 | 1 |
Ba (mp-122) | 0.0000 | 0.000 | 1 |
Ce (mp-10024) | 0.0000 | 0.228 | 1 |
Np (mp-10207) | 0.0000 | 0.447 | 1 |
Gd (mp-11421) | 0.0000 | 0.088 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cd Ge_d P |
Final Energy/Atom-3.5593 eV |
Corrected Energy-14.2372 eV
Uncorrected energy = -14.2372 eV
Corrected energy = -14.2372 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)