Final Magnetic Moment0.041 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.505 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.48 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 210.2 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 76.5 |
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 127.5 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 321.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 280.4 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 137.8 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 229.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 204.0 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 204.0 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 25.5 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 1> | 262.7 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 178.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 229.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 280.4 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 204.0 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 210.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 331.4 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 137.8 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 45.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 91.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 262.7 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 321.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 331.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 0> | 159.2 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 178.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 210.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 1> | 250.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 331.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 102.0 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 229.7 |
CdS (mp-672) | <1 1 0> | <1 1 1> | 250.7 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 331.4 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 238.7 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 178.5 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 204.0 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 321.6 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 127.5 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 305.9 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 76.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 76.5 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 137.8 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 318.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 229.4 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 229.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 102.0 |
BN (mp-984) | <1 0 0> | <0 0 1> | 331.4 |
BN (mp-984) | <1 0 1> | <0 0 1> | 229.4 |
BN (mp-984) | <1 1 0> | <1 0 0> | 321.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 25.5 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 305.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca2Mg3Si (mp-1095343) | 0.1158 | 0.119 | 3 |
Eu2Ga3Ir (mp-609413) | 0.2122 | 0.000 | 3 |
Er2Al3Co (mp-567849) | 0.0420 | 0.000 | 3 |
Sc2Al3Ru (mp-10911) | 0.2292 | 0.000 | 3 |
Mg2Cu3Si (mp-10746) | 0.2158 | 0.000 | 3 |
NdMn2 (mp-1095569) | 0.1856 | 0.436 | 2 |
BaMg2 (mp-1935) | 0.1263 | 0.000 | 2 |
CaZn2 (mp-13364) | 0.1590 | 0.025 | 2 |
ThMn2 (mp-1095511) | 0.1917 | 0.073 | 2 |
SmMn2 (mp-1095689) | 0.1277 | 0.148 | 2 |
Co (mp-1072089) | 0.3080 | 0.199 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Lu_3 Al Co |
Final Energy/Atom-5.0700 eV |
Corrected Energy-60.8397 eV
-60.8397 eV = -60.8397 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)