Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.676 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.012 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.19 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToHo2Si2O7 |
Band Gap4.618 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 132.8 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 160.9 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 132.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 354.1 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 221.3 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 284.1 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 221.3 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 354.1 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 354.1 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 284.1 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 177.0 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 265.5 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 1> | 284.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 354.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 354.1 |
CdS (mp-672) | <1 0 1> | <0 1 -1> | 266.4 |
CdS (mp-672) | <1 1 1> | <1 1 1> | 254.4 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 354.1 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 241.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 354.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 88.5 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 177.0 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 221.3 |
GaSe (mp-1943) | <0 0 1> | <1 0 1> | 279.2 |
GaSe (mp-1943) | <1 0 1> | <0 1 -1> | 266.4 |
BN (mp-984) | <0 0 1> | <1 0 1> | 93.1 |
BN (mp-984) | <1 0 1> | <1 0 1> | 279.2 |
BN (mp-984) | <1 1 0> | <0 0 1> | 309.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 221.3 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 309.8 |
LiNbO3 (mp-3731) | <1 1 1> | <0 0 1> | 132.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 354.1 |
MoS2 (mp-1434) | <0 0 1> | <1 1 1> | 254.4 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 221.3 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 309.8 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 309.8 |
C (mp-66) | <1 0 0> | <0 0 1> | 354.1 |
C (mp-66) | <1 1 0> | <0 0 1> | 309.8 |
Al (mp-134) | <1 1 0> | <0 0 1> | 354.1 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 284.1 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 221.3 |
CdTe (mp-406) | <1 1 0> | <0 1 1> | 189.4 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 221.3 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 221.3 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 309.8 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 354.1 |
BaTiO3 (mp-5986) | <1 0 0> | <1 1 1> | 254.4 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 221.3 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 309.8 |
LiTaO3 (mp-3666) | <1 1 1> | <0 0 1> | 132.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Tb2Si2O7 (mp-17308) | 0.1054 | 0.000 | 3 |
Tm2Si2O7 (mp-18318) | 0.1325 | 0.037 | 3 |
Gd2Si2O7 (mp-542469) | 0.2495 | 0.011 | 3 |
Y2Si2O7 (mp-556860) | 0.1167 | 0.036 | 3 |
Dy2Si2O7 (mp-17062) | 0.0513 | 0.005 | 3 |
CaSnP2O7 (mvc-5479) | 0.6286 | 0.034 | 4 |
Na3B(PO4)2 (mp-559783) | 0.5934 | 0.000 | 4 |
LiBiP2O7 (mp-584134) | 0.5589 | 0.035 | 4 |
CaMnP2O7 (mp-18743) | 0.6084 | 0.000 | 4 |
SrY2Si3O10 (mp-1020706) | 0.5265 | 0.012 | 4 |
Na5Ca2Al(PO4)4 (mp-559777) | 0.5796 | 0.000 | 5 |
BaNaNd(GeO3)3 (mp-14353) | 0.5129 | 0.006 | 5 |
SrTiZn(PO4)2 (mvc-2665) | 0.6462 | 0.170 | 5 |
BaNaEu(SiO3)3 (mp-1019735) | 0.6347 | 0.000 | 5 |
BaNaNd(SiO3)3 (mp-13791) | 0.6315 | 0.002 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ho_3 Si O |
Final Energy/Atom-8.1969 eV |
Corrected Energy-380.3280 eV
-380.3280 eV = -360.6638 eV (uncorrected energy) - 19.6641 eV (MP Anion Correction)
|