Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.590 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.68 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinIm3m [229] |
Hall-I 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 1> | 135.9 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 78.5 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 110.9 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 78.5 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 110.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 313.8 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 110.9 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 78.5 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 156.9 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 221.9 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 235.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 1> | 135.9 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 221.9 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 235.4 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 313.8 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 313.8 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 235.4 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 313.8 |
LaF3 (mp-905) | <0 0 1> | <1 1 1> | 135.9 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 313.8 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 156.9 |
InP (mp-20351) | <1 0 0> | <1 0 0> | 313.8 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 313.8 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 78.5 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 110.9 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 156.9 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 313.8 |
Au (mp-81) | <1 0 0> | <1 0 0> | 156.9 |
Au (mp-81) | <1 1 0> | <1 1 0> | 221.9 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 78.5 |
Ga2O3 (mp-886) | <1 1 0> | <1 1 0> | 221.9 |
CdSe (mp-2691) | <1 1 0> | <1 1 0> | 110.9 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 156.9 |
CaCO3 (mp-3953) | <1 1 0> | <1 0 0> | 156.9 |
YAlO3 (mp-3792) | <1 0 1> | <1 0 0> | 235.4 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <1 0 0> | 156.9 |
CsI (mp-614603) | <1 0 0> | <1 0 0> | 313.8 |
MgF2 (mp-1249) | <1 1 1> | <1 0 0> | 235.4 |
GaSb (mp-1156) | <1 0 0> | <1 0 0> | 78.5 |
GaSb (mp-1156) | <1 1 0> | <1 1 0> | 110.9 |
MgF2 (mp-1249) | <1 0 0> | <1 0 0> | 235.4 |
SrTiO3 (mp-4651) | <1 1 0> | <1 0 0> | 313.8 |
Cu (mp-30) | <1 1 0> | <1 1 0> | 110.9 |
SrTiO3 (mp-4651) | <0 0 1> | <1 0 0> | 156.9 |
GaTe (mp-542812) | <0 0 1> | <1 1 0> | 221.9 |
ZnTe (mp-2176) | <1 0 0> | <1 0 0> | 78.5 |
ZnTe (mp-2176) | <1 1 0> | <1 1 0> | 110.9 |
CaF2 (mp-2741) | <1 0 0> | <1 0 0> | 156.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sm3(GaNi3)2 (mp-504614) | 0.1099 | 0.000 | 3 |
Sm3(AlNi3)2 (mp-573541) | 0.0902 | 0.000 | 3 |
Ho3(AlNi3)2 (mp-30791) | 0.0372 | 0.000 | 3 |
Dy3(AlNi3)2 (mp-16807) | 0.0217 | 0.000 | 3 |
Y3(AlNi3)2 (mp-4577) | 0.0814 | 0.000 | 3 |
Ca3Ag8 (mp-646824) | 0.5455 | 0.028 | 2 |
TmMn2 (mp-30786) | 0.6481 | 0.033 | 2 |
SrZn2 (mp-13365) | 0.6798 | 0.049 | 2 |
ErMn2 (mp-913259) | 0.6543 | 0.042 | 2 |
NdMn2 (mp-569334) | 0.6351 | 0.436 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Er_3 Al Ni_pv |
Final Energy/Atom-5.6692 eV |
Corrected Energy-124.7215 eV
-124.7215 eV = -124.7215 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)