Final Magnetic Moment0.005 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.609 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.005 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.27 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToRb2Ga2B2O7 + Rb5B19O31 + RbLiB4O7 + LiGaO2 |
Band Gap3.667 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP2/c [13] |
Hall-P 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 252.6 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 224.3 |
LaAlO3 (mp-2920) | <1 1 1> | <0 1 0> | 252.6 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 293.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 195.5 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 142.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 162.9 |
GaAs (mp-2534) | <1 1 0> | <1 0 -1> | 142.3 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 213.5 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 222.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 228.1 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 293.3 |
GaN (mp-804) | <1 0 0> | <1 1 -1> | 220.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 293.3 |
SiO2 (mp-6930) | <0 0 1> | <1 0 -1> | 213.5 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 71.2 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 325.9 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 162.9 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 293.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 162.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 -1> | 284.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 324.7 |
ZnSe (mp-1190) | <1 1 0> | <1 0 -1> | 142.3 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 213.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 228.1 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 -1> | 142.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 325.9 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 252.6 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 260.7 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 228.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 228.1 |
LiF (mp-1138) | <1 0 0> | <1 0 -1> | 284.7 |
LiF (mp-1138) | <1 1 1> | <1 0 -1> | 142.3 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 162.9 |
Te2W (mp-22693) | <0 1 0> | <1 0 -1> | 213.5 |
Te2W (mp-22693) | <1 1 0> | <1 0 -1> | 213.5 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 97.8 |
Te2Mo (mp-602) | <1 0 0> | <1 0 -1> | 213.5 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 222.4 |
Ag (mp-124) | <1 1 1> | <1 0 1> | 148.3 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 259.8 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 325.9 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 65.2 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 130.4 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 293.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 358.5 |
GaSe (mp-1943) | <1 0 0> | <0 1 1> | 270.8 |
GaSe (mp-1943) | <1 1 0> | <0 0 1> | 228.1 |
BN (mp-984) | <0 0 1> | <0 1 1> | 180.5 |
BN (mp-984) | <1 0 1> | <0 0 1> | 162.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BaAl4O7 (mp-1019532) | 0.7144 | 0.024 | 3 |
KZn4(BO3)3 (mp-6652) | 0.3890 | 0.011 | 4 |
RbZn4(BO3)3 (mp-542143) | 0.2980 | 0.001 | 4 |
CsZn4(BO3)3 (mp-1019723) | 0.3636 | 0.006 | 4 |
BaZn2(BO3)2 (mp-557974) | 0.6721 | 0.013 | 4 |
Rb2Ga2B2O7 (mp-560010) | 0.6246 | 0.000 | 4 |
RbLi2V2(BO3)3 (mp-772424) | 0.2215 | 0.120 | 5 |
RbLi2Mn2(BO3)3 (mp-770725) | 0.3686 | 0.291 | 5 |
RbLi2Ni2(BO3)3 (mp-770719) | 0.1089 | 0.195 | 5 |
RbLi2Fe2(BO3)3 (mp-770709) | 0.1885 | 0.021 | 5 |
RbLi2Co2(BO3)3 (mp-770633) | 0.1530 | 0.185 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv Li_sv Ga_d B O |
Final Energy/Atom-6.6741 eV |
Corrected Energy-239.5606 eV
-239.5606 eV = -226.9194 eV (uncorrected energy) - 12.6412 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)