material

CaS

ID:

mp-1672

DOI:

10.17188/1192117


Tags: Calcium sulfide Oldhamite

Material Details

Final Magnetic Moment
0.002 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.480 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.57 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
2.560 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 28902 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
YVO4 (mp-19133) <0 0 1> <1 0 0> 0.000 261.4
Cu (mp-30) <1 0 0> <1 0 0> 0.000 65.4
KCl (mp-23193) <1 0 0> <1 0 0> 0.001 163.4
Al (mp-134) <1 1 0> <1 1 0> 0.001 46.2
Al (mp-134) <1 0 0> <1 0 0> 0.001 32.7
BN (mp-984) <0 0 1> <1 1 1> 0.002 169.8
MgO (mp-1265) <1 0 0> <1 0 0> 0.002 163.4
TiO2 (mp-390) <0 0 1> <1 0 0> 0.003 130.7
Ni (mp-23) <1 1 0> <1 1 0> 0.009 138.6
LaAlO3 (mp-2920) <1 0 1> <1 1 1> 0.013 226.4
AlN (mp-661) <1 0 1> <1 0 0> 0.013 196.1
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.015 46.2
KTaO3 (mp-3614) <1 0 0> <1 0 0> 0.016 32.7
CdWO4 (mp-19387) <0 1 1> <1 1 0> 0.028 323.5
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.032 184.8
LaAlO3 (mp-2920) <0 0 1> <1 1 1> 0.034 226.4
NaCl (mp-22862) <1 1 1> <1 1 1> 0.037 56.6
NaCl (mp-22862) <1 1 0> <1 1 0> 0.037 46.2
CdTe (mp-406) <1 1 1> <1 1 1> 0.037 226.4
CdTe (mp-406) <1 1 0> <1 1 0> 0.038 184.8
NaCl (mp-22862) <1 0 0> <1 0 0> 0.039 32.7
ZnSe (mp-1190) <1 1 1> <1 1 1> 0.042 56.6
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.042 46.2
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.045 32.7
C (mp-48) <1 0 1> <1 0 0> 0.047 261.4
Fe3O4 (mp-19306) <1 0 0> <1 0 0> 0.049 294.1
InSb (mp-20012) <1 1 1> <1 1 1> 0.049 226.4
InSb (mp-20012) <1 1 0> <1 1 0> 0.050 184.8
TePb (mp-19717) <1 1 1> <1 1 1> 0.053 226.4
TePb (mp-19717) <1 1 0> <1 1 0> 0.054 184.8
SiC (mp-7631) <0 0 1> <1 1 1> 0.057 226.4
AlN (mp-661) <0 0 1> <1 1 1> 0.060 226.4
TiO2 (mp-2657) <1 1 1> <1 1 0> 0.061 323.5
SiC (mp-11714) <0 0 1> <1 1 1> 0.063 226.4
AlN (mp-661) <1 0 0> <1 1 1> 0.066 283.0
GaAs (mp-2534) <1 1 1> <1 1 1> 0.071 56.6
GaAs (mp-2534) <1 1 0> <1 1 0> 0.072 46.2
GaAs (mp-2534) <1 0 0> <1 0 0> 0.076 32.7
WS2 (mp-224) <0 0 1> <1 1 1> 0.089 169.8
MoS2 (mp-1434) <0 0 1> <1 1 1> 0.089 169.8
LiF (mp-1138) <1 1 1> <1 0 0> 0.095 228.7
CdS (mp-672) <1 1 1> <1 0 0> 0.101 261.4
Mg (mp-153) <1 0 1> <1 1 0> 0.106 323.5
ZnO (mp-2133) <1 0 1> <1 1 1> 0.110 339.6
YAlO3 (mp-3792) <0 1 1> <1 1 1> 0.110 339.6
Al (mp-134) <1 1 1> <1 0 0> 0.111 228.7
DyScO3 (mp-31120) <1 0 0> <1 1 0> 0.113 46.2
TbScO3 (mp-31119) <1 0 0> <1 1 0> 0.116 46.2
Bi2Te3 (mp-34202) <0 0 1> <1 1 1> 0.118 226.4
Ge (mp-32) <1 1 1> <1 1 1> 0.133 56.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
123 24 24 0 0 0
24 123 24 0 0 0
24 24 123 0 0 0
0 0 0 33 0 0
0 0 0 0 33 0
0 0 0 0 0 33
Compliance Tensor Sij (10-12Pa-1)
8.7 -1.4 -1.4 0 0 0
-1.4 8.7 -1.4 0 0 0
-1.4 -1.4 8.7 0 0 0
0 0 0 29.9 0 0
0 0 0 0 29.9 0
0 0 0 0 0 29.9
Shear Modulus GV
40 GPa
Bulk Modulus KV
57 GPa
Shear Modulus GR
38 GPa
Bulk Modulus KR
57 GPa
Shear Modulus GVRH
39 GPa
Bulk Modulus KVRH
57 GPa
Elastic Anisotropy
0.19
Poisson's Ratio
0.22

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
4.99 -0.00 -0.00
-0.00 4.99 0.00
-0.00 0.00 4.99
Dielectric Tensor εij (total)
12.09 -0.00 -0.00
-0.00 12.09 0.00
-0.00 0.00 12.09
Polycrystalline dielectric constant εpoly
(electronic contribution)
4.99
Polycrystalline dielectric constant εpoly
(total)
12.09
Refractive Index n
2.23
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Sr4SO3 (mp-1079788) 0.0000 0.200 3
BaSr3O4 (mp-984729) 0.0000 0.044 3
ScH4Pd3 (mp-981386) 0.0000 0.037 3
Sr3CdO4 (mp-981103) 0.0000 0.019 3
SrCa3O4 (mp-978844) 0.0000 0.040 3
NbN (mp-1580) 0.0000 0.206 2
MnSe (mp-972) 0.0000 0.016 2
ErN (mp-19830) 0.0000 0.000 2
TmSb (mp-2520) 0.0000 0.000 2
CeS (mp-1096) 0.0000 0.000 2
As (mp-10) 0.0000 0.112 1
Sc (mp-1008681) 0.0000 0.719 1
Ca (mp-10683) 0.0000 0.400 1
C (mp-998866) 0.0000 2.755 1
Sb (mp-133) 0.0000 0.051 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv S
Final Energy/Atom
-5.2195 eV
Corrected Energy
-11.1024 eV
-11.1024 eV = -10.4389 eV (uncorrected energy) - 0.6635 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 619527
  • 619528
  • 619538
  • 52784
  • 619540
  • 60200
  • 30236
  • 619529
  • 186785
  • 619537
  • 619534
  • 603165
  • 619530
  • 53940
  • 28902
  • 41956
  • 619533
Submitted by
User remarks:
  • Calcium sulfide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)