Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.061 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.564 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.73 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToYP |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 188.7 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 302.6 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 119.8 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 60.5 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 302.6 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 157.3 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 290.5 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 157.3 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 222.5 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 136.9 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 205.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 157.3 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 146.7 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 325.2 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 272.5 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 136.9 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 62.9 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 205.8 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 169.4 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 266.3 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 119.8 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 21.0 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 136.9 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 104.8 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 326.8 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 325.2 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 272.5 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 157.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 188.3 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 273.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 181.5 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 181.5 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 1> | 167.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 60.5 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 157.3 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 51.3 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 62.9 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 157.3 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 136.9 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 273.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 157.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 68.5 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 83.9 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 62.9 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 145.2 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 256.7 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 291.0 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 205.8 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 157.3 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 83.9 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
157 | 102 | 102 | 0 | 0 | 0 |
102 | 157 | 102 | 0 | 0 | 0 |
102 | 102 | 157 | 0 | 0 | 0 |
0 | 0 | 0 | -56 | 0 | 0 |
0 | 0 | 0 | 0 | -56 | 0 |
0 | 0 | 0 | 0 | 0 | -56 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
13.1 | -5.2 | -5.2 | 0 | 0 | 0 |
-5.2 | 13.1 | -5.2 | 0 | 0 | 0 |
-5.2 | -5.2 | 13.1 | 0 | 0 | 0 |
0 | 0 | 0 | -17.9 | 0 | 0 |
0 | 0 | 0 | 0 | -17.9 | 0 |
0 | 0 | 0 | 0 | 0 | -17.9 |
Shear Modulus GV-23 GPa |
Bulk Modulus KV121 GPa |
Shear Modulus GR258 GPa |
Bulk Modulus KR121 GPa |
Shear Modulus GVRH118 GPa |
Bulk Modulus KVRH121 GPa |
Elastic Anisotropy-5.44 |
Poisson's Ratio0.13 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sm2AgRh (mp-972530) | 0.0000 | 0.028 | 3 |
Na2TiAu (mp-631554) | 0.0000 | 0.825 | 3 |
KFeTc2 (mp-631396) | 0.0000 | 1.417 | 3 |
Sc2OsPt (mp-862364) | 0.0000 | 0.000 | 3 |
PmSbAu2 (mp-862953) | 0.0000 | 0.000 | 3 |
TiFeCoSb (mp-998973) | 0.0000 | 0.186 | 4 |
TiAlFeCo (mp-998980) | 0.0000 | 0.000 | 4 |
MnFeCoGe (mp-1018024) | 0.0000 | 0.344 | 4 |
VFeCoSi (mp-1066609) | 0.0000 | 0.002 | 4 |
VFeCoSb (mp-1066862) | 0.0000 | 0.164 | 4 |
K3W (mp-973446) | 0.0000 | 1.504 | 2 |
LaHg (mp-734) | 0.0000 | 0.000 | 2 |
BaZn (mp-902) | 0.0000 | 0.002 | 2 |
InRh (mp-899) | 0.0000 | 0.000 | 2 |
BeCo (mp-2773) | 0.0000 | 0.000 | 2 |
Xe (mp-979285) | 0.0000 | 0.002 | 1 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.340 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Y_sv P |
Final Energy/Atom-7.0005 eV |
Corrected Energy-14.0011 eV
-14.0011 eV = -14.0011 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)