material

SrAl2

ID:

mp-1638

DOI:

10.17188/1191849


Tags: Aluminum strontium (2/1) - HP, HT Aluminium strontium (2/1) Strontium aluminide (1/2)

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.254 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.007 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.30 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
SrAl4 + Sr5Al9
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fd3m [227]
Hall
F 4d 2 3 1d
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 58167 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.006 274.8
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.010 137.4
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.011 274.8
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.017 137.4
Ga2O3 (mp-886) <1 1 0> <1 1 0> 0.021 291.5
GaP (mp-2490) <1 0 0> <1 0 0> 0.023 274.8
Ag (mp-124) <1 0 0> <1 0 0> 0.027 68.7
Ag (mp-124) <1 1 0> <1 1 0> 0.027 97.2
Ag (mp-124) <1 1 1> <1 1 1> 0.027 119.0
C (mp-66) <1 1 0> <1 1 0> 0.030 291.5
Bi2Te3 (mp-34202) <0 0 1> <1 1 1> 0.032 119.0
Al (mp-134) <1 0 0> <1 0 0> 0.037 274.8
Ga2O3 (mp-886) <1 0 0> <1 1 0> 0.045 291.5
Mg (mp-153) <1 1 1> <1 0 0> 0.047 274.8
GaN (mp-804) <1 1 1> <1 0 0> 0.071 274.8
Au (mp-81) <1 0 0> <1 0 0> 0.075 68.7
Au (mp-81) <1 1 0> <1 1 0> 0.075 97.2
Au (mp-81) <1 1 1> <1 1 1> 0.075 119.0
Mg (mp-153) <1 0 1> <1 0 0> 0.094 206.1
Ni (mp-23) <1 1 0> <1 1 0> 0.100 194.3
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.103 274.8
Cu (mp-30) <1 1 0> <1 1 0> 0.103 291.5
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 0.109 274.8
LiGaO2 (mp-5854) <1 0 1> <1 0 0> 0.156 137.4
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.156 274.8
GaN (mp-804) <1 0 1> <1 0 0> 0.166 206.1
Si (mp-149) <1 0 0> <1 0 0> 0.191 274.8
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.200 274.8
NdGaO3 (mp-3196) <0 0 1> <1 0 0> 0.206 274.8
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.249 274.8
SiC (mp-8062) <1 1 0> <1 1 0> 0.250 291.5
MgAl2O4 (mp-3536) <1 0 0> <1 0 0> 0.361 68.7
MgAl2O4 (mp-3536) <1 1 0> <1 1 0> 0.362 97.2
MgAl2O4 (mp-3536) <1 1 1> <1 1 1> 0.362 119.0
TeO2 (mp-2125) <1 0 0> <1 1 0> 0.449 291.5
BaTiO3 (mp-5986) <0 0 1> <1 1 1> 0.457 238.0
InP (mp-20351) <1 0 0> <1 0 0> 0.484 68.7
InP (mp-20351) <1 1 0> <1 1 0> 0.485 97.2
Ga2O3 (mp-886) <0 1 0> <1 1 0> 0.488 291.5
Ge (mp-32) <1 0 0> <1 0 0> 0.498 68.7
Ge (mp-32) <1 1 0> <1 1 0> 0.499 97.2
ZrO2 (mp-2858) <1 1 0> <1 0 0> 0.521 274.8
CdS (mp-672) <1 0 0> <1 1 0> 0.536 291.5
GaAs (mp-2534) <1 0 0> <1 0 0> 0.633 68.7
GaAs (mp-2534) <1 1 0> <1 1 0> 0.634 97.2
LiNbO3 (mp-3731) <1 0 0> <1 1 0> 0.640 291.5
Al2O3 (mp-1143) <1 0 0> <1 1 0> 0.642 194.3
InSb (mp-20012) <1 1 0> <1 1 0> 0.699 194.3
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.724 68.7
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.726 97.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
97 24 24 0 0 0
24 97 24 0 0 0
24 24 97 0 0 0
0 0 0 37 0 0
0 0 0 0 37 0
0 0 0 0 0 37
Compliance Tensor Sij (10-12Pa-1)
11.4 -2.3 -2.3 0 0 0
-2.3 11.4 -2.3 0 0 0
-2.3 -2.3 11.4 0 0 0
0 0 0 27.1 0 0
0 0 0 0 27.1 0
0 0 0 0 0 27.1
Shear Modulus GV
37 GPa
Bulk Modulus KV
48 GPa
Shear Modulus GR
37 GPa
Bulk Modulus KR
48 GPa
Shear Modulus GVRH
37 GPa
Bulk Modulus KVRH
48 GPa
Elastic Anisotropy
0.00
Poisson's Ratio
0.20

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
YbNi4Au (mp-1024977) 0.0000 0.040 3
TmInCu4 (mp-1024957) 0.0028 0.000 3
GdNi4Au (mp-1077131) 0.0027 0.855 3
YbCu4Au (mp-1077165) 0.0028 0.000 3
GdInCu4 (mp-1077293) 0.0009 0.000 3
PrCo2 (mp-2085) 0.0000 0.050 2
ZrMo2 (mp-2049) 0.0000 0.000 2
MgCu2 (mp-1038) 0.0000 0.000 2
YbFe2 (mp-1665) 0.0000 0.096 2
HoCo2 (mp-2396) 0.0000 0.000 2
Co (mp-1072089) 0.0000 0.199 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Sr_sv Al
Final Energy/Atom
-3.3145 eV
Corrected Energy
-19.8868 eV
Uncorrected energy = -19.8868 eV Corrected energy = -19.8868 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 246192
  • 58167
  • 181800
Submitted by
User remarks:
  • Strontium aluminide (1/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)