material

CaZn5

ID:

mp-1734

DOI:

10.17188/1192457


Tags: Calcium zinc (1/5)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.228 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.68 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P6/mmm [191]
Hall
-P 6 2
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 58947 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
YAlO3 (mp-3792) <1 0 0> <1 0 0> 0.003 160.7
LaAlO3 (mp-2920) <1 0 1> <0 0 1> 0.004 75.7
LaAlO3 (mp-2920) <1 1 1> <0 0 1> 0.004 126.1
SiO2 (mp-6930) <1 0 1> <1 1 1> 0.008 141.3
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.011 25.2
CdTe (mp-406) <1 1 1> <0 0 1> 0.013 75.7
BaTiO3 (mp-5986) <0 0 1> <1 0 1> 0.017 238.8
KP(HO2)2 (mp-23959) <0 1 0> <1 0 0> 0.019 229.5
Cu (mp-30) <1 0 0> <1 0 1> 0.019 272.9
InSb (mp-20012) <1 1 1> <0 0 1> 0.019 75.7
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.020 176.6
C (mp-48) <0 0 1> <0 0 1> 0.021 100.9
C (mp-48) <1 1 0> <1 1 0> 0.024 198.8
ZnO (mp-2133) <0 0 1> <0 0 1> 0.025 176.6
AlN (mp-661) <0 0 1> <0 0 1> 0.025 25.2
BaF2 (mp-1029) <1 0 0> <1 0 1> 0.029 238.8
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.030 302.7
Mg (mp-153) <1 1 1> <1 0 1> 0.033 272.9
AlN (mp-661) <1 1 0> <1 0 1> 0.035 136.4
SiC (mp-11714) <1 0 0> <1 1 1> 0.035 94.2
TiO2 (mp-390) <0 0 1> <1 0 1> 0.037 102.3
SiC (mp-8062) <1 1 1> <0 0 1> 0.060 100.9
TePb (mp-19717) <1 1 1> <0 0 1> 0.069 75.7
Ga2O3 (mp-886) <1 0 1> <1 1 0> 0.070 278.3
SiC (mp-7631) <0 0 1> <0 0 1> 0.072 25.2
SiC (mp-11714) <0 0 1> <0 0 1> 0.078 25.2
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.080 298.4
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.081 75.7
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.082 302.7
BaTiO3 (mp-5986) <1 1 0> <1 1 0> 0.083 119.3
KP(HO2)2 (mp-23959) <0 0 1> <1 0 0> 0.088 229.5
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.088 328.0
SrTiO3 (mp-4651) <1 1 1> <1 1 0> 0.089 278.3
DyScO3 (mp-31120) <0 1 1> <1 0 0> 0.089 160.7
GaSe (mp-1943) <0 0 1> <1 0 0> 0.090 114.8
GdScO3 (mp-5690) <1 0 0> <0 0 1> 0.093 328.0
InSb (mp-20012) <1 1 0> <1 1 1> 0.102 188.3
AlN (mp-661) <1 1 1> <1 0 0> 0.103 114.8
LiGaO2 (mp-5854) <0 1 0> <1 0 0> 0.108 229.5
MgO (mp-1265) <1 0 0> <1 0 0> 0.108 91.8
KP(HO2)2 (mp-23959) <1 1 0> <1 0 1> 0.111 136.4
CdTe (mp-406) <1 1 0> <1 1 1> 0.114 188.3
BN (mp-984) <1 0 1> <1 0 1> 0.115 102.3
TbScO3 (mp-31119) <0 1 1> <1 0 0> 0.116 160.7
C (mp-66) <1 0 0> <1 0 1> 0.117 272.9
Ag (mp-124) <1 1 1> <1 1 1> 0.121 329.6
BaTiO3 (mp-5986) <1 1 1> <1 1 1> 0.122 141.3
Cu (mp-30) <1 1 0> <1 0 1> 0.129 272.9
CdS (mp-672) <1 0 1> <1 1 0> 0.131 198.8
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.131 227.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
102 39 31 0 0 0
39 102 31 0 0 0
31 31 150 0 0 0
0 0 0 41 0 0
0 0 0 0 41 0
0 0 0 0 0 31
Compliance Tensor Sij (10-12Pa-1)
11.9 -4 -1.6 0 0 0
-4 11.9 -1.6 0 0 0
-1.6 -1.6 7.3 0 0 0
0 0 0 24.4 0 0
0 0 0 0 24.4 0
0 0 0 0 0 31.8
Shear Modulus GV
39 GPa
Bulk Modulus KV
62 GPa
Shear Modulus GR
38 GPa
Bulk Modulus KR
61 GPa
Shear Modulus GVRH
39 GPa
Bulk Modulus KVRH
61 GPa
Elastic Anisotropy
0.22
Poisson's Ratio
0.24

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
UAl3Ni2 (mp-2903) 0.0348 0.105 3
GdAl3Pd2 (mp-22505) 0.0825 0.000 3
UAl3Pd2 (mp-4561) 0.0040 0.080 3
CeAl3Pd2 (mp-4785) 0.0471 0.000 3
LaGa3Pd2 (mp-21201) 0.0067 0.000 3
LaCo5 (mp-1731) 0.0052 0.026 2
BaPd5 (mp-2606) 0.0039 0.000 2
PrZn5 (mp-12602) 0.0067 0.008 2
LaZn5 (mp-2424) 0.0071 0.007 2
CaCu5 (mp-1882) 0.0054 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv Zn
Final Energy/Atom
-1.6120 eV
Corrected Energy
-9.6719 eV
-9.6719 eV = -9.6719 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 58947
  • 619638
  • 418614
Submitted by
User remarks:
  • Calcium zinc (1/5)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)