Final Magnetic Moment0.864 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-0.315 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.51 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 349.8 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 262.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 174.9 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 371.6 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 247.1 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 327.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 196.8 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 153.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 65.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 284.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 284.2 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 218.6 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 21.9 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 247.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 349.8 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 240.5 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 284.2 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 65.6 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 262.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 87.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 349.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 349.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 196.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 349.8 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 349.8 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 87.4 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 262.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 284.2 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 262.3 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 247.1 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 284.2 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 87.4 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 87.4 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 262.3 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 284.2 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 349.8 |
BN (mp-984) | <1 0 0> | <0 0 1> | 153.0 |
BN (mp-984) | <1 0 1> | <0 0 1> | 240.5 |
BN (mp-984) | <1 1 0> | <0 0 1> | 65.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 65.6 |
BN (mp-984) | <0 0 1> | <0 0 1> | 21.9 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 349.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 284.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 196.8 |
Al (mp-134) | <1 0 0> | <0 0 1> | 349.8 |
Al (mp-134) | <1 1 0> | <0 0 1> | 349.8 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 349.8 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 43.7 |
Al (mp-134) | <1 1 1> | <0 0 1> | 87.4 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 247.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ce2Zn2Cu5 (mp-640899) | 0.4964 | 0.023 | 3 |
Ce2Zn2Ni5 (mp-17587) | 0.5374 | 0.004 | 3 |
Y3AlNi8 (mp-13096) | 0.6507 | 0.209 | 3 |
Sm2Co7 (mp-540547) | 0.1704 | 0.000 | 2 |
Y2Ni7 (mp-574339) | 0.1659 | 0.000 | 2 |
Th2Ni7 (mp-867004) | 0.1362 | 0.000 | 2 |
Dy2Ni7 (mp-865205) | 0.1702 | 0.000 | 2 |
La2Rh7 (mp-568375) | 0.1331 | 0.011 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: La Ni_pv |
Final Energy/Atom-5.9077 eV |
Corrected Energy-212.6762 eV
-212.6762 eV = -212.6762 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)