Final Magnetic Moment0.012 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.106 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.007 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.23 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCu2SnS3 + SrS |
Band Gap0.412 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3121 [152] |
HallP 31 2" |
Point Group32 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 296.9 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 174.4 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 171.4 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 171.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 244.2 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 244.2 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 197.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 313.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 313.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 104.6 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 197.9 |
Te2W (mp-22693) | <1 0 1> | <1 0 0> | 99.0 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 139.5 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 99.0 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 244.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 104.6 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 139.5 |
C (mp-66) | <1 0 0> | <0 0 1> | 313.9 |
C (mp-66) | <1 1 0> | <0 0 1> | 279.1 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 313.9 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 174.4 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 34.9 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 99.0 |
Mg (mp-153) | <1 1 0> | <1 1 0> | 171.4 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 244.2 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 104.6 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 313.9 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 313.9 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 348.8 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 197.9 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 313.9 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 174.4 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 171.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 171.4 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 197.9 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 279.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 244.2 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 99.0 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 197.9 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 313.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 139.5 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 174.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 313.9 |
BN (mp-984) | <0 0 1> | <0 0 1> | 104.6 |
BN (mp-984) | <1 0 0> | <0 0 1> | 209.3 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 313.9 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 34.9 |
Al (mp-134) | <1 1 1> | <0 0 1> | 244.2 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 99.0 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 313.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
-0.25430 | 0.25430 | 0.00000 | -0.04681 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.04681 | 0.25430 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.36266 C/m2 |
Crystallographic Direction vmax |
---|
-1.00000 |
0.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
9.63 | 0.00 | 0.00 |
0.00 | 9.63 | 0.00 |
0.00 | 0.00 | 8.73 |
Dielectric Tensor εij (total) |
||
---|---|---|
16.03 | 0.00 | 0.00 |
0.00 | 16.03 | -0.00 |
0.00 | -0.00 | 13.99 |
Polycrystalline dielectric constant
εpoly∞
9.33
|
Polycrystalline dielectric constant
εpoly
15.35
|
Refractive Index n3.05 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cd4GeS6 (mp-5151) | 0.6394 | 0.012 | 3 |
CuSbSe2 (mp-20331) | 0.6093 | 0.000 | 3 |
Cd4GeSe6 (mp-18163) | 0.6072 | 0.018 | 3 |
CuSbS2 (mp-4468) | 0.6070 | 0.000 | 3 |
CuBiS2 (mp-22982) | 0.6417 | 0.000 | 3 |
SrCu2SnS4 (mp-17322) | 0.0091 | 0.007 | 4 |
BaCu2GeSe4 (mp-17252) | 0.3135 | 0.000 | 4 |
BaCu2GeS4 (mp-17947) | 0.3529 | 0.000 | 4 |
SrCu2GeS4 (mp-18685) | 0.3333 | 0.000 | 4 |
BaCu2SnS4 (mp-17954) | 0.2063 | 0.000 | 4 |
GeAs2 (mp-17524) | 0.7022 | 0.000 | 2 |
Si (mp-644693) | 0.7403 | 0.415 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sr_sv Cu_pv Sn_d S |
Final Energy/Atom-4.5792 eV |
Corrected Energy-117.8634 eV
-117.8634 eV = -109.9019 eV (uncorrected energy) - 7.9615 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)