material

Yb2SiO5

ID:

mp-17702

DOI:

10.17188/1192645


Tags: Diytterbium oxide silicate

Material Details

Final Magnetic Moment
1.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-2.862 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.190 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.80 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
YbSiO3 + YbO + O2
Band Gap
0.118 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
C2/c [15]
Hall
-C 2yc
Point Group
2/m
Crystal System
monoclinic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
NdGaO3 (mp-3196) <1 0 1> <1 0 0> 0.004 214.2
Te2W (mp-22693) <0 0 1> <1 0 1> 0.009 155.6
TiO2 (mp-2657) <1 0 0> <1 0 -1> 0.012 318.6
Te2W (mp-22693) <1 0 1> <0 0 1> 0.016 100.9
Mg (mp-153) <1 0 0> <0 0 1> 0.016 100.9
TbScO3 (mp-31119) <1 1 0> <1 0 -1> 0.028 318.6
BaTiO3 (mp-5986) <1 1 0> <1 0 -1> 0.032 239.0
GaN (mp-804) <1 0 0> <0 0 1> 0.036 100.9
CdS (mp-672) <0 0 1> <1 0 0> 0.038 214.2
CsI (mp-614603) <1 1 1> <1 0 0> 0.038 214.2
Te2Mo (mp-602) <0 0 1> <1 0 0> 0.039 142.8
DyScO3 (mp-31120) <1 1 0> <1 0 -1> 0.040 318.6
GaN (mp-804) <0 0 1> <1 0 0> 0.041 71.4
SrTiO3 (mp-4651) <1 0 1> <1 0 0> 0.042 214.2
C (mp-48) <0 0 1> <1 0 0> 0.043 142.8
SiC (mp-11714) <0 0 1> <1 0 0> 0.051 214.2
Bi2Se3 (mp-541837) <0 0 1> <1 0 0> 0.053 214.2
SiC (mp-7631) <0 0 1> <1 0 0> 0.054 214.2
Ni (mp-23) <1 0 0> <1 0 -1> 0.055 159.3
YVO4 (mp-19133) <1 0 0> <1 0 -1> 0.071 318.6
KCl (mp-23193) <1 1 0> <1 0 0> 0.074 285.6
BaF2 (mp-1029) <1 0 0> <1 0 -1> 0.076 79.7
Y3Fe5O12 (mp-19648) <1 0 0> <1 0 -1> 0.083 159.3
LiGaO2 (mp-5854) <1 1 0> <1 0 0> 0.101 142.8
LiAlO2 (mp-3427) <1 0 0> <0 0 1> 0.101 100.9
BN (mp-984) <1 0 0> <1 0 0> 0.117 214.2
BaTiO3 (mp-5986) <1 0 0> <1 0 0> 0.123 285.6
LiAlO2 (mp-3427) <1 1 0> <1 0 0> 0.125 142.8
AlN (mp-661) <0 0 1> <1 0 -1> 0.127 239.0
YAlO3 (mp-3792) <1 1 1> <1 0 -1> 0.133 318.6
MgF2 (mp-1249) <1 0 1> <1 0 0> 0.136 214.2
Au (mp-81) <1 0 0> <1 0 -1> 0.159 159.3
NaCl (mp-22862) <1 0 0> <1 0 -1> 0.165 159.3
NdGaO3 (mp-3196) <0 1 1> <1 0 0> 0.166 214.2
CdWO4 (mp-19387) <1 1 0> <1 0 0> 0.170 285.6
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.171 214.2
AlN (mp-661) <1 0 1> <1 0 0> 0.187 71.4
SiC (mp-8062) <1 0 0> <0 1 1> 0.191 172.0
Al2O3 (mp-1143) <0 0 1> <1 0 0> 0.213 142.8
BaF2 (mp-1029) <1 1 0> <1 0 0> 0.215 285.6
SrTiO3 (mp-4651) <1 1 0> <1 0 -1> 0.241 318.6
YVO4 (mp-19133) <1 1 0> <1 0 -1> 0.260 318.6
AlN (mp-661) <1 0 0> <1 0 1> 0.267 155.6
CdS (mp-672) <1 0 0> <1 0 -1> 0.274 318.6
LiGaO2 (mp-5854) <1 0 0> <1 0 0> 0.282 71.4
SiC (mp-11714) <1 0 1> <1 0 0> 0.310 285.6
PbSe (mp-2201) <1 0 0> <1 0 -1> 0.323 79.7
SrTiO3 (mp-4651) <0 0 1> <1 0 -1> 0.336 159.3
KCl (mp-23193) <1 0 0> <1 0 -1> 0.348 79.7
GaSb (mp-1156) <1 0 0> <1 0 -1> 0.376 79.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
124 63 44 0 3 0
63 123 63 0 -4 0
44 63 143 0 15 0
0 0 0 24 0 6
3 -4 15 0 43 0
0 0 0 6 0 19
Compliance Tensor Sij (10-12Pa-1)
11.1 -5.2 -1.1 0 -0.9 0
-5.2 13.2 -4.6 0 3.1 0
-1.1 -4.6 9.8 0 -3.7 0
0 0 0 45.4 0 -14.9
-0.9 3.1 -3.7 0 24.9 0
0 0 0 -14.9 0 57
Shear Modulus GV
32 GPa
Bulk Modulus KV
81 GPa
Shear Modulus GR
27 GPa
Bulk Modulus KR
80 GPa
Shear Modulus GVRH
29 GPa
Bulk Modulus KVRH
81 GPa
Elastic Anisotropy
0.97
Poisson's Ratio
0.34

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Dy2SiO5 (mp-752405) 0.5865 0.023 3
Sr2GeSe4 (mp-30293) 0.5617 0.000 3
Sr2SnS4 (mp-30294) 0.5949 0.000 3
Dy4(SiS4)3 (mp-10771) 0.6055 0.002 3
Tb4(SiS4)3 (mp-16402) 0.6081 0.000 3
KNdGeS4 (mp-861866) 0.5526 0.000 4
KLaGeS4 (mp-559043) 0.5555 0.000 4
KLaGeSe4 (mp-21097) 0.5515 0.000 4
KCeGeSe4 (mp-21176) 0.5675 0.000 4
KEuGeS4 (mp-21903) 0.5708 0.026 4
Na2SrVP2O9 (mp-565217) 0.7147 0.000 5
K3WS3ClO (mp-565818) 0.6729 0.162 5
Na2CaVP2O9 (mp-566264) 0.6304 0.000 5
SrMgTi(PO4)2 (mvc-2641) 0.6905 0.152 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Yb_2 Si O
Final Energy/Atom
-6.9170 eV
Corrected Energy
-224.5644 eV
Uncorrected energy = -221.3444 eV Composition-based energy adjustment (-0.161 eV/atom x 20.0 atoms) = -3.2200 eV Corrected energy = -224.5644 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 4446
Submitted by
User remarks:
  • Diytterbium oxide silicate

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)