material

Sr2TaN3

ID:

mp-17518

DOI:

10.17188/1192552


Tags: Distrontium trinitridotantalate

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.332 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.06 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
2.484 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
C2/c [15]
Hall
-C 2yc
Point Group
2/m
Crystal System
monoclinic

Electronic Structure

Topological data for ICSD ID 96126 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
BaTiO3 (mp-5986) <1 1 0> <1 0 0> 0.013 143.9
BN (mp-984) <1 1 1> <0 1 0> 0.046 307.8
MgO (mp-1265) <1 1 0> <0 0 1> 0.056 206.8
ZnO (mp-2133) <1 1 0> <0 0 1> 0.088 275.8
TeO2 (mp-2125) <0 0 1> <1 1 0> 0.090 163.2
Mg (mp-153) <1 0 0> <0 1 0> 0.097 230.9
SiO2 (mp-6930) <1 0 0> <0 1 0> 0.099 307.8
AlN (mp-661) <1 0 1> <1 0 0> 0.104 143.9
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.106 275.8
CdWO4 (mp-19387) <0 0 1> <0 0 1> 0.111 275.8
PbS (mp-21276) <1 1 0> <0 0 1> 0.112 206.8
BaTiO3 (mp-5986) <1 0 1> <0 1 1> 0.113 206.7
Al (mp-134) <1 0 0> <0 0 1> 0.117 275.8
Ga2O3 (mp-886) <1 0 0> <0 0 1> 0.186 275.8
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.192 275.8
DyScO3 (mp-31120) <0 0 1> <0 1 0> 0.196 153.9
WS2 (mp-224) <1 0 0> <1 1 1> 0.271 179.2
MgF2 (mp-1249) <1 0 0> <0 1 0> 0.280 307.8
Mg (mp-153) <1 1 1> <0 1 1> 0.292 206.7
GaN (mp-804) <0 0 1> <1 0 0> 0.294 143.9
TbScO3 (mp-31119) <0 0 1> <0 1 0> 0.323 153.9
MgAl2O4 (mp-3536) <1 1 0> <0 0 1> 0.391 275.8
Te2Mo (mp-602) <1 1 0> <0 0 1> 0.399 275.8
YAlO3 (mp-3792) <0 0 1> <0 1 0> 0.410 307.8
C (mp-66) <1 1 0> <0 1 0> 0.412 307.8
TbScO3 (mp-31119) <0 1 0> <0 1 0> 0.416 307.8
GdScO3 (mp-5690) <0 1 0> <0 1 0> 0.420 307.8
InP (mp-20351) <1 1 0> <0 0 1> 0.421 206.8
DyScO3 (mp-31120) <0 1 0> <0 1 0> 0.457 307.8
BN (mp-984) <1 0 1> <0 1 0> 0.470 307.8
Au (mp-81) <1 1 0> <0 0 1> 0.524 275.8
ZrO2 (mp-2858) <0 1 0> <0 1 0> 0.528 230.9
MgF2 (mp-1249) <1 1 0> <0 0 1> 0.557 206.8
CdWO4 (mp-19387) <1 0 1> <0 0 1> 0.587 137.9
NdGaO3 (mp-3196) <0 1 0> <0 1 0> 0.599 307.8
ZrO2 (mp-2858) <1 0 0> <0 1 0> 0.609 307.8
WS2 (mp-224) <1 1 0> <1 0 1> 0.612 161.8
TiO2 (mp-2657) <1 0 1> <0 0 1> 0.669 206.8
AlN (mp-661) <1 1 1> <0 0 1> 0.672 206.8
ZnO (mp-2133) <1 0 1> <0 0 1> 0.672 137.9
GdScO3 (mp-5690) <0 0 1> <0 1 0> 0.676 153.9
SiO2 (mp-6930) <1 1 0> <0 1 0> 0.676 230.9
ZrO2 (mp-2858) <1 0 -1> <1 1 1> 0.679 179.2
InAs (mp-20305) <1 1 0> <0 0 1> 1.022 206.8
ZnTe (mp-2176) <1 1 0> <0 0 1> 1.072 206.8
CsI (mp-614603) <1 1 0> <0 0 1> 1.173 275.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
127 44 36 0 -0 0
44 144 36 0 14 0
36 36 120 0 12 0
0 0 0 28 0 6
-0 14 12 0 38 0
0 0 0 6 0 37
Compliance Tensor Sij (10-12Pa-1)
9.3 -2.4 -2.2 0 1.7 0
-2.4 8.3 -1.5 0 -2.5 0
-2.2 -1.5 9.7 0 -2.6 0
0 0 0 37.1 0 -6.1
1.7 -2.5 -2.6 0 27.8 0
0 0 0 -6.1 0 28.1
Shear Modulus GV
39 GPa
Bulk Modulus KV
69 GPa
Shear Modulus GR
36 GPa
Bulk Modulus KR
67 GPa
Shear Modulus GVRH
38 GPa
Bulk Modulus KVRH
68 GPa
Elastic Anisotropy
0.41
Poisson's Ratio
0.27

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
5.81 0.00 0.04
0.00 5.54 0.00
0.04 0.00 5.92
Dielectric Tensor εij (total)
10.47 0.00 -0.14
0.00 9.68 0.00
-0.14 0.00 11.14
Polycrystalline dielectric constant εpoly
(electronic contribution)
5.76
Polycrystalline dielectric constant εpoly
(total)
10.43
Refractive Index n
2.40
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ba2MgO3 (mp-779511) 0.3922 0.030 3
Sr2NbN3 (mp-17701) 0.1398 0.000 3
Ca2VN3 (mp-17892) 0.2377 0.000 3
Ba2ZnO3 (mp-17911) 0.4340 0.000 3
Ba2NbN3 (mp-17024) 0.4262 0.000 3
Ba4LiW2N7 (mp-6665) 0.6199 0.000 4
Ba4LiMo2N7 (mp-6011) 0.6064 0.000 4
Li3Sb(PO4)2 (mp-777071) 0.6516 0.069 4
K6W2N4O3 (mp-744081) 0.6192 0.265 4
LiMnPO4 (mp-859131) 0.6301 0.091 4
RbSrSiHO4 (mp-995216) 0.7147 0.018 5
KBaSiHO4 (mp-995194) 0.7204 0.011 5
KCaSiHO4 (mp-995190) 0.7055 0.016 5
NaCaSiHO4 (mp-634418) 0.6949 0.000 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Sr_sv Ta_pv N
Final Energy/Atom
-7.8477 eV
Corrected Energy
-192.6770 eV
Uncorrected energy = -188.3450 eV Composition-based energy adjustment (-0.361 eV/atom x 12.0 atoms) = -4.3320 eV Corrected energy = -192.6770 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 96126
Submitted by
User remarks:
  • Distrontium trinitridotantalate

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)