Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.795 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.009 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.75 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCd2Sb2O7 |
Band Gap1.031 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinImma [74] |
Hall-I 2b 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <1 0 1> | 285.9 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 304.4 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 228.3 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 228.3 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 187.9 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 233.3 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 228.3 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 304.4 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 304.4 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 152.2 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 228.3 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 228.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 330.5 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 275.4 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 311.1 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 152.2 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 217.6 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 155.6 |
Te2W (mp-22693) | <1 1 0> | <0 0 1> | 110.2 |
YVO4 (mp-19133) | <0 0 1> | <1 1 0> | 108.8 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 93.9 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 275.4 |
TePb (mp-19717) | <1 0 0> | <1 1 0> | 217.6 |
Te2Mo (mp-602) | <0 0 1> | <1 0 1> | 285.9 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 155.6 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 155.6 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 217.6 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 275.4 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 275.4 |
BN (mp-984) | <1 0 0> | <1 0 1> | 95.3 |
BN (mp-984) | <1 1 0> | <0 0 1> | 165.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 275.4 |
MoS2 (mp-1434) | <0 0 1> | <0 1 1> | 281.8 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 228.3 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 281.8 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 1> | 93.9 |
CdTe (mp-406) | <1 0 0> | <1 1 0> | 217.6 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 330.5 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 76.1 |
TiO2 (mp-2657) | <0 0 1> | <1 1 0> | 108.8 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 1 0> | 108.8 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <0 1 0> | 152.2 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 1 1> | 187.9 |
C (mp-66) | <1 0 0> | <1 1 0> | 217.6 |
C (mp-66) | <1 1 0> | <1 1 0> | 108.8 |
Mg (mp-153) | <0 0 1> | <0 1 1> | 281.8 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 233.3 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 228.3 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 1 0> | 217.6 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 1 0> | 217.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca2Os2O7 (mp-2923) | 0.2343 | 0.000 | 3 |
Na2Te2O7 (mp-20254) | 0.3968 | 0.000 | 3 |
Sr2Sb2O7 (mp-4103) | 0.3374 | 0.000 | 3 |
Ca2Sb2O7 (mp-16280) | 0.1463 | 0.000 | 3 |
Ag2Te2O7 (mp-13211) | 0.3751 | 0.002 | 3 |
Na2GaNiF7 (mp-565426) | 0.3397 | 0.055 | 4 |
Na2FeNiF7 (mp-566483) | 0.2985 | 0.170 | 4 |
Na2FeNiF7 (mp-558817) | 0.2327 | 0.172 | 4 |
Na2FeNiF7 (mp-621502) | 0.2320 | 0.172 | 4 |
Na2CrNiF7 (mp-566540) | 0.2752 | 0.000 | 4 |
NaYb3Ti2(SbO7)2 (mp-695026) | 0.5737 | 0.074 | 5 |
KCaNb2O6F (mp-682067) | 0.5439 | 0.009 | 5 |
NaGd3Ti2(SbO7)2 (mp-40451) | 0.5472 | 0.000 | 5 |
NaDy3Ti2(SbO7)2 (mp-40478) | 0.5140 | 0.000 | 5 |
YTi2CdO6F (mp-686765) | 0.5742 | 0.142 | 5 |
NaYTiNbO6F (mp-42599) | 0.4604 | 0.053 | 6 |
NaPrTiNbO6F (mp-42897) | 0.5662 | 0.035 | 6 |
NaGdTiNbO6F (mp-42981) | 0.4993 | 0.047 | 6 |
NaCeTiNbO6F (mp-43055) | 0.5730 | 0.039 | 6 |
NaNdTiNbO6F (mp-43134) | 0.5566 | 0.038 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cd Sb O |
Final Energy/Atom-5.4120 eV |
Corrected Energy-128.8967 eV
-128.8967 eV = -119.0647 eV (uncorrected energy) - 9.8321 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)