Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.170 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.44 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.018 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 0 1> | <0 0 1> | 74.7 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 251.0 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 224.2 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 298.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 149.5 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 149.5 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 224.2 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 224.2 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 224.2 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 224.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 298.9 |
BN (mp-984) | <1 0 1> | <0 0 1> | 298.9 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 224.2 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 298.9 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 298.9 |
MgO (mp-1265) | <1 0 0> | <1 1 0> | 180.5 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 224.2 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 74.7 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 224.2 |
PbS (mp-21276) | <1 0 0> | <1 1 0> | 180.5 |
InP (mp-20351) | <1 0 0> | <1 1 0> | 180.5 |
WSe2 (mp-1821) | <0 0 1> | <0 1 0> | 251.0 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 149.5 |
BaTiO3 (mp-5986) | <1 0 1> | <0 1 0> | 251.0 |
MoSe2 (mp-1634) | <0 0 1> | <0 1 0> | 251.0 |
Si (mp-149) | <1 0 0> | <0 0 1> | 149.5 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 224.2 |
C (mp-48) | <0 0 1> | <0 0 1> | 298.9 |
C (mp-48) | <1 0 1> | <0 0 1> | 298.9 |
C (mp-48) | <1 1 0> | <0 0 1> | 298.9 |
C (mp-48) | <1 1 1> | <0 0 1> | 298.9 |
ZrO2 (mp-2858) | <1 1 -1> | <1 1 0> | 180.5 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 1> | 178.1 |
ZnO (mp-2133) | <1 0 1> | <1 0 0> | 159.9 |
ZnO (mp-2133) | <1 1 1> | <0 0 1> | 224.2 |
GaSb (mp-1156) | <1 1 0> | <0 0 1> | 224.2 |
Cu (mp-30) | <1 0 0> | <0 1 0> | 251.0 |
GaTe (mp-542812) | <1 0 1> | <0 0 1> | 298.9 |
LiAlO2 (mp-3427) | <1 0 0> | <0 0 1> | 224.2 |
ZnTe (mp-2176) | <1 1 0> | <0 0 1> | 224.2 |
LiAlO2 (mp-3427) | <1 0 1> | <0 0 1> | 298.9 |
Al2O3 (mp-1143) | <0 0 1> | <0 0 1> | 298.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
6.72 | 0.00 | 0.08 |
0.00 | 6.29 | 0.00 |
0.08 | 0.00 | 6.62 |
Dielectric Tensor εij (total) |
||
---|---|---|
14.63 | 0.00 | -0.46 |
0.00 | 12.72 | 0.00 |
-0.46 | 0.00 | 16.35 |
Polycrystalline dielectric constant
εpoly∞
6.54
|
Polycrystalline dielectric constant
εpoly
14.56
|
Refractive Index n2.56 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ba2MgO3 (mp-779511) | 0.4033 | 0.030 | 3 |
Ba2TaN3 (mp-17400) | 0.1940 | 0.000 | 3 |
Sr2TaN3 (mp-17518) | 0.4262 | 0.000 | 3 |
Ca2VN3 (mp-17892) | 0.4933 | 0.000 | 3 |
Sr2VN3 (mp-17012) | 0.4151 | 0.000 | 3 |
Ba4LiW2N7 (mp-6665) | 0.6096 | 0.000 | 4 |
Ba4LiMo2N7 (mp-6011) | 0.5913 | 0.000 | 4 |
Na6U2Mo4O21 (mp-704703) | 0.6633 | 0.004 | 4 |
K3Np(MoO5)2 (mp-616718) | 0.6543 | 0.000 | 4 |
K6W2N4O3 (mp-744081) | 0.6482 | 0.265 | 4 |
K2LiVPO6 (mp-764301) | 0.7368 | 0.081 | 5 |
Na2TeHSO5F3 (mp-696485) | 0.7469 | 0.016 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Nb_pv N |
Final Energy/Atom-7.4696 eV |
Corrected Energy-179.2693 eV
-179.2693 eV = -179.2693 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)