material

Zr2Te2P

ID:

mp-16765

DOI:

10.17188/1192152


Material Details

Final Magnetic Moment
0.014 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.284 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.96 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
R3m [166]
Hall
-R 3 2"
Point Group
3m
Crystal System
trigonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.000 51.4
Ag (mp-124) <1 1 1> <0 0 1> 0.000 90.0
MgAl2O4 (mp-3536) <1 1 1> <0 0 1> 0.000 115.7
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.005 205.7
Au (mp-81) <1 1 1> <0 0 1> 0.012 90.0
BN (mp-984) <1 0 1> <0 0 1> 0.014 141.4
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.018 321.4
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.019 38.6
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.020 38.6
InP (mp-20351) <1 1 1> <0 0 1> 0.023 244.3
GaN (mp-804) <0 0 1> <0 0 1> 0.024 115.7
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.026 51.4
Cu (mp-30) <1 1 1> <0 0 1> 0.027 90.0
NaCl (mp-22862) <1 1 1> <0 0 1> 0.029 167.1
MgF2 (mp-1249) <1 1 0> <0 0 1> 0.029 102.9
Si (mp-149) <1 1 1> <0 0 1> 0.030 51.4
BN (mp-984) <0 0 1> <0 0 1> 0.035 38.6
InSb (mp-20012) <1 0 0> <0 0 1> 0.037 308.6
CdTe (mp-406) <1 0 0> <0 0 1> 0.040 308.6
WS2 (mp-224) <0 0 1> <0 0 1> 0.051 115.7
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.051 115.7
LaF3 (mp-905) <0 0 1> <0 0 1> 0.053 321.4
TiO2 (mp-390) <1 1 1> <0 0 1> 0.053 270.0
CdWO4 (mp-19387) <0 1 1> <0 0 1> 0.061 321.4
Ga2O3 (mp-886) <1 0 1> <0 0 1> 0.065 321.4
MgF2 (mp-1249) <1 1 1> <0 0 1> 0.085 90.0
GaSe (mp-1943) <1 0 0> <0 0 1> 0.093 205.7
ZrO2 (mp-2858) <0 1 0> <0 0 1> 0.104 308.6
Mg (mp-153) <0 0 1> <0 0 1> 0.108 115.7
YAlO3 (mp-3792) <0 1 1> <0 0 1> 0.110 334.3
LiF (mp-1138) <1 0 0> <0 0 1> 0.115 270.0
NdGaO3 (mp-3196) <1 0 1> <0 0 1> 0.141 321.4
Ni (mp-23) <1 1 0> <0 0 1> 0.144 347.1
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.146 90.0
TiO2 (mp-390) <0 0 1> <0 0 1> 0.146 102.9
AlN (mp-661) <1 0 0> <0 0 1> 0.146 347.1
C (mp-66) <1 1 1> <0 0 1> 0.153 90.0
ZnO (mp-2133) <1 1 0> <0 0 1> 0.167 334.3
C (mp-48) <1 1 0> <1 0 0> 0.170 234.9
ZnO (mp-2133) <1 0 0> <0 0 1> 0.172 141.4
CdTe (mp-406) <1 1 0> <0 0 1> 0.172 308.6
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.174 90.0
Ge (mp-32) <1 0 0> <0 0 1> 0.180 270.0
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.180 244.3
InSb (mp-20012) <1 1 0> <0 0 1> 0.184 308.6
GaSe (mp-1943) <0 0 1> <0 0 1> 0.191 12.9
TeO2 (mp-2125) <0 1 0> <0 0 1> 0.204 205.7
CeO2 (mp-20194) <1 0 0> <0 0 1> 0.206 205.7
TePb (mp-19717) <1 1 0> <0 0 1> 0.212 308.6
TiO2 (mp-390) <1 0 1> <1 0 0> 0.215 117.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
111 29 7 -3 0 0
29 111 7 3 0 0
7 7 19 0 0 0
-3 3 0 7 0 0
0 0 0 0 7 -3
0 0 0 0 -3 41
Compliance Tensor Sij (10-12Pa-1)
10 -2.6 -2.9 4.9 0 0
-2.6 10 -2.9 -4.9 0 0
-2.9 -2.9 55.9 0 0 0
4.9 -4.9 0 139.1 0 0
0 0 0 0 139.1 9.9
0 0 0 0 9.9 25.2
Shear Modulus GV
24 GPa
Bulk Modulus KV
36 GPa
Shear Modulus GR
12 GPa
Bulk Modulus KR
17 GPa
Shear Modulus GVRH
18 GPa
Bulk Modulus KVRH
27 GPa
Elastic Anisotropy
6.24
Poisson's Ratio
0.22

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Y2GeI2 (mp-676315) 0.2026 0.000 3
Gd2CCl2 (mp-29394) 0.2223 0.014 3
Lu2CCl2 (mp-573376) 0.1489 0.000 3
Ta2CS2 (mp-559976) 0.1686 0.007 3
Ti2Te2P (mp-12527) 0.1336 0.000 3
NaLa6OsI12 (mp-569905) 0.6518 0.000 4
Na2Cl (mp-990084) 0.3744 0.104 2
PbI2 (mp-640058) 0.4020 0.004 2
HfTe2 (mp-32887) 0.3936 0.000 2
CrSe2 (mp-1009581) 0.3698 0.000 2
ZrSe2 (mp-2076) 0.4008 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Zr_sv Te P
Final Energy/Atom
-6.8747 eV
Corrected Energy
-35.2175 eV
Uncorrected energy = -34.3735 eV Composition-based energy adjustment (-0.422 eV/atom x 2.0 atoms) = -0.8440 eV Corrected energy = -35.2175 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by