material

Ca6FeN5

ID:

mp-16916

DOI:

10.17188/1192237


Tags: Hexacalcium iron(III) nitride

Material Details

Final Magnetic Moment
2.989 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.945 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.93 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mcm [193]
Hall
-P 6c 2
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 33796 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.000 101.4
Mg (mp-153) <0 0 1> <0 0 1> 0.001 236.6
AlN (mp-661) <1 0 0> <1 0 1> 0.003 251.3
AlN (mp-661) <0 0 1> <0 0 1> 0.005 33.8
WS2 (mp-224) <1 1 1> <0 0 1> 0.005 236.6
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.008 304.2
YAlO3 (mp-3792) <0 0 1> <0 0 1> 0.013 169.0
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.019 236.6
WS2 (mp-224) <0 0 1> <0 0 1> 0.020 236.6
BaF2 (mp-1029) <1 1 0> <1 0 1> 0.034 167.5
LaF3 (mp-905) <0 0 1> <0 0 1> 0.043 135.2
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.048 304.2
Cu (mp-30) <1 1 0> <1 0 1> 0.052 167.5
C (mp-66) <1 0 0> <0 0 1> 0.052 270.4
ZnO (mp-2133) <0 0 1> <0 0 1> 0.055 236.6
BN (mp-984) <0 0 1> <0 0 1> 0.061 135.2
InSb (mp-20012) <1 1 0> <1 0 1> 0.075 251.3
SiC (mp-11714) <1 0 0> <1 0 1> 0.077 251.3
C (mp-48) <0 0 1> <0 0 1> 0.080 101.4
CeO2 (mp-20194) <1 1 0> <0 0 1> 0.083 169.0
Si (mp-149) <1 1 0> <0 0 1> 0.084 169.0
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.085 135.2
CdTe (mp-406) <1 1 0> <1 0 1> 0.086 251.3
NdGaO3 (mp-3196) <0 1 0> <0 0 1> 0.086 169.0
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.087 236.6
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.088 236.6
C (mp-66) <1 1 0> <0 0 1> 0.088 270.4
SiC (mp-8062) <1 1 0> <0 0 1> 0.090 135.2
GaSe (mp-1943) <0 0 1> <0 0 1> 0.097 236.6
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.103 76.6
InAs (mp-20305) <1 0 0> <1 0 0> 0.104 76.6
TiO2 (mp-2657) <1 1 1> <1 1 0> 0.106 265.4
SiC (mp-8062) <1 0 0> <1 0 0> 0.107 76.6
Te2Mo (mp-602) <1 0 1> <0 0 1> 0.114 169.0
ZrO2 (mp-2858) <1 0 0> <0 0 1> 0.119 169.0
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.120 153.3
MgF2 (mp-1249) <1 1 1> <0 0 1> 0.123 270.4
CdSe (mp-2691) <1 0 0> <1 0 0> 0.141 76.6
ZrO2 (mp-2858) <1 1 0> <0 0 1> 0.146 202.8
GaP (mp-2490) <1 0 0> <1 0 0> 0.146 153.3
Te2W (mp-22693) <0 0 1> <1 0 0> 0.149 153.3
Cu (mp-30) <1 0 0> <0 0 1> 0.152 270.4
SiC (mp-8062) <1 1 1> <0 0 1> 0.158 33.8
GaSb (mp-1156) <1 0 0> <1 0 0> 0.161 76.6
MgF2 (mp-1249) <1 1 0> <1 0 1> 0.167 83.8
AlN (mp-661) <1 0 1> <0 0 1> 0.167 338.0
ZrO2 (mp-2858) <0 1 0> <0 0 1> 0.178 169.0
GaN (mp-804) <1 0 1> <0 0 1> 0.180 135.2
SiC (mp-7631) <0 0 1> <0 0 1> 0.181 33.8
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.182 153.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.

Once you have registered you can also "vote" for full calculation of this material's elastic properties.

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ca6GaN5 (mp-17875) 0.2713 0.000 3
Sr6GaN5 (mp-18635) 0.1579 0.004 3
Ca6FeN5 (mvc-16363) 0.0146 0.000 3
Ca6MnN5 (mvc-16454) 0.0763 0.000 3
Ca6MnN5 (mp-17577) 0.0745 0.000 3
RbMgBO3 (mp-1020633) 0.7402 0.000 4
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv Fe_pv N
Final Energy/Atom
-5.9644 eV
Corrected Energy
-146.7568 eV
Uncorrected energy = -143.1468 eV Composition-based energy adjustment (-0.361 eV/atom x 10.0 atoms) = -3.6100 eV Corrected energy = -146.7568 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 33796
Submitted by
User remarks:
  • Hexacalcium iron(III) nitride

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)