Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.299 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.005 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density11.16 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLuAg2 + Lu6Pb5 + Pb |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP62m [189] |
HallP 6 2 |
Point Group6m2 |
Crystal Systemhexagonal |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 337.6 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 235.7 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 192.9 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 235.7 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 304.6 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 175.8 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 176.7 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 203.0 |
BaF2 (mp-1029) | <1 1 0> | <1 1 1> | 227.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 144.7 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 337.6 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 169.2 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 270.7 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 192.9 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 304.6 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 203.0 |
KCl (mp-23193) | <1 1 0> | <1 1 1> | 227.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 304.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 1> | 227.7 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 192.9 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 176.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 338.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 1> | 303.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 192.9 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 294.6 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 294.6 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 101.5 |
LiF (mp-1138) | <1 1 0> | <1 1 1> | 303.6 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 192.9 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 175.8 |
Te2W (mp-22693) | <1 1 0> | <1 0 1> | 117.8 |
Te2W (mp-22693) | <1 1 1> | <0 0 1> | 241.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 337.6 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 241.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 144.7 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 270.7 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 270.7 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 270.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 0> | 175.8 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 101.5 |
GaSe (mp-1943) | <1 1 0> | <1 1 1> | 227.7 |
BN (mp-984) | <0 0 1> | <1 1 0> | 175.8 |
BN (mp-984) | <1 0 0> | <1 0 0> | 169.2 |
BN (mp-984) | <1 0 1> | <1 0 1> | 58.9 |
BN (mp-984) | <1 1 0> | <1 1 1> | 227.7 |
BN (mp-984) | <1 1 1> | <1 1 0> | 175.8 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 0> | 117.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 192.9 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 304.6 |
Al (mp-134) | <1 0 0> | <1 0 0> | 338.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TmAgPb (mp-20522) | 0.0265 | 0.000 | 3 |
LuAgSn (mp-3608) | 0.0181 | 0.010 | 3 |
ErAgPb (mp-16745) | 0.0240 | 0.000 | 3 |
TmAgSn (mp-2990) | 0.0327 | 0.012 | 3 |
ErAgSn (mp-13265) | 0.0436 | 0.012 | 3 |
Yb3In3Ge2Au (mp-981207) | 0.2933 | 0.000 | 4 |
LiYb2InGe2 (mp-977355) | 0.5102 | 0.000 | 4 |
Sr2LiInGe2 (mp-571617) | 0.4904 | 0.000 | 4 |
LiCa2InGe2 (mp-570850) | 0.5129 | 0.000 | 4 |
U3Al3NiRu2 (mp-1080528) | 0.5037 | 0.088 | 4 |
Fe2P (mp-778) | 0.4958 | 0.001 | 2 |
Pu2Co (mp-20026) | 0.5186 | 0.144 | 2 |
CaH2 (mp-23713) | 0.5949 | 0.000 | 2 |
SrH2 (mp-23714) | 0.5942 | 0.000 | 2 |
BaCl2 (mp-567680) | 0.5784 | 0.030 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Lu_3 Ag Pb_d |
Final Energy/Atom-3.9876 eV |
Corrected Energy-35.8884 eV
-35.8884 eV = -35.8884 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)