material

Sr2NbN3

ID:

mp-17701

DOI:

10.17188/1192644


Tags: Distrontium niobium nitride

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Unknown
Formation Energy / Atom
-1.234 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.73 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
2.293 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
C2/c [15]
Hall
-C 2yc
Point Group
2/m
Crystal System
monoclinic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
BaTiO3 (mp-5986) <1 1 0> <1 0 0> 0.001 143.1
BN (mp-984) <1 1 1> <0 1 0> 0.031 308.2
TeO2 (mp-2125) <0 0 1> <1 1 0> 0.050 162.5
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.061 275.6
Mg (mp-153) <1 0 0> <0 1 0> 0.074 231.2
Al (mp-134) <1 0 0> <0 0 1> 0.075 275.6
MgO (mp-1265) <1 1 0> <0 0 1> 0.091 206.7
AlN (mp-661) <1 0 1> <1 0 0> 0.100 143.1
Ga2O3 (mp-886) <1 0 0> <0 0 1> 0.136 275.6
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.138 275.6
DyScO3 (mp-31120) <0 0 1> <0 1 0> 0.142 154.1
PbS (mp-21276) <1 1 0> <0 0 1> 0.142 206.7
MgF2 (mp-1249) <1 0 0> <0 1 0> 0.186 308.2
ZnO (mp-2133) <1 1 0> <0 1 0> 0.191 154.1
CdWO4 (mp-19387) <0 0 1> <0 0 1> 0.195 275.6
C (mp-66) <1 1 0> <0 1 0> 0.221 231.2
Cu (mp-30) <1 0 0> <0 0 1> 0.222 275.6
TiO2 (mp-2657) <1 0 0> <0 1 0> 0.225 231.2
WS2 (mp-224) <1 0 0> <1 1 1> 0.233 178.9
GdScO3 (mp-5690) <0 1 0> <0 1 0> 0.246 308.2
GaN (mp-804) <0 0 1> <1 0 0> 0.251 143.1
TbScO3 (mp-31119) <0 0 1> <0 1 0> 0.263 154.1
TbScO3 (mp-31119) <0 1 0> <0 1 0> 0.266 308.2
Mg (mp-153) <1 1 1> <0 1 1> 0.300 206.7
DyScO3 (mp-31120) <0 1 0> <0 1 0> 0.318 308.2
Au (mp-81) <1 1 0> <0 0 1> 0.375 275.6
MgF2 (mp-1249) <1 1 0> <0 0 1> 0.400 206.7
InP (mp-20351) <1 1 0> <0 0 1> 0.439 206.7
Te2Mo (mp-602) <1 1 0> <0 0 1> 0.455 275.6
Te2W (mp-22693) <1 1 1> <0 1 0> 0.462 231.2
MgF2 (mp-1249) <1 0 1> <0 0 1> 0.467 206.7
Ag (mp-124) <1 1 0> <0 0 1> 0.477 275.6
MgAl2O4 (mp-3536) <1 1 0> <0 0 1> 0.485 275.6
TiO2 (mp-2657) <1 0 1> <0 0 1> 0.495 206.7
ZnO (mp-2133) <1 0 1> <0 0 1> 0.496 137.8
WS2 (mp-224) <1 1 0> <1 0 1> 0.517 161.5
BN (mp-984) <1 0 1> <0 1 0> 0.531 308.2
CdWO4 (mp-19387) <1 0 1> <0 0 1> 0.541 137.8
YAlO3 (mp-3792) <0 0 1> <0 1 0> 0.554 308.2
NdGaO3 (mp-3196) <0 1 0> <0 1 0> 0.560 308.2
TeO2 (mp-2125) <1 0 0> <1 0 0> 0.589 143.1
SiO2 (mp-6930) <1 1 0> <0 1 0> 0.609 231.2
GdScO3 (mp-5690) <0 0 1> <0 1 0> 0.614 154.1
Cu (mp-30) <1 1 0> <0 0 1> 0.637 275.6
PbSe (mp-2201) <1 1 0> <0 0 1> 0.647 275.6
GaSb (mp-1156) <1 1 0> <0 0 1> 0.666 275.6
LaF3 (mp-905) <1 1 0> <0 0 1> 0.675 275.6
CdSe (mp-2691) <1 1 0> <0 0 1> 0.686 275.6
AlN (mp-661) <1 1 1> <0 0 1> 0.709 206.7
TeO2 (mp-2125) <0 1 0> <1 0 0> 0.848 143.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
131 47 40 0 -2 0
47 148 39 0 13 0
40 39 120 0 11 0
0 0 0 29 0 5
-2 13 11 0 37 0
0 0 0 5 0 37
Compliance Tensor Sij (10-12Pa-1)
9.3 -2.5 -2.5 0 2.2 0
-2.5 8.2 -1.6 0 -2.5 0
-2.5 -1.6 10 0 -2.5 0
0 0 0 35.5 0 -5.1
2.2 -2.5 -2.5 0 28.9 0
0 0 0 -5.1 0 27.7
Shear Modulus GV
39 GPa
Bulk Modulus KV
72 GPa
Shear Modulus GR
36 GPa
Bulk Modulus KR
70 GPa
Shear Modulus GVRH
38 GPa
Bulk Modulus KVRH
71 GPa
Elastic Anisotropy
0.35
Poisson's Ratio
0.28

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
36
U Values
--
Pseudopotentials
VASP PAW: N Sr_sv Nb_pv
Final Energy/Atom
-7.4573 eV
Corrected Energy
-178.9754 eV
-178.9754 eV = -178.9754 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 51028

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)