Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.411 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.91 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.643 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 319.4 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 127.8 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 127.8 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 191.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 255.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 1> | 195.2 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 319.4 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 191.6 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 295.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 255.5 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 255.5 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 191.6 |
Te2W (mp-22693) | <1 0 0> | <0 1 0> | 295.1 |
Te2W (mp-22693) | <1 1 0> | <0 1 0> | 221.3 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 221.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 191.6 |
Al (mp-134) | <1 1 1> | <0 1 1> | 195.2 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 295.1 |
CdTe (mp-406) | <1 1 0> | <0 1 1> | 195.2 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 295.1 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 191.6 |
Al (mp-134) | <1 1 0> | <0 0 1> | 255.5 |
C (mp-66) | <1 0 0> | <0 1 0> | 295.1 |
C (mp-66) | <1 1 0> | <0 1 1> | 292.8 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 191.6 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 147.5 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 319.4 |
KP(HO2)2 (mp-23959) | <0 1 1> | <0 1 0> | 221.3 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 127.8 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 319.4 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 73.8 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 191.6 |
Ni (mp-23) | <1 1 1> | <0 1 1> | 292.8 |
Au (mp-81) | <1 1 0> | <0 0 1> | 191.6 |
C (mp-48) | <1 0 0> | <0 0 1> | 191.6 |
WSe2 (mp-1821) | <1 0 1> | <0 0 1> | 255.5 |
InSb (mp-20012) | <1 1 0> | <0 1 1> | 195.2 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 127.8 |
MoSe2 (mp-1634) | <1 0 1> | <0 0 1> | 255.5 |
Si (mp-149) | <1 1 0> | <0 0 1> | 127.8 |
CdWO4 (mp-19387) | <0 1 0> | <0 1 0> | 295.1 |
TiO2 (mp-390) | <1 1 0> | <0 0 1> | 255.5 |
C (mp-48) | <1 0 1> | <0 0 1> | 319.4 |
ZrO2 (mp-2858) | <0 0 1> | <0 1 0> | 221.3 |
MgF2 (mp-1249) | <0 0 1> | <0 1 0> | 221.3 |
ZnO (mp-2133) | <1 1 1> | <0 1 0> | 295.1 |
Cu (mp-30) | <1 1 1> | <0 0 1> | 319.4 |
Ge (mp-32) | <1 1 0> | <0 0 1> | 191.6 |
LiAlO2 (mp-3427) | <1 0 1> | <0 1 0> | 295.1 |
SiC (mp-8062) | <1 1 0> | <0 1 1> | 292.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Na_pv Ge_d As |
Final Energy/Atom-3.1840 eV |
Corrected Energy-114.6229 eV
-114.6229 eV = -114.6229 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)