Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.832 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.03 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.544 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KCl (mp-23193) | <1 0 0> | <0 0 1> | 256.4 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 307.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 153.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 205.1 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 307.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 153.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 102.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 307.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 209.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 256.4 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 256.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 51.3 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 209.4 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 102.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 153.8 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 256.4 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 256.4 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 91.3 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 256.4 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 273.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 256.4 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 256.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 91.3 |
Bi2Se3 (mp-541837) | <1 0 1> | <0 0 1> | 256.4 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 307.6 |
Al (mp-134) | <1 1 0> | <0 1 1> | 209.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 51.3 |
BN (mp-984) | <0 0 1> | <0 1 0> | 273.9 |
TeO2 (mp-2125) | <0 1 0> | <0 0 1> | 205.1 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 102.5 |
Al (mp-134) | <1 0 0> | <0 0 1> | 307.6 |
Al (mp-134) | <1 1 1> | <0 0 1> | 256.4 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 153.8 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 307.6 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 256.4 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 205.1 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 205.1 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 307.6 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 256.4 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 307.6 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 256.4 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 307.6 |
C (mp-66) | <1 1 0> | <0 0 1> | 256.4 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 102.5 |
PbS (mp-21276) | <1 1 1> | <0 1 0> | 182.6 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 153.8 |
InP (mp-20351) | <1 1 1> | <0 1 0> | 182.6 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 307.6 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 307.6 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 256.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CsHo3Te5 (mp-18505) | 0.2142 | 0.000 | 3 |
TlIn5Se7 (mp-574279) | 0.5868 | 0.020 | 3 |
TlIn5S7 (mp-562480) | 0.5415 | 0.000 | 3 |
Mn(SbS2)2 (mp-10412) | 0.6017 | 0.013 | 3 |
InBiS3 (mp-1078776) | 0.4968 | 0.003 | 3 |
Li4Ti5VO12 (mp-771445) | 0.6456 | 0.105 | 4 |
LiCoCuO4 (mp-764366) | 0.5985 | 0.062 | 4 |
Li2Ti2VO6 (mp-774083) | 0.6340 | 0.078 | 4 |
Li4Co5SbO12 (mp-761626) | 0.6023 | 0.069 | 4 |
Li2Mn2NiO6 (mp-565580) | 0.6413 | 0.069 | 4 |
In6Se7 (mp-567596) | 0.5826 | 0.042 | 2 |
In6S7 (mp-555853) | 0.5540 | 0.008 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cs_sv Er_3 Se |
Final Energy/Atom-5.3965 eV |
Corrected Energy-194.2742 eV
-194.2742 eV = -194.2742 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)