Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.074 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.004 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density12.57 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToGe2Os + Os |
Band Gap0.742 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPbcn [60] |
Hall-P 2n 2ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 128.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 271.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 1> | 173.6 |
InAs (mp-20305) | <1 1 1> | <0 1 1> | 260.4 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 67.7 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 326.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 163.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 163.1 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 326.3 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 67.7 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 163.1 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 243.1 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 270.6 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 121.5 |
Te2Mo (mp-602) | <1 0 0> | <0 1 1> | 260.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 271.9 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 173.6 |
GaSe (mp-1943) | <1 0 0> | <0 1 1> | 260.4 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 326.3 |
Al (mp-134) | <1 0 0> | <0 0 1> | 163.1 |
Al (mp-134) | <1 1 0> | <0 0 1> | 163.1 |
CdTe (mp-406) | <1 1 0> | <1 0 1> | 121.5 |
TeO2 (mp-2125) | <0 0 1> | <1 1 0> | 128.0 |
TeO2 (mp-2125) | <1 0 0> | <0 0 1> | 217.5 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 54.4 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 326.3 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 271.9 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 1> | 121.5 |
C (mp-66) | <1 0 0> | <1 1 0> | 128.0 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 0> | 128.0 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 326.3 |
GdScO3 (mp-5690) | <1 0 1> | <0 1 1> | 173.6 |
GdScO3 (mp-5690) | <1 1 0> | <1 1 0> | 128.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 271.9 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 108.8 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 270.6 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 326.3 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 270.6 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 67.7 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 326.3 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 326.3 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 326.3 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 326.3 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 326.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 326.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 326.3 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 326.3 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 326.3 |
PbS (mp-21276) | <1 1 1> | <0 1 1> | 260.4 |
InP (mp-20351) | <1 0 0> | <0 1 1> | 173.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
23.84 | 0.00 | 0.00 |
0.00 | 22.66 | 0.00 |
0.00 | 0.00 | 22.87 |
Dielectric Tensor εij (total) |
||
---|---|---|
81.09 | 0.00 | 0.00 |
0.00 | 58.29 | 0.00 |
0.00 | 0.00 | 57.86 |
Polycrystalline dielectric constant
εpoly∞
23.13
|
Polycrystalline dielectric constant
εpoly
65.75
|
Refractive Index n4.81 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Pr3RuCl3 (mp-639135) | 0.7344 | 0.000 | 3 |
KTiI3 (mp-640578) | 0.7306 | 0.119 | 3 |
Ca3AlSb3 (mvc-16396) | 0.7028 | 0.000 | 3 |
K2ZrTe3 (mp-29602) | 0.6640 | 0.000 | 3 |
Ca3(AlAs2)2 (mp-28304) | 0.6636 | 0.118 | 3 |
Na2Zr(CuS2)2 (mp-556536) | 0.6467 | 0.000 | 4 |
Si3Ru2 (mp-669501) | 0.6199 | 0.235 | 2 |
Ge3Ru2 (mp-21945) | 0.1718 | 0.000 | 2 |
Si3Ru2 (mp-22192) | 0.1116 | 0.000 | 2 |
Mg4Si3 (mp-1074396) | 0.6931 | 0.345 | 2 |
Si3Os2 (mp-16608) | 0.1603 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ge_d Os_pv |
Final Energy/Atom-7.3357 eV |
Corrected Energy-293.4275 eV
-293.4275 eV = -293.4275 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)