Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingUnknown |
Formation Energy / Atom-3.310 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.013 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.44 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToDy2SO2 + Dy2S3 + SiO2 |
Band Gap2.611 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI41/amd [141] |
HallI 4bw 2bw 1bw |
Point Group4/mmm |
Crystal Systemtetragonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
TeO2 (mp-2125) | <1 0 1> | <1 0 0> | 160.7 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 137.7 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 137.7 |
Au (mp-81) | <1 0 0> | <0 0 1> | 137.7 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 137.7 |
MgAl2O4 (mp-3536) | <1 0 0> | <0 0 1> | 137.7 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 137.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Tm4Si2S3O7 (mp-16591) | 0.0744 | 0.041 | 4 |
Y4Si2S3O7 (mp-1020598) | 0.0291 | 0.015 | 4 |
Tb4Si2S3O7 (mp-16590) | 0.0244 | 0.005 | 4 |
Er4Si2S3O7 (mp-6316) | 0.0446 | 0.029 | 4 |
Ho4Si2S3O7 (mp-6757) | 0.0236 | 0.022 | 4 |
KCu3S2ClO9 (mp-555595) | 0.6747 | 0.014 | 5 |
CaEr15Si8Se11ClO28 (mp-720985) | 0.4085 | 0.039 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points11 |
U Values-- |
PseudopotentialsVASP PAW: O Si S Dy_3 |
Final Energy/Atom-7.6398 eV |
Corrected Energy-516.5720 eV
-516.5720 eV = -488.9463 eV (uncorrected energy) - 27.6256 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)