material

PuN

ID:

mp-1719

DOI:

10.17188/1192383


Tags: Plutonium(III) nitride Plutonium nitride (1/1)

Material Details

Final Magnetic Moment
4.810 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FiM
Formation Energy / Atom
-1.478 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
14.20 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fm3m [225]
Hall
-F 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 31718 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CdTe (mp-406) <1 0 0> <1 0 0> 0.000 219.8
InSb (mp-20012) <1 0 0> <1 0 0> 0.001 219.8
BN (mp-984) <0 0 1> <1 1 1> 0.003 169.2
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.003 69.1
Al (mp-134) <1 1 0> <1 1 0> 0.004 69.1
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.008 195.3
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.009 122.1
Fe2O3 (mp-24972) <0 0 1> <1 1 1> 0.012 296.0
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.015 122.1
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.016 219.8
NaCl (mp-22862) <1 1 1> <1 1 1> 0.021 169.2
NaCl (mp-22862) <1 1 0> <1 1 0> 0.021 138.1
Cu (mp-30) <1 1 1> <1 1 1> 0.024 296.0
AlN (mp-661) <1 0 1> <1 0 0> 0.028 268.6
Fe3O4 (mp-19306) <1 1 1> <1 1 1> 0.030 126.9
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.030 219.8
Fe3O4 (mp-19306) <1 1 0> <1 1 0> 0.030 103.6
C (mp-48) <1 0 0> <1 0 0> 0.030 268.6
GaN (mp-804) <0 0 1> <1 1 1> 0.033 169.2
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.036 310.8
GaP (mp-2490) <1 0 0> <1 0 0> 0.039 122.1
PbSe (mp-2201) <1 0 0> <1 0 0> 0.050 195.3
Ni (mp-23) <1 1 0> <1 1 0> 0.055 34.5
Ni (mp-23) <1 1 1> <1 0 0> 0.056 170.9
Ni (mp-23) <1 0 0> <1 0 0> 0.057 24.4
TePb (mp-19717) <1 1 1> <1 1 1> 0.070 296.0
WS2 (mp-224) <0 0 1> <1 1 1> 0.081 169.2
Mg (mp-153) <1 1 1> <1 0 0> 0.082 122.1
MoS2 (mp-1434) <0 0 1> <1 1 1> 0.082 169.2
C (mp-48) <1 0 1> <1 1 0> 0.086 241.7
ZnO (mp-2133) <1 0 1> <1 1 1> 0.089 296.0
GaSb (mp-1156) <1 0 0> <1 0 0> 0.089 195.3
MgO (mp-1265) <1 1 1> <1 1 1> 0.097 126.9
BaF2 (mp-1029) <1 0 0> <1 0 0> 0.097 195.3
MgO (mp-1265) <1 1 0> <1 1 0> 0.098 103.6
LiGaO2 (mp-5854) <1 1 1> <1 1 0> 0.103 276.3
GaN (mp-804) <1 1 1> <1 0 0> 0.113 122.1
CsI (mp-614603) <1 0 0> <1 0 0> 0.124 122.1
CdSe (mp-2691) <1 0 0> <1 0 0> 0.127 195.3
YAlO3 (mp-3792) <0 1 1> <1 1 1> 0.130 338.3
ZnSe (mp-1190) <1 1 1> <1 1 1> 0.141 169.2
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.142 138.1
LiF (mp-1138) <1 0 0> <1 0 0> 0.164 219.8
Mg (mp-153) <0 0 1> <1 1 1> 0.169 169.2
CdWO4 (mp-19387) <1 0 0> <1 1 1> 0.175 126.9
GdScO3 (mp-5690) <0 1 1> <1 1 0> 0.198 276.3
LiAlO2 (mp-3427) <1 1 1> <1 0 0> 0.198 219.8
C (mp-48) <0 0 1> <1 0 0> 0.198 170.9
ZrO2 (mp-2858) <1 1 0> <1 1 0> 0.204 276.3
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.204 195.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
292 85 85 0 0 0
85 292 85 0 0 0
85 85 292 0 0 0
0 0 0 83 0 0
0 0 0 0 83 0
0 0 0 0 0 83
Compliance Tensor Sij (10-12Pa-1)
3.9 -0.9 -0.9 0 0 0
-0.9 3.9 -0.9 0 0 0
-0.9 -0.9 3.9 0 0 0
0 0 0 12 0 0
0 0 0 0 12 0
0 0 0 0 0 12
Shear Modulus GV
91 GPa
Bulk Modulus KV
154 GPa
Shear Modulus GR
90 GPa
Bulk Modulus KR
154 GPa
Shear Modulus GVRH
91 GPa
Bulk Modulus KVRH
154 GPa
Elastic Anisotropy
0.06
Poisson's Ratio
0.25

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Sr4SO3 (mp-1079788) 0.0000 0.200 3
BaSr3O4 (mp-984729) 0.0000 0.044 3
ScH4Pd3 (mp-981386) 0.0000 0.039 3
Sr3CdO4 (mp-981103) 0.0000 0.019 3
SrCa3O4 (mp-978844) 0.0000 0.040 3
YBi (mp-23241) 0.0000 0.000 2
EuN (mp-20340) 0.0000 0.000 2
NpC (mp-2546) 0.0000 0.171 2
HoSb (mp-2050) 0.0000 0.000 2
EuO (mp-21394) 0.0000 0.000 2
As (mp-10) 0.0000 0.126 1
Sc (mp-1008681) 0.0000 0.719 1
Ca (mp-10683) 0.0000 0.393 1
C (mp-998866) 0.0000 2.763 1
Sb (mp-133) 0.0000 0.051 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Pu N
Final Energy/Atom
-12.5878 eV
Corrected Energy
-25.1756 eV
-25.1756 eV = -25.1756 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 644641
  • 76444
  • 644639
  • 644643
  • 603919
  • 31718
  • 644640
Submitted by
User remarks:
  • Plutonium nitride (1/1)