Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.555 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.075 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density16.01 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiPt2 + Pt |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/m [87] |
Hall-I 4 |
Point Group4/m |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 321.7 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 303.3 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 106.7 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 151.6 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 227.5 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 214.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 151.6 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 227.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 160.8 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 227.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 160.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 276.7 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 227.5 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 53.6 |
Al (mp-134) | <1 0 0> | <1 0 0> | 160.8 |
Al (mp-134) | <1 1 0> | <1 0 0> | 160.8 |
Al (mp-134) | <1 1 1> | <1 1 0> | 227.5 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 107.2 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 268.1 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 160.8 |
TeO2 (mp-2125) | <0 1 1> | <1 1 0> | 75.8 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 92.2 |
C (mp-66) | <1 0 0> | <1 0 0> | 321.7 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 160.8 |
GdScO3 (mp-5690) | <0 1 1> | <1 1 0> | 227.5 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 276.7 |
Mg (mp-153) | <0 0 1> | <1 1 0> | 227.5 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 268.1 |
Mg (mp-153) | <1 1 1> | <1 1 0> | 151.6 |
GaP (mp-2490) | <1 1 0> | <1 0 0> | 214.4 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 0> | 160.8 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 0> | 53.6 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 276.7 |
TbScO3 (mp-31119) | <1 1 1> | <1 0 1> | 213.3 |
Ni (mp-23) | <1 0 0> | <1 1 0> | 303.3 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 268.1 |
InSb (mp-20012) | <1 1 1> | <1 0 0> | 160.8 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 160.8 |
NdGaO3 (mp-3196) | <0 0 1> | <1 1 0> | 151.6 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 0> | 53.6 |
NdGaO3 (mp-3196) | <1 1 1> | <1 0 1> | 213.3 |
Si (mp-149) | <1 1 0> | <1 0 0> | 214.4 |
WS2 (mp-224) | <1 0 0> | <1 0 0> | 268.1 |
WS2 (mp-224) | <1 1 0> | <1 0 0> | 160.8 |
WS2 (mp-224) | <1 1 1> | <1 0 0> | 160.8 |
C (mp-48) | <0 0 1> | <1 0 0> | 321.7 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 160.8 |
NaCl (mp-22862) | <1 1 0> | <1 1 0> | 227.5 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 276.7 |
ZrO2 (mp-2858) | <0 1 0> | <1 1 0> | 303.3 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
307 | 151 | 151 | 0 | 0 | 0 |
151 | 188 | 289 | 49 | 0 | 0 |
151 | 289 | 188 | -49 | 0 | 0 |
0 | 49 | -49 | 33 | 0 | 0 |
0 | 0 | 0 | 0 | -13 | 0 |
0 | 0 | 0 | 0 | 0 | -13 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
4.7 | -1.5 | -1.5 | 0 | 0 | 0 |
-1.5 | -0.5 | 3.6 | 6.1 | 0 | 0 |
-1.5 | 3.6 | -0.5 | -6.1 | 0 | 0 |
0 | 6.1 | -6.1 | 12.6 | 0 | 0 |
0 | 0 | 0 | 0 | -75.4 | 0 |
0 | 0 | 0 | 0 | 0 | -75.4 |
Shear Modulus GV7 GPa |
Bulk Modulus KV207 GPa |
Shear Modulus GR-37 GPa |
Bulk Modulus KR207 GPa |
Shear Modulus GVRH-15 GPa |
Bulk Modulus KVRH207 GPa |
Elastic Anisotropy-5.99 |
Poisson's Ratio0.54 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Tm2NiSn6 (mp-1079270) | 0.7254 | 0.000 | 3 |
Er2NiSn6 (mp-1079596) | 0.7445 | 0.000 | 3 |
Lu2NiSn6 (mp-31136) | 0.7223 | 0.001 | 3 |
Ni12P5 (mp-2790) | 0.2573 | 0.000 | 2 |
Yb8Tl3 (mp-570438) | 0.7217 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si Pt |
Final Energy/Atom-6.4353 eV |
Corrected Energy-109.4009 eV
-109.4009 eV = -109.4009 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)